# US 2026/0078522 A1 · Group iii nitride single crystal growth method

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0078522 A1
- Document ID: US20260078522A1
- Status: Published application
- Kind: A1
- Application number: 19/317,770
- Filed: 2025-09-03
- Published: 2026-03-19
- Earliest claimed: 2024-09-17
- Assignees: Toyoda Gosei Co., Ltd.; The University of Osaka
- Applicants: Toyoda Gosei Co., Ltd.; The University of Osaka
- Inventors: Taku FUJIMORI; Miki MORIYAMA; Yusuke MORI; Masayuki IMANISHI; Shigeyoshi USAMI
- Web page: https://patentgrep.com/patent/US20260078522A1

## CPC

- C30B 19/02: using molten solvents, e.g. flux
- C30B 29/403: {AIII-nitrides}
- C30B 19/04: the solvent being a component of the crystal composition
- C30B 19/12: characterised by the substrate
- C30B 29/406: {Gallium nitride}
- C30B: SINGLE-CRYSTAL GROWTH (by using ultra-high pressure, e.g. for the formation of diamonds, B01J3/06); UNIDIRECTIONAL SOLIDIFICATION OF EUTECTIC MATERIAL OR UNIDIRECTIONAL DEMIXING OF EUTECTOID MATERIAL; REFINING BY ZONE-MELTING OF MATERIAL (zone-refining of metals or alloys C22B); PRODUCTION OF A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (casting of metals, casting of other substances by the same processes or devices B22D; working of plastics B29; modifying the physical structure of metals or alloys C21D, C22F); SINGLE CRYSTALS OR HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE; AFTER-TREATMENT OF SINGLE CRYSTALS OR A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (for producing semiconductor devices or parts thereof H10); APPARATUS THEREFOR

## Abstract

A Group III nitride single crystal growth method is a method for growing a Group III nitride single crystal on a Group III nitride substrate, and includes: repeatedly performing, to form a thickened Group III nitride single crystal on the Group III nitride substrate, a process of: immersing the Group III nitride substrate in a mixed melt containing a Group III metal and Na stored in a crucible; pulling up the Group III nitride substrate from the mixed melt; and heating the Group III nitride substrate, pulled up from the mixed melt, in a nitrogen atmosphere, and the crucible is an alumina crucible containing alumina as a main component and containing an alkali metal other than Na or an alkaline earth metal.

## Claims

### Claim 1

A Group III nitride single crystal growth method, which is a method for growing a Group III nitride single crystal on a Group III nitride substrate, the method comprising:
a thickening step of repeatedly performing, to form a thickened Group III nitride single crystal on the Group III nitride substrate, a process of: immersing the Group III nitride substrate in a mixed melt containing a Group III metal and Na stored in a crucible; pulling up the Group III nitride substrate from the mixed melt; and heating the Group III nitride substrate, pulled up from the mixed melt, in a nitrogen atmosphere, wherein
the crucible is an alumina crucible containing alumina as a main component and containing an alkali metal other than Na or an alkaline earth metal.

### Claim 2 (depends on 1)

The Group III nitride single crystal growth method according to claim 1, wherein the alkali metal other than Na or the alkaline earth metal melted from the crucible in the thickening step is mixed in the mixed melt at a ratio of 0.01 mol % to less than 0.05 mol %.

### Claim 3 (depends on 1)

The Group III nitride single crystal growth method according to claim 1, wherein in the thickening step, an immersion time, which is a time for immersing the Group III nitride substrate in the mixed melt, is within a range of 1 minute to 10 minutes, and a vapor phase heating time, which is a time for heating the Group III nitride substrate in the nitrogen atmosphere after being pulled up from the mixed melt, is within a range of 10 minutes to 120 minutes.

### Claim 4 (depends on 2)

The Group III nitride single crystal growth method according to claim 2, wherein in the thickening step, an immersion time, which is a time for immersing the Group III nitride substrate in the mixed melt, is within a range of 1 minute to 10 minutes, and a vapor phase heating time, which is a time for heating the Group III nitride substrate in the nitrogen atmosphere after being pulled up from the mixed melt, is within a range of 10 minutes to 120 minutes.

### Claim 5 (depends on 1)

The Group III nitride single crystal growth method according to claim 1, further comprising:
an initial nucleus forming step of immersing, in the mixed melt stored in the crucible, a seed substrate having a plurality of seed crystals, made from a Group III nitride single crystal, formed on an upper surface of the seed substrate, to grow a Group III nitride single crystal from the plurality of seed crystals and to form a plurality of initial nuclei; and
a flattening step of repeatedly performing a process of: immersing the seed substrate having the initial nuclei formed thereon in the mixed melt stored in the crucible; pulling up the seed substrate from the mixed melt; and heating the seed substrate, pulled up from the mixed melt, in a nitrogen atmosphere, to grow a Group III nitride single crystal from the initial nuclei, to fill a space between the adjacent ones of the plurality of initial nuclei with the Group III nitride single crystal, so that a crystal surface of the seed substrate is flatten, wherein
in the thickening step, the seed substrate having the flattened crystal surface formed in the flattening step is used as the Group III nitride substrate.

### Claim 6 (depends on 2)

The Group III nitride single crystal growth method according to claim 2, further comprising:
an initial nucleus forming step of immersing, in the mixed melt stored in the crucible, a seed substrate having a plurality of seed crystals, made from a Group III nitride single crystal, formed on an upper surface of the seed substrate, to grow a Group III nitride single crystal from the plurality of seed crystals and to form a plurality of initial nuclei; and
a flattening step of repeatedly performing a process of: immersing the seed substrate having the initial nuclei formed thereon in the mixed melt stored in the crucible; pulling up the seed substrate from the mixed melt; and heating the seed substrate, pulled up from the mixed melt, in a nitrogen atmosphere, to grow a Group III nitride single crystal from the initial nuclei, to fill a space between the adjacent ones of the plurality of initial nuclei with the Group III nitride single crystal, so that a crystal surface of the seed substrate is flatten, wherein
in the thickening step, the seed substrate having the flattened crystal surface formed in the flattening step is used as the Group III nitride substrate.

### Claim 7 (depends on 5)

The Group III nitride single crystal growth method according to claim 5, wherein a ratio of the alkali metal other than Na or the alkaline earth metal in the mixed melt increases in an order of the initial nucleus forming step, the flattening step, and the thickening step.

### Claim 8 (depends on 6)

The Group III nitride single crystal growth method according to claim 6, wherein a ratio of the alkali metal other than Na or the alkaline earth metal in the mixed melt increases in an order of the initial nucleus forming step, the flattening step, and the thickening step.