# US 2026/0085251 A1 · Sliding composition and use thereof, and method for producing sliding composition

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0085251 A1
- Document ID: US20260085251A1
- Status: Published application
- Kind: A1
- Application number: 19/111,318
- Filed: 2023-09-13
- Published: 2026-03-26
- Earliest claimed: 2022-09-14
- Assignees: Mitsui Chemicals, Inc.
- Applicants: Mitsui Chemicals, Inc.
- Inventors: Yasuhiro SHIBATA; Kakeru CHIGAMA; Akihiro YAMAMOTO
- Web page: https://patentgrep.com/patent/US20260085251A1

## CPC

- C08L 23/04: Homopolymers or copolymers of ethene
- C10M 107/04: Polyethylene
- C08L 23/142: {at least partially crystalline copolymers of propene with other olefins}
- C10M 107/06: containing propene
- C10M 107/32: Condensation polymers of aldehydes or ketones; Polyesters; Polyethers
- C10M 107/50: containing silicon
- C10M 177/00: Special methods of preparation of lubricating compositions; Chemical modification by after-treatment of components or of the whole of a lubricating composition, not covered by other classes
- C08G 77/04: Polysiloxanes
- C08L 2205/035: containing four or more polymers in a blend
- C08L 2205/22: Mixtures comprising a continuous polymer matrix in which are dispersed crosslinked particles of another polymer
- C10M 2205/0225: used as base material
- C10M 2205/0245: used as base material
- C10M 2209/1013: used as base material
- C10M 2229/0405: used as base material
- C10N 2050/08: Solids
- C10N 2070/00: Specific manufacturing methods for lubricant compositions
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- C10M: LUBRICATING COMPOSITIONS (well drilling compositions C09K8/02); USE OF CHEMICAL SUBSTANCES EITHER ALONE OR AS LUBRICATING INGREDIENTS IN A LUBRICATING COMPOSITION (mould release, i.e. separating, agents for metals B22C3/00, for plastics or substances in a plastic state, in general B29C33/56, for glass C03B40/02; textile lubricating compositions D06M11/00, D06M13/00, D06M15/00; immersion oils for microscopy G02B21/33)
- C08G: MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS
- C10N: INDEXING SCHEME ASSOCIATED WITH SUBCLASS C10M RELATING TO LUBRICATING COMPOSITIONS

## Abstract

One aspect of the present invention relates to a sliding composition film or a method for producing a sliding composition, the sliding composition including an ethylene/α-olefin/nonconjugated polyene copolymer (A); a propylene-based random copolymer (B1) and a propylene homopolymer (B2), having a melt flow rate of 0.1 to 4.0 g/10 min; high-density polyethylene (C1) having a density of 940 to 970 kg/m3 and a MFR of 0.1 g/10 min or less; ultra-high molecular weight polyethylene (C2) having an intrinsic viscosity [η] of 10 to 40 dl/g (in decalin at 135° C.), an average particle size D50 of 22 to 50 μm, and a density of less than 940 kg/m3; and a silicone compound (D) having a kinematic viscosity of 3,000 to 1,000,000 cSt (at 25° C.) in each predetermined content, in which the ethylene/α-olefin/nonconjugated polyene copolymer (A) is at least partially cross-linked with a phenolic resin-based cross-linking agent.

## Claims

### Claim 1

A sliding composition, comprising:
7.0% by mass or more of an ethylene/α-olefin/nonconjugated polyene copolymer (A);
6.0% by mass or more of a propylene-based random copolymer (B1) having a melt flow rate of 0.1 to 4.0 g/10 min measured at 190° C. under a load of 2.16 kgf;
10.0% by mass or more of a propylene homopolymer (B2) having a melt flow rate of 0.1 to 4.0 g/10 min measured at 190° C. under a load of 2.16 kgf;
15.0% by mass or more of high-density polyethylene (C1) having a density of 940 to 970 kg/m3 and a melt flow rate of 0.1 g/10 min or less measured at 190° C. under a load of 2.16 kgf;
10.0% by mass or more of ultra-high molecular weight polyethylene (C2) having an intrinsic viscosity [η] of 10 to 40 dl/g, as measured in a decalin solvent at 135° C., an average particle size D50 of 22 to 50 μm, and a density of less than 940 kg/m3; and
5.0 to 8.0% by mass of a silicone compound (D) having a kinematic viscosity of 3,000 to 1,000,000 cSt at 25° C.,
wherein a total content of components (A), (B1), (B2), (C1), (C2) and (D) is 100.0% by mass or less, and
the ethylene/α-olefin/nonconjugated polyene copolymer (A) is at least partially cross-linked with a phenolic resin-based cross-linking agent.

