# US 2026/0083680 A1 · Mesoporous nano-magnesium oxide for drug loading and preparation method thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0083680 A1
- Document ID: US20260083680A1
- Status: Published application
- Kind: A1
- Application number: 19/302,131
- Filed: 2025-08-18
- Published: 2026-03-26
- Earliest claimed: 2024-09-24
- Assignees: Shanghai Institute of Technology
- Applicants: Shanghai Institute of Technology
- Inventors: Chun XU
- Web page: https://patentgrep.com/patent/US20260083680A1

## CPC

- A61K 9/5115: {Inorganic compounds}
- C01F 5/06: by thermal decomposition of magnesium compounds (calcining magnesite or dolomite C04B2/10)
- A61K 9/5192: {Processes}
- A61K 9/143: {with inorganic compounds}
- A61K: PREPARATIONS FOR MEDICAL, DENTAL OR TOILETRY PURPOSES (devices or methods specially adapted for bringing pharmaceutical products into particular physical or administering forms A61J3/00; chemical aspects of, or use of materials for deodorisation of air, for disinfection or sterilisation, or for bandages, dressings, absorbent pads or surgical articles A61L; soap compositions C11D)
- C01F: COMPOUNDS OF THE METALS BERYLLIUM, MAGNESIUM, ALUMINIUM, CALCIUM, STRONTIUM, BARIUM, RADIUM, THORIUM, OR OF THE RARE-EARTH METALS (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts of peroxyacids C01B15/00; sulfides or polysulfides of magnesium, calcium, strontium, or barium C01B17/42; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds other than ammonia or cyanogen containing nitrogen and non-metals and optionally metals C01B21/082; amides or imides of silicon C01B21/087}; metal {imides or} amides C01B21/092, {C01B21/0923}; nitrites C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; compounds having molecular sieve properties but not having base-exchange properties C01B37/00; compounds having molecular sieve and base-exchange properties, e.g. crystalline zeolites, C01B39/00; cyanides C01C3/08; salts of cyanic acid C01C3/14; salts of cyanamide C01C3/16; thiocyanates C01C3/20; {double sulfates of magnesium with sodium or potassium C01D5/12; with other alkali metals C01D15/00, C01D17/00})

## Abstract

A mesoporous nano-magnesium oxide for drug loading and a preparation method thereof are provided. The mesoporous nano-magnesium oxide particle has a particle size of 50 nm to 150 nm, and includes abundant mesoporous structures with a pore size of 2 nm to 20 nm. A surface of the particle has a positive potential in absolute ethanol, with a Zeta potential distribution of 10 mV to 100 mV. The preparation method includes: preparing a mixture of magnesium oxalate and CTAB as a precursor; adding the precursor to a quartz crucible, and placing the quartz crucible in a muffle furnace; calcining at 200℃ for 1 h to make the CTAB in the mixture completely decomposed to produce pure magnesium oxalate; and heating to 530°C, and calcining for 1 h to 6 h to make the magnesium oxalate fully decomposed to produce the nano-magnesium oxide microparticle.

## Claims

### Claim 1

A mesoporous nano-magnesium oxide for drug loading, wherein a particle of the mesoporous nano-magnesium oxide for the drug loading has a particle size of 50 nm to 150 nm and comprises abundant mesoporous structures on a surface of the particle of the mesoporous nano-magnesium oxide with a pore size of 2 nm to 20 nm.

### Claim 2 (depends on 1)

The mesoporous nano-magnesium oxide for the drug loading according to claim 1, wherein the surface of the particle of the mesoporous nano-magnesium oxide for the drug loading has a positive potential in absolute ethanol, with a Zeta potential distribution of 10 mV to 100 mV.

### Claim 3 (depends on 1)

A preparation method of the mesoporous nano-magnesium oxide for the drug loading according to claim 1, comprising the following steps:
(1) a preparation of a magnesium oxalate precursor:
with magnesium chloride hexahydrate as a magnesium source, oxalic acid dihydrate as a precipitating agent, a mixture of deionized water and n-butanol as a solvent, cetyltrimethylammonium bromide (CTAB) as a dispersing agent, and acetic acid added to increase a hydrogen ion concentration, conducting a co-precipitation reaction to synthesize the magnesium oxalate precursor, wherein the magnesium oxalate precursor is a mixture of magnesium oxalate and the CTAB; and
(2) a preparation of a nano-magnesium oxide microparticle
adding the magnesium oxalate precursor to a quartz crucible, and placing the quartz crucible in a muffle furnace; calcining at 200℃ for 1 h to make the CTAB in the mixture completely decomposed to produce pure magnesium oxalate; and heating to 530°C, and calcining for 1 h to 6 h to make the pure magnesium oxalate fully decomposed to produce the nano-magnesium oxide microparticle.

