# US 2026/0084970 A1 · Pitch-based composite powders containing a graphitization catalyst and methods for production and use thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0084970 A1
- Document ID: US20260084970A1
- Status: Published application
- Kind: A1
- Application number: 19/407,916
- Filed: 2025-12-03
- Published: 2026-03-26
- Earliest claimed: 2023-06-15
- Assignees: ExxonMobil Technology and Engineering Company
- Applicants: ExxonMobil Technology and Engineering Company
- Inventors: Krishnan Anantha Narayana Iyer; Ali H. Slim; Shiun Ling; Li Wang; Liang Li; Caiguo Gong
- Web page: https://patentgrep.com/patent/US20260084970A1

## CPC

- C01B 32/205: Preparation
- H01M 4/133: Electrodes based on carbonaceous material, e.g. graphite-intercalation compounds or CFx
- H01M 4/364: {as mixtures}
- H01M 4/587: for inserting or intercalating light metals
- H01M 4/8605: {Porous electrodes}
- H01M 4/8652: {as mixture}
- H01M 4/90: Selection of catalytic material
- H01M 4/9016: {Oxides, hydroxides or oxygenated metallic salts}
- H01M 4/96: Carbon-based electrodes
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- C01P 2002/02: Amorphous compounds
- C01P 2002/74: by peak-intensities or a ratio thereof only
- C01P 2002/88: by thermal analysis data, e.g. TGA, DTA, DSC
- C01P 2004/61: Micrometer sized, i.e. from 1-100 micrometer
- C01P 2006/40: Electric properties
- Y02E 60/10: Energy storage using batteries
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

Composite powders for electrode production may be formed by blending a graphitization catalyst or precursor thereof with petroleum pitch under grinding conditions. The composite powders may comprise about 0.1 wt. % to about 30 wt. % graphitization catalyst or a precursor thereof, based on total mass of the composite powder, and about 20 wt. % to about 99.9 wt. % petroleum pitch, based on total mass of the composite powder. The graphitization catalyst or the precursor thereof is dispersed in a matrix comprising the petroleum pitch, and the petroleum pitch comprises a plurality of pitch particles. The composite powders may be subsequently carbonized and then graphitized under conditions that may be less severe than un-catalyzed graphitization. The grinding conditions for forming the composite powders may include melt blending to form a continuous pitch matrix, wherein at least a portion of the graphitization catalyst or the precursor thereof may be dispersed within an interior of the pitch particles.

## Claims

### Claim 1

A composite powder for an electrode comprising:
about 0.1 wt. % to about 30 wt. % graphitization catalyst or a precursor thereof, based on a total mass of the composite powder; and
about 20 wt. % to 99.9 wt. % petroleum pitch, based on a total mass of the composite powder, wherein the graphitization catalyst or the precursor thereof is dispersed in a matrix comprising the petroleum pitch, and the petroleum pitch comprises a plurality of pitch particles, wherein the composite powder has an extent of anisotropy evident by a I(101)/I(100) peak ratio from about 0.2 to about 0.99 from X-ray diffraction (XRD) patterns.

### Claim 2 (depends on 1)

The composite powder of claim 1, wherein the petroleum pitch comprises about 50 wt. % or greater mesophase pitch.

### Claim 3 (depends on 1)

The composite powder of claim 1, wherein the graphitization catalyst or the precursor thereof is dispersed in an interstitial space between the pitch particles.

### Claim 4 (depends on 1)

The composite powder of claim 1, wherein at least a portion of the graphitization catalyst or the precursor thereof is dispersed within an interior of the pitch particles, wherein the graphitization catalyst or the precursor thereof comprises an oxide, a carbide, a salt, a coordination compound, or any combination thereof.

### Claim 5 (depends on 1)

The composite powder of claim 1, wherein the pitch particles have a particle size D50 ranging from about 1 □m to about 25 □m.

### Claim 6 (depends on 1)

The composite powder of claim 1, wherein the composite powder comprises about 0.1 wt. % to about 10 wt. % graphitization catalyst, wherein the graphitization catalyst or the precursor thereof comprises a compound containing at least one of a Group 2 element, a Group 4 element, a Group 5 element, a Group 6 element, a Group 7 element, a Group 8 element, a Group 9 element, a Group 10 element, a Group 13 element, Cu, Zn, or Si.

### Claim 7 (depends on 1)

The composite powder of claim 1, wherein the graphitization catalyst or the precursor thereof comprises a boron, iron, titanium, zirconium, manganese, nickel, cobalt, molybdenum, vanadium-containing compound, or any combination thereof.

### Claim 8 (depends on 1)

The composite powder of claim 1, wherein the graphitization catalyst comprise a boron-containing compound selected from the group consisting of boric acid, sodium tetraborate, tetrahydroxyborate salts, orthoborate salts, metaborate salts, triborate salts, tetraborate salts, pentaborate salts, octaborate salts, boronic acids, boronate esters, boron oxides, boron carbides, and combinations thereof.

### Claim 9

A method for forming a composite powder for an electrode comprising:
forming a blend comprising about 0.1 wt. % to about 35 wt. % graphitization catalyst or a precursor thereof and about 20 wt. % to about 99.9 wt. % petroleum pitch, each based on a total mass of the blend; and
processing the blend under grinding conditions to form a composite powder, wherein the graphitization catalyst is dispersed in a matrix comprising the petroleum pitch and the petroleum pitch comprises a plurality of pitch particles, wherein the composite powder has an extent of anisotropy evident by a I(101)/I(100) peak ratio from about 0.2 to about 0.99 from X-ray diffraction (XRD) patterns.

