# US 2026/0081056 A1 · Method for producing grain-oriented electrical steel sheet, and induction heating device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0081056 A1
- Document ID: US20260081056A1
- Status: Published application
- Kind: A1
- Application number: 19/108,555
- Filed: 2023-09-05
- Published: 2026-03-19
- Earliest claimed: 2022-09-06
- Assignees: Jfe Steel Corporation
- Applicants: JFE Steel Corporation
- Inventors: Yusuke SHIMOYAMA; Yukihiro SHINGAKI; Takashi TERASHIMA
- Web page: https://patentgrep.com/patent/US20260081056A1

## CPC

- H01F 1/14783: {with insulating coating}
- B21B 1/26: by hot-rolling {, e.g. Steckel hot mill}
- B21B 1/28: by cold-rolling {, e.g. Steckel cold mill}
- C21D 1/26: Methods of annealing
- C21D 3/04: Decarburising
- C21D 6/001: {containing Ni (C21D6/004 takes precedence)}
- C21D 6/002: {containing Cr (C21D6/004 takes precedence)}
- C21D 6/005: {containing Mn}
- C21D 6/008: {containing Si}
- C21D 8/1222: {Hot rolling}
- C21D 8/1233: {Cold rolling}
- C21D 8/1255: {with diffusion of elements, e.g. decarburising, nitriding}
- C21D 8/1261: {following hot rolling}
- C21D 8/1266: {between cold rolling steps}
- C21D 9/46: for sheet metals
- C22C 38/001: {containing N}
- C22C 38/002: {containing In, Mg, or other elements not provided for in one single group C22C38/001 - C22C38/60}
- C22C 38/008: {containing tin}
- C22C 38/02: containing silicon
- C22C 38/04: containing manganese
- C22C 38/06: containing aluminium
- C22C 38/08: containing nickel {(C22C38/105 takes precedence)}
- C22C 38/12: containing tungsten, tantalum, molybdenum, vanadium, or niobium
- C22C 38/16: containing copper
- C22C 38/20: with copper
- C22C 38/22: with molybdenum or tungsten
- C22C 38/34: with more than 1.5% by weight of silicon
- C22C 38/60: containing lead, selenium, tellurium, or antimony, or more than 0.04% by weight of sulfur
- H01F 1/147: Alloys characterised by their composition {(treatment thereof for enhancing their electromagnetic properties C21D8/12)}
- H01F 1/16: in the form of sheets (H01F1/147 takes precedence)
- H05B 6/101: {for local heating of metal pieces}
- H05B 6/104: {metal pieces being elongated like wires or bands}
- H05B 6/40: Establishing desired heat distribution, e.g. to heat particular parts of workpieces
- C21D 1/42: Induction heating
- C21D 8/1272: {Final recrystallisation annealing}
- C21D 8/1283: {Application of a separating or insulating coating}
- C21D 2201/05: Grain orientation
- C22C 2202/02: Magnetic
- H01F: MAGNETS; INDUCTANCES; TRANSFORMERS; SELECTION OF MATERIALS FOR THEIR MAGNETIC PROPERTIES
- B21B: ROLLING OF METAL (auxiliary operations used in connection with metal-working operations covered in B21, see B21C; bending by rolling B21D; manufacture of particular objects, e.g. screws, wheels, rings, barrels, balls, by rolling B21H; pressure welding by means of a rolling mill B23K20/04)
- C21D: MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass C23F17/00; unidirectional solidification of eutectic materials or unidirectional demixing of eutectoid materials C30B)
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- H05B: ELECTRIC HEATING; ELECTRIC LIGHT SOURCES NOT OTHERWISE PROVIDED FOR; CIRCUIT ARRANGEMENTS FOR ELECTRIC LIGHT SOURCES, IN GENERAL

## Abstract

A method for producing a grain-oriented electrical steel sheet is disclosed including hot rolling a steel material to obtain a hot-rolled sheet, subjecting the hot-rolled sheet to one cold-rolling step, or two or more cold-rolling steps with intermediate annealing interposed between each cold-rolling step so as to obtain a cold-rolled sheet with a final thickness, and subjecting the cold-rolled sheet to decarburization annealing which also serves as primary recrystallization annealing and then to finishing annealing, in which the decarburization annealing includes a heating step in which the steel sheet is rapidly heated at an average heating rate of 250° C./s or more from 400° C. to a temperature T(° C.) of 700 to 900° C. and then held at a heating rate of ⅔ of the average heating rate or less in any of temperature ranges between 500° C. and 700° C. for a time of 0.10 seconds or more but less than 1.00 seconds.

