# US 2026/0083882 A1 · Heat shrink tube

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0083882 A1
- Document ID: US20260083882A1
- Status: Published application
- Kind: A1
- Application number: 19/086,581
- Filed: 2025-03-21
- Published: 2026-03-26
- Earliest claimed: 2024-09-20
- Assignees: Zeus Co., Ltd.
- Applicants: Zeus Company LLC
- Inventors: Zeth John Eberling; Tyler Austin Poole; Josh G. Fogle
- Web page: https://patentgrep.com/patent/US20260083882A1

## CPC

- A61L 29/06: obtained otherwise than by reactions only involving carbon-to-carbon unsaturated bonds
- A61L 29/14: Materials characterised by their function or physical properties {, e.g. lubricating compositions}
- B29C 61/08: by stretching tubes {(in general B29C55/22, B29C55/28)}
- B29C 63/42: using tubular layers or sheathings
- A61L: METHODS OR APPARATUS FOR STERILISING MATERIALS OR OBJECTS IN GENERAL; DISINFECTION, STERILISATION OR DEODORISATION OF AIR; CHEMICAL ASPECTS OF BANDAGES, DRESSINGS, ABSORBENT PADS OR SURGICAL ARTICLES; MATERIALS FOR BANDAGES, DRESSINGS, ABSORBENT PADS OR SURGICAL ARTICLES (preservation of bodies or disinfecting characterised by the agents employed A01N; preserving, e.g. sterilising, food or foodstuffs A23; preparations for medical, dental or toiletry purposes A61K)
- B29C: SHAPING OR JOINING OF PLASTICS; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDED FOR; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING (making preforms B29B11/00; making laminated products by combining previously unconnected layers which become one product whose layers will remain together B32B37/00 - B32B41/00)

## Abstract

The present disclosure provides tubings including at least one amorphous polymer resin. The tubings can exhibit heat shrink capability and, optionally, translucency or transparency through a wall of the tubing. After heating to recover the tubings, they can advantageously release cleanly from any underlying materials with which they are in intimate contact. The disclosure further provides methods of making and using such tubings and various applications for such tubings.

## Claims

### Claim 1

A heat shrink tubing for recovery over a polymer substrate, wherein the heat shrink tubing comprises at least one amorphous polymer resin,
wherein the heat shrink tubing exhibits a recovery temperature and a Vicat softening temperature and the polymer substrate exhibits a melting point such that:
a. a first delta (ΔTO) between the melting point of the polymer substrate and an onset point of the recovery temperature of the heat shrink tubing is a positive value; and
b. a second delta (ΔVO) between the Vicat softening temperature of the heat shrink tubing and the onset point of the recovery temperature of the heat shrink tubing is a positive value.

### Claim 2 (depends on 1)

The heat shrink tubing of claim 1, wherein the at least one amorphous polymer resin is a non-fluorinated amorphous polymer.

### Claim 3 (depends on 1)

The heat shrink tubing of claim 1, comprising no fluorinated polymer.

### Claim 4 (depends on 1)

The heat shrink tubing of claim 1, that exhibits translucency or transparency.

### Claim 5 (depends on 1)

The heat shrink tubing of claim 1, wherein the tubing comprises no more than one amorphous polymer resin.

### Claim 6 (depends on 5)

The heat shrink tubing of claim 5, wherein the no more than one amorphous polymer is selected from the group consisting of poly(etherimide) (PEI), poly(imide) (PI), poly(carbonate) (PC), poly(siloxane), poly(sulfone) (PSU), poly(ethersulfone) (PESU), poly(phenylene sulfone) (PPSU), polyetherimide siloxane (PEI-Sil) copolymer, and copolymers and derivatives of any one or more thereof.

### Claim 7 (depends on 1)

The heat shrink tubing of claim 1, wherein the tubing comprises two or more amorphous polymer resins.

### Claim 8 (depends on 7)

The heat shrink tubing of claim 7, wherein the two or more amorphous polymer resins comprise:
a first amorphous polymer resin selected from the group consisting of poly(etherimide) (PEI), poly(imide) (PI), poly(carbonate) (PC), poly(siloxane), poly(sulfone) (PSU), poly(ethersulfone) (PESU), poly(phenylene sulfone) (PPSU), and copolymers, blends, and derivatives of any combination thereof; and
a second amorphous polymer resin selected from the group consisting of poly(etherimide) (PEI), poly(imide) (PI), poly(carbonate) (PC), poly(siloxane), poly(sulfone) (PSU), poly(ethersulfone) (PESU), poly(phenylene sulfone) (PPSU), polyetherimide siloxane (PEI-Sil) copolymer, and other copolymers, blends, and derivatives of any combination thereof.

### Claim 9 (depends on 1)

The heat shrink tubing of claim 1, consisting essentially of the at least one amorphous polymer resin.

### Claim 10 (depends on 1)

The heat shrink tubing of claim 1, further comprising one or more additives.

### Claim 11 (depends on 1)

The heat shrink tubing of claim 1, wherein the tubing exhibits longitudinal peelability.

### Claim 12 (depends on 11)

The heat shrink tubing of claim 11, wherein the longitudinal peelability does not require a physical score line or cut or embedded physical component to promote the longitudinal peelability or wherein the longitudinal peelability requires a physical score line, cut, or nick that is less than about 1/50th the length of the tubing.

### Claim 13 (depends on 1)

The heat shrink tubing of claim 1, wherein the tubing has an average wall thickness of less than 0.02 inches.

### Claim 14 (depends on 13)

The heat shrink tubing of claim 13, wherein the average wall thickness is 0.002 inches to 0.01 inches.

### Claim 15 (depends on 13)

The heat shrink tubing of claim 13, wherein the average wall thickness is 0.004 inches to 0.0099 inches.

### Claim 16 (depends on 1)

A catheter assembly comprising the heat shrink tubing of claim 1.

### Claim 17 (depends on 1)

A construction, comprising a recovered heat shrink tubing comprising the heat shrink tubing of claim 1 recovered over the polymer substrate, wherein the polymer substrate is in reflowed form.

### Claim 18 (depends on 17)

The construction of claim 17, wherein the polymer substrate exhibits a coefficient of variation (CoV) of its outer diameter (OD) of 0.005 or less.

### Claim 19 (depends on 17)

The construction of claim 17, wherein the recovered heat shrink tubing exhibits a longitudinal to radial percent shrinkage heat shrink ratio of 0.5 or less with respect to the heat shrink tubing.

### Claim 20 (depends on 17)

The construction of claim 17, wherein the recovered heat shrink tubing exhibits contact clarity through to the polymer substrate.

### Claim 21 (depends on 17)

The construction of claim 17, wherein the recovered heat shrink tubing has an average wall thickness of 0.001 to 0.028 inches.

### Claim 22 (depends on 21)

The construction of claim 21, wherein the average wall thickness is obtained when subjected to unrestricted recovery at 420° F. for five minutes.

### Claim 23

A method of preparing a heat shrink tubing for recovery over a polymer substrate, comprising:
selecting a heat shrink tubing material comprising at least one amorphous polymer resin that exhibits a recovery temperature and a Vicat softening temperature; and
selecting a polymer substrate material that exhibits a melting point,
wherein the recovery temperature, Vicat softening temperature, and melting point are such that:
a. a first delta (ΔTO) between the melting point of the polymer substrate and an onset point of the recovery temperature of the heat shrink tubing is a positive value; and
b. a second delta (ΔVO) between the Vicat softening temperature of the heat shrink tubing and the onset point of the recovery temperature of the heat shrink tubing is a positive value.