# US 2026/0082824 A1 · Resistive random-access memory devices with engineered electronic defects and methods for making the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0082824 A1
- Document ID: US20260082824A1
- Status: Published application
- Kind: A1
- Application number: 19/300,643
- Filed: 2025-08-14
- Published: 2026-03-19
- Earliest claimed: 2020-07-06
- Assignees: TetraMem Inc.
- Applicants: TetraMem Inc.
- Inventors: Minxian Zhang; Ning Ge
- Web page: https://patentgrep.com/patent/US20260082824A1

## CPC

- G11C 13/0007: {comprising metal oxide memory material, e.g. perovskites}
- H10N 70/023: {by chemical vapor deposition, e.g. MOCVD, ALD}
- H10B 63/80: {Arrangements comprising multiple bistable or multi-stable switching components of the same type on a plane parallel to the substrate, e.g. cross-point arrays}
- H10N 70/011: {Manufacture or treatment of multistable switching devices}
- H10N 70/026: {by physical vapor deposition, e.g. sputtering}
- H10N 70/24: {based on migration or redistribution of ionic species, e.g. anions, vacancies}
- H10N 70/826: {adapted for essentially vertical current flow, e.g. sandwich or pillar type devices}
- H10N 70/828: {Current flow limiting means within the switching material region, e.g. constrictions}
- H10N 70/841: {Electrodes}
- H10N 70/8833: {Binary metal oxides, e.g. TaOx}
- G11C 2213/32: Material having simple binary metal oxide structure
- G11C 2213/50: Resistive cell structure aspects
- G11C 2213/52: Structure characterized by the electrode material, shape, etc.
- G11C 2213/79: Array wherein the access device being a transistor
- H10B 63/30: {comprising selection components having three or more electrodes, e.g. transistors}
- G11C: STATIC STORES (semiconductor memory devices H10B)
- H10N: ELECTRIC SOLID-STATE DEVICES NOT OTHERWISE PROVIDED FOR
- H10B: ELECTRONIC MEMORY DEVICES

## Abstract

The present disclosure relates to resistive random-access memory (RRAM) devices. A method for fabricating resistive random-access memory (RRAM) device may include fabricating, on a first electrode of the RRAM device, a first interface layer comprising a first discontinuous film of a first material; fabricating, on the first interface layer, a switching oxide layer comprising at least one transition metal oxide; fabricating a second interface layer on the switching oxide layer; and fabricating a defect engineering layer on the second interface layer. The first material is more chemically stable than the at least one transition metal oxide. The defect engineering layer includes a layer of Ti in some embodiments.

## Claims

### Claim 1

A method for fabricating resistive random-access memory (RRAM) device, the method comprising:
fabricating an interface layer on a switching oxide layer, wherein the switching oxide layer comprises at least one transition metal oxide, and wherein the interface layer comprises a discontinuous film of a material that is more chemically stable than the at least one transition metal oxide; and
fabricating, on the interface layer, a defect engineering layer for generating electronic defects in the switching oxide layer, comprising:
fabricating, on the interface layer, a first layer of a first metallic material, wherein at least a portion of the first layer of the first metallic material is deposited on the switching oxide layer through the interface layer; and
fabricating, on the first layer of the first metallic material, a second layer of a second metallic material.

### Claim 2 (depends on 1)

The method of claim 1, further comprising fabricating the switching oxide layer on a first electrode.

### Claim 3 (depends on 1)

The method of claim 1, wherein the at least one transition metal oxide comprises at least one of HfOx or TaOy, wherein x≤2.0, and wherein y≤2.5.

### Claim 4 (depends on 3)

The method of claim 3, wherein the material that is more chemically stable than the at least one metal oxide comprises at least one of Al2O3, MgO, Y2O3, or La2O3.

### Claim 5 (depends on 1)

The method of claim 1, wherein fabricating the first layer of the first metallic material on the second interface layer comprises fabricating, on the second interface layer, a layer of titanium; and wherein fabricating, on the first layer of the first metallic material, the second layer of the second metallic material comprises depositing the second metallic material on the layer of titanium.

### Claim 6 (depends on 1)

The method of claim 1, wherein the material is more chemically stable than an oxide of the first metallic material and the at least one transition metal oxide.

### Claim 7 (depends on 1)

The method of claim 1, wherein the first metallic material comprises at least one of Ti, Hf, or Zr.

### Claim 8 (depends on 7)

The method of claim 7, wherein the second metallic material comprises tantalum.

### Claim 9 (depends on 8)

The method of claim 8, wherein the second layer of the second metallic material comprises one or more alloys containing tantalum.

### Claim 10

A resistive random-access memory (RRAM) device, comprising:
a first electrode;
a switching oxide layer fabricated on the first electrode, wherein the switching oxide layer comprises at least one transition metal oxide;
an interface layer fabricated on a switching oxide layer, wherein the interface layer comprises a discontinuous film of a material that is more chemically stable than the at least one transition metal oxide; and
a defect engineering layer for generating electronic defects in the switching oxide layer, wherein the defect engineering layer comprises:
a first layer of a first metallic material, wherein at least a portion of the first layer of the first metallic material is deposited on the switching oxide layer through the interface layer; and
a second layer of a second metallic material on the first layer of the first metallic material.

### Claim 11 (depends on 10)

The RRAM device of claim 10, wherein a thickness of the interface layer is between 0.2 nm and 1 nm.

### Claim 12 (depends on 10)

The RRAM device of claim 10, wherein the at least one transition metal oxide comprises at least one of HfOx or TaOy, wherein x≤2.0, and wherein y≤2.5, and wherein the material that is more chemically stable than the at least one metal oxide comprises at least one of Al2O3, MgO, Y2O3, or La2O3.

### Claim 13 (depends on 10)

The RRAM device of claim 10, wherein the defect engineering layer directly contacts at least a portion of the switching oxide layer.

### Claim 14 (depends on 10)

The RRAM device of claim 10, wherein the second layer of the second metallic material does not contact the switching oxide layer.

### Claim 15 (depends on 10)

The RRAM device of claim 10, wherein the first layer of the first metallic material comprises a layer of titanium.

### Claim 16 (depends on 10)

The RRAM of claim 10, wherein the first metallic material comprises at least one of Ti, Hf, or Zr.

### Claim 17 (depends on 16)

The RRAM device of claim 16, wherein the material of the interfaced layer is more chemically stable than an oxide of the first metallic material and the at least one transition metal oxide.

### Claim 18 (depends on 16)

The RRAM device of claim 16, wherein the second metallic material comprises tantalum.

### Claim 19 (depends on 18)

The RRAM device of claim 18, wherein the second layer of the second metallic material comprises one or more alloys containing tantalum.

### Claim 20 (depends on 10)

The RRAM device of claim 10, wherein the electronic defects comprise oxygen vacancy defects in the at least one transition metal oxide.