## Claims

### Claim 1

A method for producing a grain-oriented electrical steel sheet, comprising:
hot rolling a steel material to obtain a hot-rolled sheet;
subjecting the hot-rolled sheet to one cold-rolling step, or two or more cold-rolling steps with intermediate annealing interposed between each cold-rolling step so as to obtain a cold-rolled sheet with a final thickness; and
subjecting the cold-rolled sheet to decarburization annealing which also serves as primary recrystallization annealing and then to finishing annealing,
characterized in that
the decarburization annealing includes a heating step in which the steel sheet is rapidly heated at an average heating rate of 250° C./s or more from 400° C. to a temperature T(° C.) of 700 to 900° C. and then held at a heating rate of ⅔ of the average heating rate or less in any of temperature ranges between 500° C. and 700° C. for a time of 0.10 seconds or more but less than 1.00 seconds.

### Claim 2 (depends on 1)

The method for producing a grain-oriented electrical steel sheet according to claim 1, wherein
the steel material has a component composition containing elements of a following group A or B, with a balance being Fe and unavoidable impurities:
group A: C: 0.01 to 0.10 mass %, Si: 2.0 to 4.5 mass %, Mn: 0.01 to 0.50 mass %, Al: 0.0100 to 0.0400 mass %, N: 0.0050 to 0.0120 mass %, and at least one of S and Se: a total of 0.01 to 0.05 mass %, and
group B: C: 0.01 to 0.10 mass %, Si: 2.0 to 4.5 mass %, Mn: 0.01 to 0.50 mass %, Al: less than 0.0100 mass %, N: 0.0050 mass % or less, S: 0.0070 mass % or less, and Se: 0.0070 mass % or less.

### Claim 3 (depends on 2)

The method for producing a grain-oriented electrical steel sheet according to claim 2, wherein
the steel material further contains, in addition to the component composition, at least one element selected from the group consisting of Sb: 0.500 mass % or less, Cu: 1.50 mass % or less, P: 0.500 mass % or less, Cr: 1.50 mass % or less, Ni: 1.500 mass % or less, Sn: 0.50 mass % or less, Nb: 0.0100 mass % or less, Mo: 0.50 mass % or less, B: 0.0070 mass % or less, and Bi: 0.0500 mass % or less.

### Claim 4 (depends on 1)

The method for producing a grain-oriented electrical steel sheet according to claim 1, wherein
the rapid heating in the decarburization annealing is performed using a transverse induction heating device.

### Claim 5 (depends on 4)

A transverse induction heating device for use in the method for producing a grain-oriented electrical steel sheet according to claim 4, comprising
a heating coil having a shape of a rounded rectangle including two parallel lines of equal length lying along a sheet width direction, and two semicircles, wherein
relationships of R1≥w and R2<v are satisfied, where R1 represents a maximum inner diameter (m) of the heating coil in the sheet width direction, R2 represents a maximum inner diameter (m) of the heating coil in a threading direction, w represents a width (m) of the steel sheet, and v represents a threading speed (m/s) of the steel sheet.

### Claim 6 (depends on 2)

The method for producing a grain-oriented electrical steel sheet according to claim 2, wherein
the rapid heating in the decarburization annealing is performed using a transverse induction heating device.

### Claim 7 (depends on 3)

The method for producing a grain-oriented electrical steel sheet according to claim 3, wherein
the rapid heating in the decarburization annealing is performed using a transverse induction heating device.

### Claim 8 (depends on 6)

A transverse induction heating device for use in the method for producing a grain-oriented electrical steel sheet according to claim 6, comprising a heating coil having a shape of a rounded rectangle including two parallel lines of equal length lying along a sheet width direction, and two semicircles, wherein
relationships of R1≥w and R2<v are satisfied, where R1 represents a maximum inner diameter (m) of the heating coil in the sheet width direction, R2 represents a maximum inner diameter (m) of the heating coil in a threading direction, w represents a width (m) of the steel sheet, and v represents a threading speed (m/s) of the steel sheet.

### Claim 9 (depends on 7)

A transverse induction heating device for use in the method for producing a grain-oriented electrical steel sheet according to claim 7, comprising a heating coil having a shape of a rounded rectangle including two parallel lines of equal length lying along a sheet width direction, and two semicircles, wherein
relationships of R1≥w and R2<v are satisfied, where R1 represents a maximum inner diameter (m) of the heating coil in the sheet width direction, R2 represents a maximum inner diameter (m) of the heating coil in a threading direction, w represents a width (m) of the steel sheet, and v represents a threading speed (m/s) of the steel sheet.