# US 2026/0085175 A1 · Membrane material having immiscible polymers for use in optical fiber cable structures

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0085175 A1
- Document ID: US20260085175A1
- Status: Published application
- Kind: A1
- Application number: 19/408,822
- Filed: 2025-12-04
- Published: 2026-03-26
- Earliest claimed: 2023-06-08
- Assignees: Corning Research & Development Corporation
- Applicants: Corning Research & Development Corporation
- Inventors: Michael Alexander Heinz
- Web page: https://patentgrep.com/patent/US20260085175A1

## CPC

- C08L 23/06: Polyethylene
- G02B 6/4486: {Protective covering}
- C08L 23/12: Polypropene
- C08L 23/14: Copolymers of propene (C08L23/16 takes precedence)
- C08L 67/02: Polyesters derived from dicarboxylic acids and dihydroxy compounds (C08L67/06 takes precedence)
- G02B 6/443: {Protective covering}
- C08L 2203/30: used for thermoforming
- C08L 2205/025: containing two or more polymers of the same hierarchy C08L, and differing only in parameters such as density, comonomer content, molecular weight, structure
- C08L 2205/03: containing three or more polymers in a blend
- C08L 2207/062: HDPE
- G02B 6/441: {built up from sub-bundles (G02B6/4429, G02B6/4439, G02B6/4479 take precedence)}
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- G02B: OPTICAL ELEMENTS, SYSTEMS OR APPARATUS

## Abstract

Provided are embodiments of an extruded membrane material. The extruded membrane material includes a first thermoplastic polymer and a second thermoplastic polymer. The first thermoplastic polymer and the second thermoplastic polymer are immiscible. The first thermoplastic polymer forms a first phase oriented along an extrusion direction, and the second thermoplastic polymer forms a second phase oriented along the extrusion direction. The first phase is co-continuous with the second phase. Further, the extruded membrane material has a tensile yield strength of at least 10 MPa along the extrusion direction and a peel strength of 4 N or less transverse to the extrusion direction.

## Claims

### Claim 1

A subunit, comprising:
a plurality of optical fibers; and
a membrane surrounding the plurality of optical fibers, the membrane formed of an extruded material comprising:
a first thermoplastic polymer; and
a second thermoplastic polymer;
wherein the first thermoplastic polymer and the second thermoplastic polymer are immiscible;
wherein the first thermoplastic polymer forms a first phase oriented along an extrusion direction and the second thermoplastic polymer forms a second phase oriented along the extrusion direction, the first phase being co-continuous with the second phase;
wherein the extruded membrane material comprises a tensile yield strength of at least 10 MPa along the extrusion direction and a peel strength of 4 N or less transverse to the extrusion direction.

### Claim 2 (depends on 1)

The subunit of claim 1, wherein the first thermoplastic polymer is a polyolefin.

### Claim 3 (depends on 2)

The subunit of claim 2, wherein the polyolefin is selected from a group consisting of polyethylene, a polypropylene, a polyolefin-based elastomer, and combinations thereof.

### Claim 4 (depends on 2)

The subunit of claim 2, wherein the polyolefin is a polyethylene or a polypropylene.

### Claim 5 (depends on 4)

The subunit of claim 4, wherein the second thermoplastic polymer is a technical thermoplastic.

### Claim 6 (depends on 5)

The subunit of claim 5, wherein the technical thermoplastic is selected from a group consisting of a polyester, a polyether, a polyamide, a polyacetal, a polysulfone, a polyimide, a polyketone, and combinations thereof.

### Claim 7 (depends on 5)

The subunit of claim 5, wherein the extruded material comprises from 25 wt % to 85 wt % of the polyolefin and from 15 wt % to 75 wt % of the technical thermoplastic.

### Claim 8 (depends on 1)

The subunit of claim 1, wherein the first thermoplastic polymer and the second thermoplastic polymer are selected from a group consisting of a polyolefin, a polyvinylchloride, a polystyrene, an acrylonitrile butadiene styrene, a styrene-acrylonitrile, a styrene-ethylene-butylene-styrene, and combinations thereof.

### Claim 9 (depends on 1)

The subunit of claim 1, wherein the extruded material further comprises a third thermoplastic polymer.

### Claim 10 (depends on 9)

The subunit of claim 9, wherein the third thermoplastic polymer comprises a technical thermoplastic.

### Claim 11 (depends on 10)

The subunit of claim 10, comprising from 5 wt % to 95 wt % of the first thermoplastic polymer, from 5 wt % to 93 wt % of the second thermoplastic polymer, and from 2 wt % to 10 wt % of the technical thermoplastic.

### Claim 12 (depends on 1)

The subunit of claim 1, wherein the membrane has a thickness of 100 μm or less.

### Claim 13 (depends on 1)

An optical fiber cable, comprising:
a cable jacket comprising an inner surface and an outer surface, the inner surface defining a central bore extending along a longitudinal axis of the optical fiber cable and the outer surface defining an outermost surface of the optical fiber cable;
a plurality of subunits according to claim 1 disposed within the central bore;
wherein the outer surface of the cable jacket defines a cross-sectional area perpendicular to the longitudinal axis and wherein the optical fiber cable comprises a fiber density of at least 7.5 fibers/mm2 as measured at the cross-sectional area.

### Claim 14

A method of forming an optical fiber subunit, comprising:
blending a first thermoplastic polymer with a second thermoplastic polymer, the first thermoplastic polymer being immiscible with the second thermoplastic polymer;
extruding the first thermoplastic polymer and the second thermoplastic polymer together to form a membrane that surrounds a plurality of optical fibers, wherein the first thermoplastic polymer forms a first phase oriented along an extrusion direction and the second thermoplastic polymer forms a second phase oriented along the extrusion direction, the first phase being co-continuous with the second phase;
wherein the membrane has a tensile yield strength of at least 10 MPa along the extrusion direction and a peel strength of 4 N or less transverse to the extrusion direction.

### Claim 15 (depends on 14)

The method of claim 14, wherein blending further comprises blending the first thermoplastic polymer and the second thermoplastic polymer with a coupling agent.

### Claim 16 (depends on 15)

The method of claim 15, wherein the coupling agent comprises either the first thermoplastic polymer or the second thermoplastic polymer functionalized with a functional group selected from a group consisting of maleic anhydride, silane, epoxy, acrylate, amine, hydroxyl, melamine, zirconate, titanate, polyol, or ester.

### Claim 17 (depends on 15)

The method of claim 15, wherein the membrane material comprises up to 15 wt % of the coupling agent.

### Claim 18 (depends on 15)

The method of claim 15, wherein the first thermoplastic polymer is a first polyolefin.

### Claim 19 (depends on 18)

The method of claim 18, wherein the second thermoplastic polymer is a technical thermoplastic.

### Claim 20 (depends on 18)

The method of claim 18, wherein the second thermoplastic polymer is a second polyolefin different from the first polyolefin.