# US 2026/0084387 A1 · Multilayer Piezoelectret Film Element, Polymeric Porous Sheet, and Method for Manufacturing the Same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0084387 A1
- Document ID: US20260084387A1
- Status: Published application
- Kind: A1
- Application number: 19/328,828
- Filed: 2025-09-15
- Published: 2026-03-26
- Earliest claimed: 2024-09-20
- Assignees: Hubei Xiangyuan High-Tech Co., Ltd
- Applicants: Hubei Xiangyuan High-Tech Co., Ltd
- Inventors: Xin Zhang; Qiong Wei
- Web page: https://patentgrep.com/patent/US20260084387A1

## CPC

- B29D 7/01: Films or sheets
- B29C 35/0866: {using particle radiation}
- B29C 2035/0877: {using electron radiation, e.g. beta-rays}
- B29K 2023/0625: {LLDPE, i.e. linear low density polyethylene}
- B29K 2105/041: {Microporous}
- B29K 2105/24: crosslinked or vulcanised
- B29K 2995/0003: having particular electrical or magnetic properties, e.g. piezoelectric
- B29K 2995/0063: Density
- B29K 2995/0097: Thickness
- B29D: PRODUCING PARTICULAR ARTICLES FROM PLASTICS OR FROM SUBSTANCES IN A PLASTIC STATE (making granules B29B9/00; making preforms B29B11/00)
- B29C: SHAPING OR JOINING OF PLASTICS; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDED FOR; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING (making preforms B29B11/00; making laminated products by combining previously unconnected layers which become one product whose layers will remain together B32B37/00 - B32B41/00)
- B29K: INDEXING SCHEME ASSOCIATED WITH SUBCLASSES B29B, B29C OR B29D, RELATING TO MOULDING MATERIALS OR TO MATERIALS FOR {MOULDS, } REINFORCEMENTS, FILLERS OR PREFORMED PARTS, e.g. INSERTS

## Abstract

A multilayer piezoelectret film element, a polymeric porous sheet, and a method for preparing them are disclosed. The present disclosure ensures that the gas can be ionized without damaging the polymeric porous sheet by adjusting the gap between pores and the dielectric strength of the polymeric porous sheet in the multilayer piezoelectret film element. The polymeric porous sheet has a high piezoelectric constant after electric polarization and surface metallization treatment, and can generate a significant amount of charge under mechanical pressure, thereby exhibiting high sensitivity in applications such as piezoelectric sensors, and solving the problems of low piezoelectric activity and fast loss of piezoelectric activity of the polarized polymeric piezoelectret film element in the art. Moreover, the production process is simple, which can ensure continuous production of the polymeric piezoelectret film element.

## Claims

### Claim 1

A multilayer piezoelectret film element, comprising a first conductive layer, a flexible porous film layer, and a second conductive layer in sequence, wherein the flexible porous film layer comprises a polymeric porous sheet, and the polymeric porous sheet has a thickness H of 50 μm to 2,000 μm and a density of 100 kg/m3 to 900 kg/m3;
the number of pores having a Dzd in the range of 5 μm to 50 μm account for 80% or more of the total number of pores in the polymeric porous sheet, where Dzd is defined as the maximum pore diameter of a single pore in the thickness direction;
Hp/H is 5%-60%, where Hp is defined as the average value of the cumulative thickness of the polymer matrix excluding pores in the thickness direction, and H is defined as the thickness of the polymeric porous sheet; and
the dielectric strength of the polymeric porous sheet in the thickness direction is 10 to 60 MV/m.

### Claim 2 (depends on 1)

The multilayer piezoelectret film element according to claim 1, wherein the other side of the first conductive layer opposite to the flexible porous film layer is further provided with a base support layer, and the other side of the second conductive layer opposite to the flexible porous film layer is further provided with an overcoat layer.

### Claim 3 (depends on 1)

The multilayer piezoelectret film element according to claim 1, wherein the pores in the polymeric porous sheet contain gas, and the gas comprises one or more selected from air, nitrogen, oxygen, argon, carbon dioxide, fluorine gas, chlorine gas, and water vapor; and/or
the flexible porous film layer is formed by subjecting the polymeric porous sheet to electric polarization and surface metallization treatment.

### Claim 4

A polymeric porous sheet, wherein the polymeric porous sheet has a thickness H of 50 μm to 2,000 μm and a density of 100 kg/m3 to 900 kg/m3;
the number of pores having a Dzd in the range of 5 μm to 50 μm account for 80% or more of the total number of pores in the polymeric porous sheet, where Dzd is defined as the maximum pore diameter of a single pore in the thickness direction;
Hp/H is 5%-60%, where Hp is defined as the average value of the cumulative thickness of the polymer matrix excluding pores in the thickness direction, and H is defined as the thickness of the polymeric porous sheet; and
the dielectric strength of the polymeric porous sheet in the thickness direction is 10 to 60 MV/m.

### Claim 5 (depends on 4)

The polymeric porous sheet according to claim 4, wherein the polymeric porous sheet comprises at least a polypropylene-based resin.

### Claim 6 (depends on 4)

The polymeric porous sheet according to claim 4, wherein the polymeric porous sheet is made from at least a base resin, the base resin is a blended resin obtained by melt blending of a composition comprising two or more polyolefin resins but not subjected to crosslinking and foaming, and the base resin has a dielectric constant of 2.2 to 2.4 and a melting peak temperature of 135° C. to 150° C.

### Claim 7 (depends on 6)

The polymeric porous sheet according to claim 6, wherein the base resin for the polymeric porous sheet has a standard crosslinking degree of 40% to 80% at a radiation dose of 25 Mrad.

### Claim 8 (depends on 4)

The polymeric porous sheet according to claim 4, wherein the polymeric porous sheet is a crosslinked foamed sheet, and the polymeric porous sheet has a crosslinking degree of 10% to 70%.

### Claim 9 (depends on 4)

The polymeric porous sheet according to claim 4, wherein the polymeric porous sheet comprises a xylene-soluble portion and a xylene-insoluble portion; wherein in the DSC curve of the soluble portion, the ratio of the peak area of a melting temperature above 130° C. to the total peak area is 10% to 40%.

### Claim 10 (depends on 4)

The polymeric porous sheet according to claim 4, wherein the polymeric porous sheet has a dimensional change rate of −5% to 5% at 60° C.

### Claim 11 (depends on 4)

The polymeric porous sheet according to claim 4, wherein the polymeric porous sheet has an elongation at break greater than 100%, and a compressive stress at 10% of 5 kPa to 150 kPa.

### Claim 12 (depends on 4)

A method for manufacturing a polymeric porous sheet according to claim 4, comprising subjecting at least a base resin to extrusion molding, electron beam radiation crosslinking, foaming at atmospheric pressure and a high temperature, bidirectional stretching, and calendering, to manufacture the polymeric porous sheet;
wherein the base resin is a blended resin obtained by melt blending of a composition comprising two or more polyolefin resins but not subjected to crosslinking and foaming; the base resin has a dielectric constant of 2.2 to 2.4 and a melting peak temperature of 135° C. to 150° C.; and the base resin has a standard crosslinking degree of 40% to 80% at a radiation dose of 25 Mrad.