# US 2026/0085161 A1 · Ultra-high molecular weight polyethylene (uhmwpe) particles and filled articles produced therewith

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0085161 A1
- Document ID: US20260085161A1
- Status: Published application
- Kind: A1
- Application number: 19/099,410
- Filed: 2023-08-09
- Published: 2026-03-26
- Earliest claimed: 2022-08-09
- Assignees: W. L. Gore & Associates, Inc.; W. L. Gore & Associates G.K.
- Applicants: W. L. Gore & Associates, Inc.; W. L. Gore & Associates G.K.
- Inventors: Guy A. Sbriglia; Jeffrey A. Knopf; Mark D. Edmundson; Shunsuke Takaki; Shailesh P. Vidhate; Ryuta Yamamoto; Joseph W. Henderson
- Web page: https://patentgrep.com/patent/US20260085161A1

## CPC

- H01M 4/622: {being polymers}
- C08F 10/02: Ethene
- C08J 3/203: {Solid polymers with solid and/or liquid additives}
- C08K 3/04: Carbon
- C08K 3/22: of metals
- C08L 23/06: Polyethylene
- H01M 4/0435: {Rolling or calendering}
- H01M 4/131: Electrodes based on mixed oxides or hydroxides, or on mixtures of oxides or hydroxides, e.g. LiCoOx
- H01M 4/133: Electrodes based on carbonaceous material, e.g. graphite-intercalation compounds or CFx
- H01M 4/136: Electrodes based on inorganic compounds other than oxides or hydroxides, e.g. sulfides, selenides, tellurides, halogenides or LiCoFy
- H01M 4/1391: of electrodes based on mixed oxides or hydroxides, or on mixtures of oxides or hydroxides, e.g. LiCoOx
- H01M 4/1393: of electrodes based on carbonaceous material, e.g. graphite-intercalation compounds or CFx
- H01M 4/1397: of electrodes based on inorganic compounds other than oxides or hydroxides, e.g. sulfides, selenides, tellurides, halogenides or LiCoFy
- H01M 4/525: of mixed oxides or hydroxides containing iron, cobalt or nickel for inserting or intercalating light metals, e.g. LiNiO2, LiCoO2 or LiCoOxFy
- H01M 4/5825: {Oxygenated metallic salts or polyanionic structures, e.g. borates, phosphates, silicates, olivines}
- H01M 4/587: for inserting or intercalating light metals
- H01M 4/625: {Carbon or graphite}
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- C08J 2323/06: Polyethene
- C08J 2427/18: Homopolymers or copolymers of tetrafluoroethylene
- C08K 2003/2289: {of cobalt}
- C08K 2003/2293: {of nickel}
- C08K 2201/001: Conductive additives
- C08L 2203/20: use in electrical or conductive gadgets
- C08L 2207/068: Ultra high molecular weight polyethylene
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- C08F: MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

Apparatuses, systems, materials, and methods for preparing polyethylene electrodes for use in energy storage and transfer via dry electrode processing is described herein. Ultra-high molecular weight polyethylene (UHMWPE) particles and filler particles are used to form a blended composition. With shear, the UHMWPE fibrillates to durably enmesh the filler particles. The blended composition with the fibrillated UHMWPE particles may, in turn, be used to form an article, such as an electrode. The blended composition may contain less than 10% by weight of the UHMWPE. The UHMWPE has a molecular weight of at least about 2,000,000 g/mol, a bulk density from about 0.04 g/mL to about 0.25 g/mL, and a melt enthalpy of at least 190 J/g. In some embodiments, the UHMWPE may be conditioned to alter the size and/or shape of the particles. The median diameter of the conditioned UHMWPE particles is from 5 microns to 300 microns.

## Claims

### Claim at position 1

-67. (canceled)

### Claim 68

A method of manufacturing an article comprising:
shearing filler particles and ultra-high molecular weight polyethylene (UHMWPE) particles having a molecular weight of at least 2,000,000 g/mol and a melt enthalpy of at least 190 J/g to form a blended particle composition, wherein the filler particles are durably enmeshed within fibrils formed by the UHMWPE particles; and
forming the blended particle composition into an article,
wherein the article contains at least 80% by weight filler particles.

