# US 2026/0084096 A1 · High capacity carbon dioxide absorbent solvent resistant to oxidative degradation

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0084096 A1
- Document ID: US20260084096A1
- Status: Published application
- Kind: A1
- Application number: 19/408,359
- Filed: 2025-12-04
- Published: 2026-03-26
- Earliest claimed: 2023-01-17
- Assignees: Scd Co., Ltd.
- Applicants: Scd Inc
- Inventors: Safieh Karimi Vardanjini
- Web page: https://patentgrep.com/patent/US20260084096A1

## CPC

- B01D 53/1493: {Selection of liquid materials for use as absorbents}
- B01D 53/1475: {Removing carbon dioxide}
- B01D 53/62: Carbon oxides
- B01D 53/78: with gas-liquid contact
- B01D 2251/306: of potassium
- B01D 2251/604: Hydroxides
- B01D 2252/20478: Alkanolamines
- B01D 2252/20484: with one hydroxyl group
- B01D 2252/604: Stabilisers or agents inhibiting degradation
- B01D 2257/504: Carbon dioxide
- B01D 2258/0233: from cement factories
- B01D 2258/025: from metallurgy plants
- B01D 2258/0283: Flue gases
- Y02C 20/40: of CO2
- B01D: SEPARATION (separating solids from solids by wet methods B03B, B03D; by pneumatic jigs or tables B03B; by other dry methods B07; magnetic or electrostatic separation of solid materials from solid materials or fluids, separation by high-voltage electric fields B03C; centrifuges, vortex apparatus B04; presses per se for squeezing-out liquid from liquid-containing material B30B9/02; treatment of water C02F, e.g. softening by ion-exchange C02F1/42; {arrangements of air intake cleaners in gas turbine plants F02C7/05} ; arrangements or mounting of filters in air-conditioning, air-humidification or ventilation F24F13/28)
- Y02C: CAPTURE, STORAGE, SEQUESTRATION OR DISPOSAL OF GREENHOUSE GASES [GHG]

## Abstract

An oxidation resistant absorbent for capturing carbon dioxide from a gas stream. The oxidation resistant absorbent includes an alkanolamine with a weight percent in a range of 10 wt. % to 35 wt. % to a total amount of the oxidation resistant absorbent, a base with a weight percent in a range of 1 wt. % to 15 wt. % to a total amount of the oxidation resistant absorbent, a plurality of nanoparticles with a weight percent in a range of 0.1 wt. % to 3 wt. % to a total amount of the oxidation resistant absorbent, and water.

## Claims

### Claim 1

An oxidation resistant absorbent for capturing carbon dioxide from a gas stream, the oxidation resistant absorbent comprising:
an alkanolamine comprising Monoethanolamine (MEA) with a weight percent of 30 wt. % to a total amount of the oxidation resistant absorbent;
an alkali comprising Potassium hydroxide (KOH) with a weight percent of 5 wt. % to a total amount of the oxidation resistant absorbent;
a plurality of nanoparticles, each respective nanoparticle comprising a silica nanoparticle coated with a layer of alumina, the plurality of nanoparticles being present in the oxidation resistant absorbent with a weight percent of 1.2 wt. % to a total amount of the oxidation resistant absorbent,
wherein a remaining weight percent of the oxidation resistant absorbent consists of water.

### Claim 2

An oxidation resistant absorbent for capturing carbon dioxide from a gas stream, the oxidation resistant absorbent comprising:
an alkanolamine with a weight percent in a range of 10 wt. % to 35 wt. % to a total amount of the oxidation resistant absorbent;
a base with a weight percent in a range of 1 wt. % to 15 wt. % to a total amount of the oxidation resistant absorbent; and
a plurality of nanoparticles with a weight percent in a range of 0.1 wt. % to 3 wt. % to a total amount of the oxidation resistant absorbent.

### Claim 3 (depends on 2)

The oxidation resistant absorbent of claim 2, wherein the alkanolamine comprises at least one of Monoethanolamine (MEA), Diethanolamine (DEA), Triethanolamine (TEA), Methyldiethanolamine (MDEA), Diisopropanolamine (DIPA), Diglycolamine (DGA), and combinations thereof.

### Claim 4 (depends on 3)

The oxidation resistant absorbent of claim 3, wherein the alkanolamine comprises MEA with a weight percent of 30 wt. % to a total amount of the oxidation resistant absorbent.

