# US 2026/0084248 A1 · Laser machining method and wafer manufacturing method

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0084248 A1
- Document ID: US20260084248A1
- Status: Published application
- Kind: A1
- Application number: 19/403,480
- Filed: 2025-11-28
- Published: 2026-03-26
- Earliest claimed: 2023-05-29
- Assignees: Dinso Corporation
- Applicants: Dinso Corporation
- Inventors: Ryota TAKAGI; Koichiro Yasuda; Gaku Shimogori; Yuto Takeuchi; Tomoki Kawazu
- Web page: https://patentgrep.com/patent/US20260084248A1

## CPC

- B23K 26/032: {using optical means}
- B23K 26/53: for modifying or reforming the material inside the workpiece, e.g. for producing break initiation cracks
- B23K 26/0622: by shaping pulses
- B23K 26/08: Devices involving relative movement between laser beam and workpiece
- B23K 26/082: Scanning systems, i.e. devices involving movement of the laser beam relative to the laser head
- B23K 26/0823: {Devices involving rotation of the workpiece}
- B23K 26/0853: {Devices involving movement of the workpiece in at least two axial directions, e.g. in a plane}
- B28D 5/0011: {with preliminary treatment, e.g. weakening by scoring}
- C30B 29/36: Carbides
- H10P 54/30: by forming weakened zones for subsequent cutting or separating, e.g. by laser treatment or by ion implantation
- H10P 90/12: {Preparing bulk and homogeneous wafers}
- B23K 26/0006: {taking account of the properties of the material involved (B23K26/32, B23K26/40 take precedence)}
- B23K 2101/40: Semiconductor devices
- B23K 2103/56: {being semiconducting}
- B23K: SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM
- B28D: WORKING STONE OR STONE-LIKE MATERIALS
- C30B: SINGLE-CRYSTAL GROWTH (by using ultra-high pressure, e.g. for the formation of diamonds, B01J3/06); UNIDIRECTIONAL SOLIDIFICATION OF EUTECTIC MATERIAL OR UNIDIRECTIONAL DEMIXING OF EUTECTOID MATERIAL; REFINING BY ZONE-MELTING OF MATERIAL (zone-refining of metals or alloys C22B); PRODUCTION OF A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (casting of metals, casting of other substances by the same processes or devices B22D; working of plastics B29; modifying the physical structure of metals or alloys C21D, C22F); SINGLE CRYSTALS OR HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE; AFTER-TREATMENT OF SINGLE CRYSTALS OR A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (for producing semiconductor devices or parts thereof H10); APPARATUS THEREFOR
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

By performing a laser scan, which includes moving an irradiation position of a laser beam along a first direction while irradiating a surface of a machining target with the laser beam, for a plurality of times with changes in position within the surface in a second direction, a plurality of irradiation trajectory lines are formed along the second direction, the second direction being orthogonal to the first direction and defined along the surface, the irradiation trajectory lines being made of irradiation marks of the laser beam and linear along the first direction. In the single laser scan, the irradiation marks are formed at a plurality of irradiation positions by intermittently irradiating with a relative movement of the laser beam relative to the machining target along the first direction, and the irradiation marks formed by the irradiation with the laser beam that precedes are irradiated with the laser beam that follows.

## Claims

### Claim 1

A laser machining method of irradiating a machining target made of a semiconductor material with a laser beam, the method comprising
a modified layer formation in which a modified layer is formed at a predetermined depth from a surface of the machining target by irradiating the surface with the laser beam which is transmissive to the surface, wherein
in the modified layer formation,
by performing a laser scan for a plurality of times with a change in position within the surface in a second direction, a plurality of irradiation trajectory lines are formed along the second direction, the laser scan including irradiating the surface with the laser beam while moving an irradiation position of the laser beam within the surface along a first direction defined along the surface, the second direction being orthogonal to the first direction and defined along the surface, the irradiation trajectory lines being made of irradiation marks of the laser beam and linear along the first direction, and
in a single laser scan, the irradiation marks are formed at a plurality of the respective irradiation positions by intermittently irradiating with the laser beam with a relative movement of the laser beam relative to the machining target along the first direction, and the irradiation marks formed by the irradiation with the laser beam that precedes are irradiated with the laser beam that follows.

### Claim 2 (depends on 1)

The laser machining method according to claim 1, wherein
the laser scan is performed between adjacent ones of the irradiation trajectory lines in the second direction.

### Claim 3 (depends on 1)

The laser machining method according to claim 1, wherein
the machining target is a single crystal SiC having a c-axis and a C-plane that are orthogonal to each other,
the c-axis is defined in a state where a center axis orthogonal to the surface is inclined in an off-angle direction by an off-angle exceeding zero degrees, and
the first direction is parallel to the off-angle direction.

### Claim 4 (depends on 2)

The laser machining method according to claim 2, wherein
a direction of the relative movement is reversed between the single laser scan and the next single laser scan.

### Claim 5 (depends on 1)

The laser machining method according to claim 1, wherein
in the single laser scan, the plurality of irradiation trajectory lines are formed by irradiating the surface with a plurality of the laser beams different at least in the irradiation position in the second direction.

