# US 2026/0085183 A1 · Fluororesin composition, molded body, and production method for fluorine resin composition

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0085183 A1
- Document ID: US20260085183A1
- Status: Published application
- Kind: A1
- Application number: 19/404,216
- Filed: 2025-12-01
- Published: 2026-03-26
- Earliest claimed: 2023-06-02
- Assignees: AGC Inc.
- Applicants: AGC Inc.
- Inventors: Kaori ABE; Mariko MATSUMOTO; Satoshi OTSUGU; Daisuke TAGUCHI
- Web page: https://patentgrep.com/patent/US20260085183A1

## CPC

- C08L 27/18: Homopolymers or copolymers or tetrafluoroethene
- C08J 3/005: {Processes for mixing polymers}
- C08J 3/03: in aqueous media
- C08J 3/14: by precipitation from solutions {(C08J3/122 takes precedence)}
- C08F 114/26: Tetrafluoroethene
- C08J 2327/18: Homopolymers or copolymers of tetrafluoroethylene
- C08L 2205/02: containing two or more polymers of the same C08L -group
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)
- C08F: MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS

## Abstract

A fluororesin composition contains a first fluororesin having a thermal history of having been heated to a melting point or higher and a second fluororesin having no thermal history of having been heated to a melting point or higher, in which the first fluororesin and the second fluororesin are non-melt-formable fluororesins, and in a case where a test piece is obtained by compression-molding the fluororesin composition to obtain a preliminary molded body and sintering the preliminary molded body at 380° C. for 2 hours or longer to be formed into a micro-dumbbell shape having a thickness of 0.5 mm and a size of 16 mm×45 mm, a metal elution amount with respect to a total mass of the test piece when the test piece is left to stand in 3.6% by mass hydrochloric acid at 23° C. for 24 hours is 5 ng/g or less.

## Claims

### Claim 1

A fluororesin composition comprising:
a first fluororesin having a thermal history of having been heated to a melting point or higher; and
a second fluororesin having no thermal history of having been heated to a melting point or higher,
wherein the first fluororesin and the second fluororesin are non-melt-formable fluororesins, and
a metal elution amount with respect to a total mass of a test piece of the fluororesin composition is 5 ng/g or less when the test piece is left to stand in 3.6% by mass hydrochloric acid at 23° C. for 24 hours, wherein the test piece is obtained by compression-molding the fluororesin composition to obtain a preliminary molded body and sintering the preliminary molded body at 380° C. for 2 hours or longer to form the preliminary molded body into a micro-dumbbell shape having a thickness of 0.5 mm and a size of 16 mm×45 mm.

### Claim 2 (depends on 1)

The fluororesin composition according to claim 1,
wherein the first fluororesin has a tetrafluoroethylene unit, and an amount of the tetrafluoroethylene unit with respect to a total mass of the first fluororesin is 99% by mass or more.

### Claim 3 (depends on 2)

The fluororesin composition according to claim 2,
wherein the second fluororesin has a tetrafluoroethylene unit, and an amount of the tetrafluoroethylene unit with respect to a total mass of the second fluororesin is 99% by mass or more.

### Claim 4 (depends on 1)

The fluororesin composition according to claim 1,
wherein an amount of the first fluororesin with respect to a total mass of the first fluororesin and the second fluororesin is 10% by mass or more.

### Claim 5 (depends on 2)

The fluororesin composition according to claim 2,
wherein an amount of the first fluororesin with respect to a total mass of the first fluororesin and the second fluororesin is 10% by mass or more.

### Claim 6 (depends on 3)

The fluororesin composition according to claim 3,
wherein an amount of the first fluororesin with respect to a total mass of the first fluororesin and the second fluororesin is 10% by mass or more.

### Claim 7 (depends on 1)

A molded body of the fluororesin composition according to claim 1.

### Claim 8 (depends on 2)

A molded body of the fluororesin composition according to claim 2.

### Claim 9 (depends on 3)

A molded body of the fluororesin composition according to claim 3.

### Claim 10 (depends on 1)

A production method for the fluororesin composition according to claim 1, the production method comprising:
washing a mixture containing the first fluororesin and the second fluororesin.

### Claim 11 (depends on 2)

A production method for the fluororesin composition according to claim 2, the production method comprising:
washing a mixture containing the first fluororesin and the second fluororesin.

### Claim 12 (depends on 3)

A production method for the fluororesin composition according to claim 3, the production method comprising:
washing a mixture containing the first fluororesin and the second fluororesin.