### Claim 10 (depends on 9)

The method of claim 9, wherein forming the blend comprises melt blending the graphitization catalyst or the precursor thereof and the petroleum pitch in a melt extruder at or above the softening temperature of the petroleum pitch to disperse the graphitization catalyst or the precursor thereof in a continuous pitch matrix, and processing the blend under the grinding conditions comprises grinding the continuous pitch matrix to form the pitch particles with at least a portion of the graphitization catalyst or the precursor thereof dispersed within an interior of the pitch particles.

### Claim 11 (depends on 9)

The method of claim 9, wherein the petroleum pitch comprises about 50 wt. % or greater mesophase pitch.

### Claim 12 (depends on 9)

The method of claim 9, wherein forming a blend is performed at a temperature inferior to 23° C.

### Claim 13 (depends on 9)

The method of claim 9, wherein the composite powder comprises about 0.1 wt. % to about 10 wt. % graphitization catalyst or the precursor thereof, and wherein the graphitization catalyst is up to about 500 nm in size before blending.

### Claim 14 (depends on 9)

The method of claim 9, wherein the graphitization catalyst comprises a boron-containing compound selected from the group consisting of boric acid, sodium tetraborate, tetrahydroxyborate salts, orthoborate salts, metaborate salts, triborate salts, tetraborate salts, pentaborate salts, octaborate salts, boronic acids, boronate esters, boron oxides, boron carbides, and combinations thereof.

### Claim 15 (depends on 9)

The method of claim 9, further comprising:
heating the composite powder at a temperature ranging from about 180° C. to about 450° C. in an environment containing about 0.1 mol % to about 5 mol % oxygen.

### Claim 16 (depends on 9)

The method of claim 9, further comprising:
at least partially carbonizing the composite powder at a carbonization temperature ranging from about 700° C. to about 1800° C. in an environment comprising about 0.1 mol % oxygen or below to at least partially convert the petroleum pitch to amorphous carbon with a degree of graphitization up to 60%.

### Claim 17 (depends on 16)

The method of claim 16, further comprising:
after at least partially carbonizing the composite powder, heating at a graphitization temperature above the carbonization temperature in an environment comprising about 0.1 mol % oxygen or below to convert at least a portion of the amorphous carbon into graphite.

### Claim 18 (depends on 17)

The method of claim 17, wherein about 80 wt. % or more of the petroleum pitch in the composite powder is converted to graphite.

### Claim 19 (depends on 17)

The method of claim 17, wherein the graphitization temperature is at a point in a range of from about 1800° C. to about 3400° C.

### Claim 20 (depends on 17)

The method of claim 17, wherein heating at the graphitization temperature takes place for about 0.1 hour to about 8 hours.

### Claim 21

An electrode material comprising:
up to about 35 wt. % graphitization catalyst comprising a Group 13 element dispersed in a carbon matrix, based on a total mass of the electrode material, wherein the electrode material is optionally coated using an amorphous carbon, wherein the carbon matrix has an extent of anisotropy evident by a I(101)/I(100) peak ratio from about 0.2 to about 0.99 from X-ray diffraction (XRD) patterns.

### Claim 22 (depends on 21)

The electrode material of claim 21, wherein a surface of the electrode material is devoid of nitrides and carbides.

### Claim 23 (depends on 21)

The electrode material of claim 21, wherein a graphite crystal size and thickness is up to 70% smaller than neat carbon precursors.

### Claim 24 (depends on 21)

A lithium-ion battery comprising the electrode material of claim 21.

### Claim 25 (depends on 24)

The lithium-ion battery of claim 24, wherein a capacity retention is up to 91% at 3 C discharging rate.

### Claim 26 (depends on 24)

The lithium-ion battery of claim 24, wherein a capacity retention is up to 59% at 6 C charging rate.

### Claim 27

A method of producing an electrode material comprising:
providing a composite powder comprising:
about 0.1 wt. % to about 30 wt. % graphitization catalyst or a precursor thereof, based on a total mass of the composite powder; and
about 20 wt. % to 99.9 wt. % petroleum pitch, based on a total mass of the composite powder, wherein the graphitization catalyst or the precursor thereof is dispersed in a matrix comprising the petroleum pitch, and the petroleum pitch comprises a plurality of pitch particles, wherein the composite powder has an extent of anisotropy evident by a I(101)/I(100) peak ratio from about 0.2 to about 0.99 from X-ray diffraction (XRD) patterns; and
heating the composite powder at a carbonization temperature sufficient to form a carbon matrix, wherein the heating occurs in an environment comprising about 0.1 mol % oxygen or below,
wherein the graphitization catalyst precursor, if present, is converted to the graphitization catalyst while forming the carbon matrix.

### Claim 28 (depends on 27)

The method of claim 27, wherein a graphitization temperature is at a point in a range of from about 1800° C. to about 3400° C.

### Claim 29 (depends on 27)

The method of claim 27, wherein a degree of graphitization greater than 90% is achieved at temperatures 2200° C. or higher.

### Claim 30 (depends on 27)

The method of claim 27, wherein a degree of graphitization greater than 90% is achieved within 0.1 hours.