### Claim 4 (depends on 3)

The preparation method of the mesoporous nano-magnesium oxide for the drug loading according to claim 3, wherein a concentration ratio of the magnesium chloride hexahydrate to the oxalic acid dihydrate is (1-3):(1-3); and the mixture of the deionized water and the n-butanol in a volume ratio of (1-3):(1-3) is added.

### Claim 5 (depends on 3)

The preparation method of the mesoporous nano-magnesium oxide for the drug loading according to claim 3, wherein during the co-precipitation reaction, 0.25 wt% to 1.25 wt% of the CTAB and the acetic acid with a concentration of 36% to 50% are added to improve a dispersibility of the magnesium oxalate.

### Claim 6 (depends on 3)

The preparation method of the mesoporous nano-magnesium oxide for the drug loading according to claim 3, wherein a process for preparing the magnesium oxalate precursor is as follows: placing a beaker with a predetermined amount of the solvent in a water bath; when a temperature of the solvent reaches a predetermined reaction temperature, adding a specified concentration ratio of the magnesium chloride hexahydrate and a predetermined amount of the CTAB, thoroughly stirring, and adding specified amounts of the oxalic acid dihydrate and the acetic acid; using an alcohol and the deionized water as detergents; conducting decantation multiple times, and retaining a lower precipitate; and oven-drying to produce the magnesium oxalate precursor.

### Claim 7 (depends on 6)

The preparation method of the mesoporous nano-magnesium oxide for the drug loading according to claim 6, wherein the predetermined reaction temperature is 40°C to 80°C, and a reaction time is 20 min to 60 min; the stirring is continuously conducted for 20 min under heating with a magnetic stirrer at a rotational speed of 100 r/min to 1,000 r/min; and after the decantation is conducted multiple times, the oven-drying is conducted at 90°C to 100°C for 1 h.

### Claim 8 (depends on 3)

The preparation method of the mesoporous nano-magnesium oxide for the drug loading according to claim 3, wherein with a decomposition of the pure magnesium oxalate, a gas is released from a surface of the nano-magnesium oxide microparticle to form a large number of mesopores and micropores, with an average pore size of 14 nm and a pore size distribution of 2 nm to 20 nm.

### Claim 9 (depends on 3)

The preparation method of the mesoporous nano-magnesium oxide for the drug loading according to claim 3, wherein the surface of the particle of the mesoporous nano-magnesium oxide for the drug loading has a positive potential in absolute ethanol, with a Zeta potential distribution of 10 mV to 100 mV.

### Claim 10 (depends on 9)

The preparation method of the mesoporous nano-magnesium oxide for the drug loading according to claim 9, wherein a concentration ratio of the magnesium chloride hexahydrate to the oxalic acid dihydrate is (1-3.):(1-3.); and the mixture of the deionized water and the n-butanol in a volume ratio of (1-3.):(1-3.) is added.

### Claim 11 (depends on 9)

The preparation method of the mesoporous nano-magnesium oxide for the drug loading according to claim 9, wherein during the co-precipitation reaction, 0.25 wt% to 1.25 wt% of the CTAB and the acetic acid with a concentration of 36% to 50% are added to improve a dispersibility of the magnesium oxalate.

### Claim 12 (depends on 9)

The preparation method of the mesoporous nano-magnesium oxide for the drug loading according to claim 9, wherein a process for preparing the magnesium oxalate precursor is as follows: placing a beaker with a predetermined amount of the solvent in a water bath; when a temperature of the solvent reaches a predetermined reaction temperature, adding a predetermined molar mass of the magnesium chloride hexahydrate and a predetermined amount of the CTAB, thoroughly stirring, and adding predetermined amounts of the oxalic acid dihydrate and the acetic acid; using an alcohol and the deionized water as detergents; conducting decantation multiple times, and retaining a lower precipitate; and oven-drying to produce the magnesium oxalate precursor.

### Claim 13 (depends on 12)

The preparation method of the mesoporous nano-magnesium oxide for the drug loading according to claim 12, wherein the predetermined reaction temperature is 40°C to 80°C, and a reaction time is 20 min to 60 min; the stirring is continuously conducted for 20 min under heating with a magnetic stirrer at a rotational speed of 100 r/min to 1,000 r/min; and after the decantation is conducted multiple times, the oven-drying is conducted at 90°C to 100°C for 1 h.

### Claim 14 (depends on 9)

The preparation method of the mesoporous nano-magnesium oxide for the drug loading according to claim 9, wherein with a decomposition of the pure magnesium oxalate, a gas is released from a surface of the nano-magnesium oxide microparticle to form a large number of mesopores and micropores, with an average pore size of 14 nm and a pore size distribution of 2 nm to 20 nm.