### Claim 69 (depends on 68)

The method of claim 68, comprising fibrillating the UHMWPE particles prior to shearing the filler particles and the UHMWPE particles.

### Claim 70 (depends on 68)

The method of claim 68, wherein forming the blended particle composition into an article includes calendering the blended particle composition.

### Claim 71 (depends on 68)

The method of claim 68, wherein the article has DSC curve with a DSC peak between about 143° C. and about 175° C. and wherein the article has a fibrillation percentage greater than 0%.

### Claim 72 (depends on 68)

The method of claim 68, wherein the particles include at least one of carbon particles, conductive carbon particles, activated carbon particles, graphite particles, carbon black particles, and lithium compound particles.

### Claim 73 (depends on 68)

The method of claim 68, comprising conditioning the UHMWPE particles prior to shearing the filler particles and the UHMWPE particles, wherein the conditioned UHMWPE particles have a median Da from about 10 microns to about 300 microns.

### Claim 74 (depends on 68)

The method of claim 68, wherein the blended particle composition comprises less than 10% by weight of the fibrillatable UHMWPE particles.

### Claim 75

A composite material comprising:
a filler material including filler particles; and
a binder system including ultra-high molecular weight polyethylene (UHMWPE) particles having a molecular weight of at least 2,000,000 g/mol and a melt enthalpy of at least 190 J/g, wherein the filler material and the UHMWPE particles are sheared and formed into an article such that the composite material includes a DSC peak from about 143° C. to about 175° C.

### Claim 76 (depends on 75)

The composite material of claim 75, wherein the composite material has a DSC curve with the DSC peak between about 143° C. and about 175° C., wherein a fibrillation percentage is determined by an integration of the DSC peak as a percentage of an integration of the DSC curve between about 100° C. and about 175° C., and wherein the article has a fibrillation percentage greater than 0%.

### Claim 77 (depends on 75)

The composite material of claim 75, wherein the filler material is selected from at least one of carbon particles, conductive carbon particles, activated carbon particles, graphite particles, carbon black particles, and lithium compound particles.

### Claim 78 (depends on 75)

The composite material of claim 75, wherein the binder system includes less than 20% by weight polytetrafluoroethylene.

### Claim 79 (depends on 75)

The composite material of claim 75, wherein the binder system is free of polytetrafluoroethylene.

### Claim 80

A electrode, comprising:
a filler material; and
a binder system including fibrillated ultra-high molecular weight polyethylene (UHMWPE) particles having:
a median Da from about 5 microns to about 300 microns,
a median sphericity from about 0.820 to about 0.880,
a median convexity from about 0.950 to about 0.990, and
a median length-to-width ratio from about 1.50 to about 1.80,
wherein the UHMWPE particles have a DSC peak from about 143° C. to about 175° C.

### Claim 81 (depends on 80)

The electrode of claim 80, wherein the filler material is at least 90% by weight of the electrode.

### Claim 82 (depends on 80)

The electrode of claim 80, wherein the UHMWPE particles are 10% or less by weight of the electrode.

### Claim 83 (depends on 80)

The electrode of claim 80, wherein the electrode is self-supporting.

### Claim 84 (depends on 80)

The electrode of claim 80, wherein the electrode has a DSC curve with a DSC peak between about 143° C. and about 175° C., and wherein the electrode has a fibrillation percentage greater than 0%.

### Claim 85 (depends on 80)

The electrode of claim 80, wherein the UHMWPE particles have a median Da from about 5 microns to about 300 microns, or a median sphericity from about 0.820 to about 0.880, or a median convexity from about 0.950 to about 0.990, or a median length-to-width ratio from about 1.50 to about 1.80.

### Claim 86 (depends on 80)

The electrode of claim 80, wherein the binder system includes less than 20% by weight polytetrafluoroethylene.

### Claim 87 (depends on 80)

The electrode of claim 80, wherein the binder system is free of polytetrafluoroethylene.