# US 2026/0081068 A1 · Method for preparation of severely plastically deformed particulates for manganese-aluminum-based alloy permanent magnets

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0081068 A1
- Document ID: US20260081068A1
- Status: Published application
- Kind: A1
- Application number: 18/818,930
- Filed: 2024-08-29
- Published: 2026-03-19
- Earliest claimed: 2023-09-01
- Assignees: University of Pittsburgh—Of the Commonwealth System of Higher Education
- Applicants: University of Pittsburgh-of the Commonwealth System of Higher Education
- Inventors: JORG M. WIEZOREK; RAVI SHANKAR MEENAKSHISUNDARAM
- Web page: https://patentgrep.com/patent/US20260081068A1

## CPC

- H01F 41/0253: {for manufacturing permanent magnets}
- B22F 1/142: Thermal or thermo-mechanical treatment
- C22C 1/04: by powder metallurgy (C22C1/08 takes precedence)
- C22F 1/02: in inert or controlled atmosphere or vacuum (adjusting the composition of the atmosphere C21D1/76)
- C22F 1/16: of other metals or alloys based thereon
- H01F 1/047: Alloys characterised by their composition
- B22F 9/04: starting from solid material, e.g. by crushing, grinding or milling ({C22C1/1084 takes precedence}; crushing, grinding or milling, in general, see the relevant subclasses, e.g. B02C)
- B22F 2009/001: {from scrap particles}
- B22F 2009/045: {by other means than ball or jet milling}
- B22F 2301/00: Metallic composition of the powder or its coating
- C22C 2202/02: Magnetic
- H01F: MAGNETS; INDUCTANCES; TRANSFORMERS; SELECTION OF MATERIALS FOR THEIR MAGNETIC PROPERTIES
- B22F: WORKING METALLIC POWDER; MANUFACTURE OF ARTICLES FROM METALLIC POWDER; MAKING METALLIC POWDER (making alloys by powder metallurgy C22C); APPARATUS OR DEVICES SPECIALLY ADAPTED FOR METALLIC POWDER
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- C22F: CHANGING THE PHYSICAL STRUCTURE OF NON-FERROUS METALS AND NON-FERROUS ALLOYS (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass, C23F17/00)

## Abstract

A method of manufacturing permanent magnet materials for use in making MnAl-based alloy permanent magnets includes providing an ε-phase MnAl-based alloy solid feedstock, end-milling the ε-phase MnAl-based alloy solid feedstock to produce a plurality of severely plastically deformed ε-phase MnAl-based alloy particulates, and creating the permanent magnet materials by thermally processing the plurality of ε-phase MnAl-based alloy particulates to produce a plurality of τ-phase MnAl-based alloy particulates. In addition, the method may further include making a permanent magnet by mixing the τ-phase MnAl-based alloy particulates with a binder to produce a mixture, and forming the mixture into a desired shaped for the permanent magnet. The forming step may include one or more of injection molding the mixture, compression bonding the mixture, calendering the mixture or extruding the mixture.

## Claims

### Claim 1

A method of manufacturing permanent magnet materials for use in making MnAl-based alloy permanent magnets, comprising:
providing an ε-phase MnAl-based alloy solid feedstock;
end-milling the ε-phase MnAl-based alloy solid feedstock to produce a plurality of severely plastically deformed ε-phase MnAl-based alloy particulates; and
creating the permanent magnet materials by thermally processing the plurality of ε-phase MnAl-based alloy particulates to produce a plurality of τ-phase MnAl-based alloy particulates.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the plurality of ε-phase MnAl-based alloy particulates have a refined microstructure having a sub-micron (<1 μm) to nanometer scale (≤100 nm) grain size.

### Claim 3 (depends on 2)

The method according to claim 2, wherein the microstructure comprises a self-similar morphology.

### Claim 4 (depends on 1)

The method according to claim 1, wherein the ε-phase MnAl-based alloy solid feedstock is a binary ε-phase MnAl alloy solid feedstock, wherein the ε-phase MnAl-based alloy particulates are ε-phase MnAl alloy particulates, and wherein the τ-phase MnAl-based alloy particulates are τ-phase MnAl alloy particulates.

### Claim 5 (depends on 1)

The method according to claim 1, wherein the ε-phase MnAl-based alloy solid feedstock is a micro-alloyed ε-phase MnAl—X alloy solid feedstock, where X represents one or more micro-alloying elements, wherein the ε-phase MnAl-based alloy particulates are micro-alloyed ε-phase MnAl-X alloy particulates, and wherein the τ-phase MnAl-based alloy particulates are micro-alloyed τ-phase MnAl—X alloy particulates.

### Claim 6 (depends on 5)

The method according to claim 5, where X represents one or more micro-alloying elements at concentrations smaller than 3 atomic (molar) percent.