### Claim 6 (depends on 1)

The laser machining method according to claim 1, comprising
controlling an irradiation condition of the laser beam based on a measurement result of a transmittance of the laser beam through the semiconductor material.

### Claim 7 (depends on 6)

The laser machining method according to claim 6, comprising:
obtaining a trend of change in a depth direction of an absorption coefficient of the laser beam in the semiconductor material based on the measurement result; and
determining the irradiation condition based on the obtained trend of change.

### Claim 8 (depends on 6)

The laser machining method according to claim 6, wherein
a measurement pitch for the transmittance is narrower at a boundary portion between a facet region and a non-facet region than at any other portion.

### Claim 9 (depends on 1)

The laser machining method according to claim 1, wherein
the machining target is a single crystal SiC ingot.

### Claim 10

A wafer manufacturing method of obtaining a wafer from an ingot, the method comprising
a separation layer formation in which a separation layer is formed at a depth corresponding to a thickness of the wafer from a surface of the ingot on one end side in a height direction by irradiating the surface with a laser beam which is transmissive to the surface, wherein
in the separation layer formation,
the separation layer is formed by performing a laser scan for a plurality of times with a change in position within the surface in a second direction to form a plurality of irradiation trajectory lines along the second direction, the laser scan including irradiating the surface with the laser beam while moving an irradiation position of the laser beam within the surface along a first direction defined along the surface, the second direction being orthogonal to the first direction and defined along the surface, the irradiation trajectory lines being made of irradiation marks of the laser beam and linear along the first direction, and
in a single laser scan, the irradiation marks are formed at a plurality of the respective irradiation positions by intermittently irradiating with the laser beam with a relative movement of the laser beam relative to the ingot along the first direction, and the irradiation marks formed by the irradiation with the laser beam that precedes are irradiated with the laser beam that follows.

### Claim 11 (depends on 10)

The wafer manufacturing method according to claim 10, wherein
the laser scan is performed between adjacent ones of the irradiation trajectory lines in the second direction.

### Claim 12 (depends on 10)

The wafer manufacturing method according to claim 10, wherein
the ingot is a single crystal SiC ingot having a c-axis and a C-plane that are orthogonal to each other,
the c-axis is defined in a state where a center axis orthogonal to the surface is inclined in an off-angle direction by an off-angle exceeding zero degrees, and
the first direction is parallel to the off-angle direction.

### Claim 13 (depends on 11)

The wafer manufacturing method according to claim 11, wherein
a direction of the relative movement is reversed between the single laser scan and the next single laser scan.

### Claim 14 (depends on 10)

The wafer manufacturing method according to claim 10, wherein
in the single laser scan, the plurality of irradiation trajectory lines are formed by irradiating the surface with a plurality of the laser beams different at least in the irradiation position in the second direction.

### Claim 15 (depends on 10)

The wafer manufacturing method according to claim 10, comprising
controlling an irradiation condition of the laser beam based on a measurement result of a transmittance of the laser beam through a material forming the ingot.

### Claim 16 (depends on 15)

The wafer manufacturing method according to claim 15, comprising:
obtaining a trend of change in the height direction of an absorption coefficient of the laser beam in the material based on the measurement result; and
determining the irradiation condition based on the obtained trend of change.

### Claim 17 (depends on 15)

The wafer manufacturing method according to claim 15, wherein
a measurement pitch for the transmittance is narrower at a boundary portion between a facet region and a non-facet region than at any other portion.

### Claim 18 (depends on 1)

The laser machining method according to claim 1, wherein
the laser scan is performed such that DYave/DPave≤5 is satisfied,
where:
DY denotes a local maximum width in the second direction of the modified layer;
DP denotes a local maximum spacing in the first direction, the local maximum spacing being a spacing between the modified layer and adjacent another modified layer at a position corresponding to the local maximum width of the modified layer;
DYave denotes an average value of the local maximum width; and
DPave denotes an average value of the local maximum spacing.

### Claim 19 (depends on 18)

The laser machining method according to claim 18, wherein
the laser scan is performed such that DYave/DPave≤2 is satisfied.

### Claim 20 (depends on 19)

The laser machining method according to claim 19, wherein
the laser scan is performed such that DYave/DPave=0.7 to 1.3 is satisfied.

### Claim 21 (depends on 10)

The wafer manufacturing method according to claim 10, wherein
the laser scan is performed such that DYave/DPave≤5 is satisfied,
where:
DY denotes a local maximum width in the second direction of a modified layer formed inside the ingot by an irradiation with the laser beam;
DP denotes a local maximum spacing in the first direction, the local maximum spacing being a spacing between the modified layer and adjacent another modified layer at a position corresponding to the local maximum width of the modified layer;
DYave denotes an average value of the local maximum width; and
DPave denotes an average value of the local maximum spacing.

### Claim 22 (depends on 21)

The wafer manufacturing method according to claim 21, wherein
the laser scan is performed such that DYave/DPave≤2 is satisfied.

### Claim 23 (depends on 22)

The wafer manufacturing method according to claim 22, wherein
the laser scan is performed such that DYave/DPave=0.7 to 1.3 is satisfied.