### Claim 5 (depends on 2)

The oxidation resistant absorbent of claim 2, wherein the base comprises at least one of a salt of an alkali metal, a salt of an alkaline earth metal, and combinations thereof.

### Claim 6 (depends on 5)

The oxidation resistant absorbent of claim 5, wherein the base comprises at least one of Potassium hydroxide (KOH), Potassium carbonate (K2CO3), Sodium hydroxide (NaOH), Sodium carbonate (Na2CO3), and combinations thereof.

### Claim 7 (depends on 6)

The oxidation resistant absorbent of claim 6, wherein the base comprises KOH with a weight percent of 5 wt. % to a total amount of the oxidation resistant absorbent.

### Claim 8 (depends on 2)

The oxidation resistant absorbent of claim 2, wherein the plurality of nanoparticles comprises a plurality of alumina-coated silica nanoparticles, each respective alumina-coated silica nanoparticle comprising a silica nanoparticle coated with a layer of alumina.

### Claim 9 (depends on 2)

The oxidation resistant absorbent of claim 2, further comprising water, wherein a remaining weight percent of the oxidation resistant absorbent comprises water.

### Claim 10

A method for fabricating an oxidation resistant absorbent for capturing carbon dioxide from a gas stream, the method comprising:
forming a first solution by dissolving an alkanolamine in water at a temperature in a range of 25° C. to 30° C. and a pressure of 1 bar;
forming a second solution by adding a base to the first solution at a temperature in a range of 25° C. to 30° C. and a pressure of 1 bar, adding the base to the first solution comprising dissolving the base in the first solution; and
adding a plurality of nanostructured material to the second solution, comprising:
forming a mixture of the plurality of nanostructured material and the second solution by mixing the plurality of nanostructured material with the second solution in a vessel at a temperature in a range of 25° C. to 30° C. and a pressure of 1 bar; and
dispersing the plurality of nanostructured material in the second solution, comprising:
increasing a pressure of the mixture of the plurality of nanostructured material and the second solution up to 200 bar utilizing a supersonic jet pump; and
recycling the pressurized mixture of the plurality of nanostructured material and the second solution into the vessel.

### Claim 11 (depends on 10)

The method of claim 10, wherein the alkanolamine comprises at least one of Monoethanolamine (MEA), Diethanolamine (DEA), Triethanolamine (TEA), Methyldiethanolamine (MDEA), Diisopropanolamine (DIPA), Diglycolamine (DGA), and combinations thereof.

### Claim 12 (depends on 10)

The method of claim 10, wherein the alkanolamine is present in the formed oxidation resistant absorbent with a weight percent in a range of 10 wt. % to 35 wt. % to a total amount of the oxidation resistant absorbent.

### Claim 13 (depends on 10)

The method of claim 10, wherein the alkanolamine comprises MEA with a weight percent of 30 wt. % to a total amount of the oxidation resistant absorbent.

### Claim 14 (depends on 10)

The method of claim 10, wherein the base comprises at least one of a salt of an alkali metal, a salt of an alkaline earth metal, and combinations thereof.

### Claim 15 (depends on 10)

The method of claim 10, wherein the base comprises at least one of Potassium hydroxide (KOH), Potassium carbonate (K2CO3), Sodium hydroxide (NaOH), Sodium carbonate (Na2CO3), and combinations thereof.

### Claim 16 (depends on 10)

The method of claim 10, wherein the base is present in the formed oxidation resistant absorbent with a weight percent in a range of 1 wt. % to 15 wt. % to a total amount of the oxidation resistant absorbent.

### Claim 17 (depends on 10)

The method of claim 10, wherein the base comprises KOH with a weight percent of 5 wt. % to a total amount of the oxidation resistant absorbent.

### Claim 18 (depends on 10)

The method of claim 10, wherein the plurality of nanoparticles comprises a plurality of alumina-coated silica nanoparticles, each respective alumina-coated silica nanoparticle comprising a silica nanoparticle coated with a layer of alumina.

### Claim 19 (depends on 10)

The method of claim 10, wherein the plurality of nanoparticles is present in the formed oxidation resistant absorbent with a weight percent in a range of 0.1 wt. % to 3 wt. % to a total amount of the oxidation resistant absorbent.