### Claim 2 (depends on 1)

The sliding composition according to claim 1, further comprising 0.1 to 10.0% by mass of a softener €,
wherein a total content of the components (A), (B1), (B2), (C1), (C2), (D) and E is 100.0% by mass or less, and
the ethylene/α-olefin/nonconjugated polyene copolymer (A) has a weight-average molecular weight of 280,000 or more and an intrinsic viscosity [η] measured in decalin at 135° C. of 3.4 dl/g or more, and when a total content of constituent units derived from ethylene and constituent units derived from an α-olefin is 100% by mass, a content of constituent units derived from ethylene is 70% by mass or less, and a content of constituent units derived from a nonconjugated polyene in all constituent units of the copolymer (A) is 6.0% by mass or less.

### Claim 3 (depends on 1)

The sliding composition according to claim 1, wherein Shore D hardness 5 seconds after starting measurement measured in accordance with ISO 7619 is 30 to 60.

### Claim 4 (depends on 1)

The sliding composition according to claim 1, wherein a content of the ethylene/α-olefin/nonconjugated polyene copolymer (A) is 7.0 to 10.0% by mass.

### Claim 5 (depends on 1)

The sliding composition according to claim 1, wherein a total content of the propylene-based random copolymer (B1) and the propylene homopolymer (B2) is 20.0% by mass or more.

### Claim 5 (depends on 1)

The sliding composition according to claim 1, wherein a content of the propylene-based random copolymer (B1) is 9.0 to 15.0% by mass, and the propylene-based random copolymer (B1) has a density of 900 to 920 kg/m3.

### Claim 7 (depends on 1)

The sliding composition according to claim 1, wherein a content of the propylene homopolymer (B2) is 10.0 to 18.0% by mass, and the propylene homopolymer (B2) has a density of 900 to 920 kg/m3.

### Claim 8 (depends on 1)

The sliding composition according to claim 1, wherein (B2)/(B1) that is a mass ratio of the propylene homopolymer (B2) to the propylene-based random copolymer (B1) is 1.0 to 3.0.

### Claim 9 (depends on 1)

The sliding composition according to claim 1, wherein a content of the ultra-high molecular weight polyethylene (C2) is 10.0 to 30.0% by mass, and the ultra-high molecular weight polyethylene (C2) has an average particle size D50 of 22 to 30 μm.

### Claim 10 (depends on 1)

A molded body obtained by molding the sliding composition according to claim 1.

### Claim 11 (depends on 10)

A glass run channel comprising the molded body according to claim 10.

### Claim 12

A method for producing a sliding composition, the sliding composition comprising:
7.0% by mass or more of an ethylene/α-olefin/nonconjugated polyene copolymer (A);
6.0% by mass or more of a propylene-based random copolymer (B1) having a melt flow rate of 0.1 to 4.0 g/10 min measured at 190° C. under a load of 2.16 kgf;
10.0% by mass or more of a propylene homopolymer (B2) having a melt flow rate of 0.1 to 4.0 g/10 min measured at 190° C. under a load of 2.16 kgf;
15.0% by mass or more of high-density polyethylene (C1) having a density of 940 to 970 kg/m3 and a melt flow rate of 0.1 g/10 min or less measured at 190° C. under a load of 2.16 kgf;
10.0% by mass or more of ultra-high molecular weight polyethylene (C2) having an intrinsic viscosity [η] of 10 to 40 dl/g, as measured in a decalin solvent at 135° C., an average particle size D50 of 22 to 50 μm, and a density of less than 940 kg/m3; and
5.0 to 8.0% by mass of a silicone compound (D) having a kinetic viscosity of 3,000 to 1,000,000 cSt at 25° C.,
wherein a total content of the components (A), (B1), (B2), (C1), (C2) and (D) is 100.0% by mass or less, and
the ethylene/α-olefin/nonconjugated polyene copolymer (A) is at least partially cross-linked,
the method comprising the step of cross-linking the ethylene/α-olefin/nonconjugated polyene copolymer (A) at least partially with a phenol resin-based cross-linking agent.