### Claim 24

A laser machining method of irradiating a machining target made of a semiconductor material with a laser beam, the method comprising
a modified layer formation in which a modified layer is formed at a predetermined depth from a surface of the machining target by irradiating the surface with the laser beam which is transmissive to the surface, wherein
in the modified layer formation,
by performing a laser scan for a plurality of times with a change in position within the surface in a second direction, a plurality of irradiation trajectory lines are formed along the second direction, the laser scan including irradiating the surface with the laser beam while moving an irradiation position of the laser beam within the surface along a first direction defined along the surface, the second direction being orthogonal to the first direction and defined along the surface, the irradiation trajectory lines being made of irradiation marks of the laser beam and linear along the first direction, and
in a single laser scan, the irradiation marks are formed at a plurality of the respective irradiation positions by intermittently irradiating with the laser beam with a relative movement of the laser beam relative to the machining target along the first direction, and a portion between a pair of the irradiation marks formed by an irradiation with a preceding beam and arrayed along the first direction is subjected to an irradiation with a following beam, the preceding beam being the laser beam that precedes, the following beam being the laser beam that follows.

### Claim 25 (depends on 24)

The laser machining method according to claim 24, wherein
in the single laser scan, the irradiation with the preceding beam and the irradiation with the following beam are performed such that the irradiation marks formed by the irradiation with the preceding beam and the irradiation marks to be formed by the irradiation with the following beam are joined.

### Claim 26 (depends on 24)

The laser machining method according to claim 24, wherein
the single laser scan includes relatively moving two of the laser beams different in position in the first direction with respect to the machining target, the two laser beams being the preceding beam and the following beam.

### Claim 27 (depends on 26)

The laser machining method according to claim 26, wherein
the irradiation with the preceding beam and the irradiation with the following beam are simultaneously performed.

### Claim 28 (depends on 24)

The laser machining method according to claim 24, wherein
in the single laser scan, the plurality of irradiation trajectory lines are formed by irradiating the surface with a plurality of the preceding beams and the following beams, the plurality of the preceding beams and the following beams being different in the irradiation position in the second direction.

### Claim 29 (depends on 1)

The laser machining method according to claim 1, wherein
the irradiation marks are each formed by a modified region and a crack, the modified region being generated by a modification of the semiconductor material through an irradiation with the laser beam, the crack originating at the modified region, and
the crack includes a first-type crack developing in a direction inclined with respect to the surface by an off-angle and a second-type crack having an inclination closer to the surface than the first-type crack.

### Claim 30

A wafer manufacturing method of obtaining a wafer from an ingot, the method comprising
a separation layer formation in which a separation layer is formed at a depth corresponding to a thickness of the wafer from a surface of the ingot on one end side in a height direction by irradiating the surface with a laser beam which is transmissive to the surface,
wherein
in the separation layer formation,
the separation layer is formed by performing a laser scan for a plurality of times with a change in position within the surface in a second direction to form a plurality of irradiation trajectory lines along the second direction, the laser scan including irradiating the surface with the laser beam while moving an irradiation position of the laser beam within the surface along a first direction defined along the surface, the second direction being orthogonal to the first direction and defined along the surface, the irradiation trajectory lines being made of irradiation marks of the laser beam and linear along the first direction, and
in a single laser scan, the irradiation marks are formed at a plurality of the respective irradiation positions by intermittently irradiating with the laser beam with a relative movement of the laser beam relative to the ingot along the first direction, and a portion between a pair of the irradiation marks formed by an irradiation with a preceding beam and arrayed along the first direction is subjected to an irradiation with a following beam, the preceding beam being the laser beam that precedes, the following beam being the laser beam that follows.

### Claim 31 (depends on 30)

The wafer manufacturing method according to claim 30, wherein
in the single laser scan, the irradiation with the preceding beam and the irradiation with the following beam are performed such that the irradiation marks formed by the irradiation with the preceding beam and the irradiation marks to be formed by the irradiation with the following beam are joined.

### Claim 32 (depends on 30)

The wafer manufacturing method according to claim 30, wherein
the single laser scan includes relatively moving two of the laser beams different in position in the first direction with respect to the ingot, the two laser beams being the preceding beam and the following beam.

### Claim 33 (depends on 32)

The wafer manufacturing method according to claim 32, wherein
the irradiation with the preceding beam and the irradiation with the following beam are simultaneously performed.

### Claim 34 (depends on 30)

The wafer manufacturing method according to claim 30, wherein
in the single laser scan, the plurality of irradiation trajectory lines are formed by irradiating the surface with a plurality of the preceding beams and the following beams, the plurality of the preceding beams and the following beams being different in the irradiation position in the second direction.

### Claim 35 (depends on 10)

The wafer manufacturing method according to claim 10, wherein
the irradiation marks are each formed of a modified region and a crack, the modified region being generated by a modification of a semiconductor material through an irradiation with the laser beam, the crack originating at the modified region, and
the crack includes a first-type crack developing in a direction inclined with respect to the surface by an off-angle and a second-type crack having an inclination closer to the surface than the first-type crack.