# US 2026/0084349 A1 · Bipolar plate production method, bipolar plate and electromechanical cell

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0084349 A1
- Document ID: US20260084349A1
- Status: Published application
- Kind: A1
- Application number: 19/109,840
- Filed: 2023-07-19
- Published: 2026-03-26
- Earliest claimed: 2022-09-09
- Assignees: Schaeffler Technologies AG & Co. KG
- Applicants: SCHAEFFLER Technologies AG & CO. KG
- Inventors: Roland Karpinski; Heiko Ballmes; Philipp Mayer; Torsten Keller
- Web page: https://patentgrep.com/patent/US20260084349A1

## CPC

- B29C 43/021: {characterised by the shape of the surface}
- H01M 8/0213: Gas-impermeable carbon-containing materials
- H01M 8/0221: Organic resins; Organic polymers
- H01M 8/0226: in the form of mixtures
- H01M 8/0247: characterised by the form (characterised by a channel configuration H01M8/0258)
- H01M 8/0254: corrugated or undulated
- H01M 8/0267: having heating or cooling means, e.g. heaters or coolant flow channels
- H01M 8/0297: Arrangements for joining electrodes, reservoir layers, heat exchange units or bipolar separators to each other (H01M8/0271 takes precedence)
- B29L 2031/3468: {Batteries, accumulators or fuel cells (battery cases B29L2031/7146)}
- Y02E 60/50: Fuel cells
- B29C: SHAPING OR JOINING OF PLASTICS; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDED FOR; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING (making preforms B29B11/00; making laminated products by combining previously unconnected layers which become one product whose layers will remain together B32B37/00 - B32B41/00)
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- B29L: INDEXING SCHEME ASSOCIATED WITH SUBCLASS B29C, RELATING TO PARTICULAR ARTICLES
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

The disclosure relates to a bipolar plate production method for producing a bipolar plate, in particular for an electrochemical cell, which method comprises the following steps: providing two foil sections made of a polymer graphite material comprising at least one polymer and at least 75 wt. % of an electrically conductive filler comprising predominantly graphite and also carbon black, inserting the two foil sections into an embossing and molding tool, closing the tool, wherein the foil sections are embossed and tightly connected to one another at their edges, forming a hollow structure between the foil sections by means of gas pressure differences at the foil surfaces, wherein the foil sections rest against surface structures of tool surfaces, which face one another, of the embossing and molding tool, removing the bipolar plate, formed from the foil sections, from the embossing and molding tool after the foil sections have solidified.

## Claims

### Claim 1

A bipolar plate production method for producing a bipolar plate for an electrochemical cell, the method having the following steps:
providing two foil sections made of a polymer graphite material comprising at least one polymer and at least 75 wt. % of an electrically conductive filler comprising predominantly graphite and also carbon black,
inserting the two foil sections into an embossing and molding tool, closing the tool, wherein the foil sections are embossed and tightly connected to one another at their edges,
forming a hollow structure between the foil sections with gas pressure differences at the foil surfaces, wherein the foil sections rest against surface structures of tool surfaces, which face one another, of the embossing and molding tool,
removing the bipolar plate formed from the foil sections, from the embossing and molding tool after the foil sections have solidified.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the foil sections with a maximum foil thickness of 0.5 mm and an electrical conductivity of at least 20 S/cm (at 20 to 24° C.) are used.

### Claim 3 (depends on 1)

The method according to claim 1 wherein the foil sections are heated before being inserted into the tool.

### Claim 4 (depends on 1)

The method according to claim 1, wherein the foil sections are sucked onto the surface structures of the tool surfaces by negative pressure.

### Claim 5 (depends on 4)

The method according to claim 4, wherein the suction of the foil sections is supported by tempered compressed air introduced between the foil sections.

### Claim 6 (depends on 4)

The method according to claim 4, wherein the solidification of the bipolar plate is at least partly caused by cooling air which is introduced between the foil sections.

### Claim 7 (depends on 1)

The method according to claim 1, wherein the foil sections are materially bonded to one another immediately upon closing of the embossing and molding tool.

### Claim 8 (depends on 1)

The method according to claim 1, wherein the foil sections are only materially bonded together after their final shaping by partial heating of the tool with the aid of gas pressure differences acting in the tool.

### Claim 9 (depends on 1)

A bipolar plate manufactured according to the method of claim 1, having at least one channel-shaped, hollow structure for fluid passage through the bipolar plate.

### Claim 10 (depends on 9)

An electrochemical cell comprising at least one bipolar plate according to claim 9.