# US 2026/0084980 A1 · Positive Electrode Active Material, Method for Preparing the Same, Positive Electrode and Lithium Secondary Battery Comprising the Same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0084980 A1
- Document ID: US20260084980A1
- Status: Published application
- Kind: A1
- Application number: 19/339,911
- Filed: 2025-09-25
- Published: 2026-03-26
- Earliest claimed: 2023-02-16
- Assignees: LG Energy Solution, Ltd.
- Applicants: LG Energy Solution, Ltd.
- Inventors: Youshin Lee; Gi Beom Han; Kang Joon Park; Jaeyoung Lee; Sin Young Park; Byungchun Park
- Web page: https://patentgrep.com/patent/US20260084980A1

## CPC

- C01G 45/1228: of the type (MnO2)-, e.g. LiMnO2 or Li(MxMn1-x)O2
- H01M 4/505: of mixed oxides or hydroxides containing manganese for inserting or intercalating light metals, e.g. LiMn2O4 or LiMn2OxFy
- H01M 4/0471: {involving thermal treatment, e.g. firing, sintering, backing particulate active material, thermal decomposition, pyrolysis}
- H01M 4/364: {as mixtures}
- H01M 4/525: of mixed oxides or hydroxides containing iron, cobalt or nickel for inserting or intercalating light metals, e.g. LiNiO2, LiCoO2 or LiCoOxFy
- H01M 10/052: Li-accumulators
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- C01P 2004/03: obtained by SEM
- C01P 2004/45: Aggregated particles or particles with an intergrown morphology
- C01P 2004/61: Micrometer sized, i.e. from 1-100 micrometer
- C01P 2004/64: Nanometer sized, i.e. from 1-100 nanometer
- C01P 2006/40: Electric properties
- H01M 2004/028: {Positive electrodes}
- Y02E 60/10: Energy storage using batteries
- C01G: COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSES C01D OR C01F (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts or peroxyacids C01B15/00; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium, or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds containing nitrogen, other non-metals and metal C01B21/082}; metal amides C01B21/092; nitrites C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; compounds having molecular sieve properties but not having base-exchange properties C01B37/00; compounds having molecular sieve and base-exchange properties, e.g. crystalline zeolites, C01B39/00; cyanides C01C3/08; salts of cyanamide C01C3/16; thiocyanates C01C3/20)
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A positive electrode active material includes a lithium-rich manganese-based oxide represented by the following Chemical Formula 1, and has a structure in which a rock-salt-type lithium manganese oxide and a layered lithium transition metal oxide are mixed. The lithium-rich manganese-based oxide may have a prescribed internal porosity. in Chemical Formula 1, 1.00<a, 0≤b≤0.53, 0≤c≤0.10, 0.47≤d≤1.00, 0≤e≤0.20, and M is at least one selected from the group consisting of Al, B, Co, W, Mg, V, Ti, Zn, Ga, In, Ru, Nb, Sn, Sr and Zr.

## Claims

### Claim 1

A positive electrode active material comprising:
a lithium-rich manganese-based oxide represented by the following Chemical Formula 1 and having a structure in which a rock-salt-type lithium manganese oxide and a layered lithium transition metal oxide are in a mixed state,
wherein the lithium-rich manganese-based oxide has an internal porosity ranging from 2.5% to 13.0%:
wherein, 1.00<a, 0<b≤0.53, 0≤c≤0.10, 0.47≤d<1.00, 0≤e≤0.20, and M is at least one selected from the group consisting of Al, B, W, Mg, V, Ti, Zn, Ga, In, Ru, Nb, Sn, Sr and Zr.

### Claim 2 (depends on 1)

The positive electrode active material of claim 1, wherein:
in Chemical Formula 1, 1.10≤a≤1.5, 0.10≤b≤0.40, 0≤c≤0.05, 0.47≤d≤0.80, and 0≤e≤0.10.

### Claim 3 (depends on 1)

The positive electrode active material of claim 1, wherein:
in Chemical Formula 1, 1.12<a<1.18, 0.24<b<0.36, 0<c<0.10, 0.47≤d<0.63, 0<e<0.05, and M is at least one selected from the group consisting of Al, Mg, V, Ti, Zr, Nb and W.

### Claim 4 (depends on 1)

The positive electrode active material of claim 1, wherein the rock-salt-type lithium manganese oxide includes Li2MnO3.

### Claim 5 (depends on 1)

The positive electrode active material of claim 1, wherein the lithium-rich manganese-based oxide is represented by the following Chemical Formula 2:
wherein, 0.2≤X≤0.5, 0.4≤y<1, 0≤z≤0.1, 0≤w≤10.2, and M is at least one selected from the group consisting of Al, B, W, Mg, V, Ti, Zn, Ga, In, Ru, Nb, Sn, Sr and Zr.

### Claim 6 (depends on 1)

The positive electrode active material of claim 1, wherein the positive electrode active material has a secondary particle shape and an average particle size (D50) ranging from 2 μm to 10 μm,
wherein the secondary particle shape has a plurality of primary particles having a particle size ranging from 50 nm to 200 nm aggregated.

### Claim 7 (depends on 1)

The positive electrode active material of claim 1, wherein the lithium-rich manganese-based oxide has the internal porosity ranging from 4.0% to 13.0%.

### Claim 8 (depends on 1)

A method for preparing the positive electrode active material of claim 1, the method comprising:
(A) mixing a lithium-rich manganese-based transition metal hydroxide precursor and a lithium raw material to form a mixture; and
(B) firing the mixture at a temperature of 600° C. or more to form the lithium-rich manganese-based oxide.

### Claim 9 (depends on 8)

The method of claim 8, wherein the lithium-rich manganese-based transition metal hydroxide precursor is represented by the following Chemical Formula 1a:
wherein, 0<b≤0.53, 0≤c≤0.10, 0.47≤d<1.00, 0≤e≤0.20, and M is at least one selected from the group consisting of Al, B, W, Mg, V, Ti, Zn, Ga, In, Ru, Nb, Sn, Sr and Zr.

### Claim 10 (depends on 8)

The method of claim 8, wherein the lithium-rich manganese-based transition metal hydroxide precursor is formed by subjecting a transition metal raw material to a co-precipitation reaction at a pH ranging from 9.5 to 12.

### Claim 11 (depends on 8)

The method of claim 8, wherein the firing is performed at a temperature ranging from 600° C. to 1000° C.

### Claim 12 (depends on 8)

The method of claim 8, wherein the lithium-rich manganese-based oxide is represented by the following Chemical Formula 2:
wherein, 0.2≤X≤0.5, 0.4≤y<1, 0≤z≤0.1, 0≤w≤0.2, and M is at least one selected from the group consisting of Al, B, W, Mg, V, Ti, Zn, Ga, In, Ru, Nb, Sn, Sr and Zr.

### Claim 13 (depends on 1)

A positive electrode comprising the positive electrode active material of claim 1.

### Claim 14 (depends on 1)

A lithium secondary battery comprising a positive electrode, a negative electrode, a separator and an electrolyte,
wherein the positive electrode includes a positive electrode active material layer containing the positive electrode active material of claim 1.