### Claim 7 (depends on 1)

The method according to claim 1, wherein the end milling is performed at room temperature.

### Claim 8 (depends on 1)

The method according to claim 1, wherein the ε-phase MnAl-based alloy solid feedstock has a composition of 54 at. % Mn and 46 at. % Al.

### Claim 9 (depends on 1)

The method according to claim 1, wherein the thermally processing comprises thermal annealing.

### Claim 10 (depends on 9)

The method according to claim 9, wherein the thermal annealing comprises isothermal annealing at temperatures ranging from 673 K to 723 K.

### Claim 11 (depends on 9)

The method according to claim 9, wherein the thermal annealing is performed under vacuum.

### Claim 12 (depends on 11)

The method according to claim 11, wherein the thermal annealing is performed under vacuum with a 10 K/s heating rate and subsequent isothermal annealing holds at 623 K, 673 K, 698 K, and 723 K.

### Claim 13 (depends on 9)

The method according to claim 9, wherein the end milling is performed with a tool speed of 4200 RPM and wherein the thermal annealing comprises annealing for 20 min at 673K.

### Claim 14 (depends on 1)

The method according to claim 1, wherein the end milling is performed with stage speeds ranging from 1 mm/s to 13 mm/s, radial depths of cut, rc, ranging from 0.05 mm to 0.5 mm, axial depths of cut, ac, ranging from 0.1 mm to 0.2 mm, and spindle/tool rotational speeds in the range of 100 rotations per minute (RPM) to 3000 RPM for manual end-milling and 750 RPM to 4200 RPM for CNC end-milling.

### Claim 15 (depends on 14)

The method according to claim 14, wherein the stage speeds are ≥10 mm/s, the rotational spindle/tool speeds are ≥600 RPM, and the radial depth of cut, rc is ≤0.1 mm.

### Claim 16 (depends on 14)

The method according to claim 14, wherein the end milling is performed with a rotational tool speed of 3000 RPM using a 13 mm/s stage speed and constant radial depths of cut of 0.05 mm and constant axial depths of cut of 0.1 mm.

### Claim 17 (depends on 1)

The method according to claim 1, wherein the end milling is performed with a fluted chamfer end mill cutting tool.

### Claim 18 (depends on 1)

The method according to claim 1, wherein the end milling is performed with a flute fine tooth roughing end mill cutting tool.

### Claim 19 (depends on 1)

The method according to claim 1, wherein the ε-phase MnAl-based alloy particulates have a saw-tooth-like appearance at a free surface thereof not in contact with a cutting tool used in the end-milling.

### Claim 20 (depends on 1)

The method according to claim 1, wherein the providing the ε-phase MnAl-based alloy solid feedstock comprises vacuum induction melting of elemental metal Mn and Al followed by casting into a number of cylindrical rods with a target composition of Mn54Al46.

### Claim 21 (depends on 20)

The method according to claim 20, wherein the providing the ε-phase MnAl-based alloy solid feedstock further comprises sectioning the rods into a number of sectioned pieces and solutionizing the number of sectioned pieces to produce the ε-phase MnAl alloy solid feedstock.

### Claim 22 (depends on 21)

The method according to claim 21, wherein the solutionizing comprises heat treating the sectioned pieces.

### Claim 23 (depends on 22)

The method according to claim 22, wherein the solutionizing comprises heat treating the sectioned pieces under an argon atmosphere.

### Claim 24 (depends on 22)

The method according to claim 22, wherein the solutionizing comprises heat treating the sectioned pieces at 1323 K (1050° C.).

### Claim 25 (depends on 24)

The method according to claim 24, wherein the solutionizing comprises heat treating the sectioned pieces at 1323 K (1050° C.) for 2 hours.

### Claim 26 (depends on 22)

The method according to claim 22, wherein the solutionizing comprises heat treating the sectioned pieces followed by water quenching.

### Claim 27 (depends on 19)

The method according to claim 19, wherein the vacuum induction melting of elemental metal Mn and Al is done with a purity of 99.95%.

### Claim 28 (depends on 1)

The method according to claim 1, wherein the end-milling the ε-phase MnAl-based alloy solid feedstock to produce the plurality of severely plastically deformed ε-phase MnAl-based alloy particulates is done in a single end milling pass.

### Claim 29 (depends on 1)

A method of making a permanent magnet, comprising:
making permanent magnet materials according to claim 1 including the τ-phase MnAl-based alloy particulates;
mixing the τ-phase MnAl-based alloy particulates with a binder to produce a mixture; and
forming the mixture into a desired shaped for the permanent magnet.

### Claim 30 (depends on 29)

The method according to claim 29, wherein the forming includes one or more of injection molding the mixture, compression bonding the mixture, calendering the mixture or extruding the mixture.