# US 2026/0078008 A1 · Production of silicon particles having a reduced surface metal content

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0078008 A1
- Document ID: US20260078008A1
- Status: Published application
- Kind: A1
- Application number: 19/106,233
- Filed: 2022-09-22
- Published: 2026-03-19
- Earliest claimed: 2022-09-22
- Assignees: Wacker Chemie AG
- Applicants: Wacker Chemie AG
- Inventors: Marco GRUBER; Rebecca BERNHARD; Sebastian LIEBISCHER; Gerlinde WENSAUER
- Web page: https://patentgrep.com/patent/US20260078008A1

## CPC

- C01B 33/037: Purification (by zone-melting C30B13/00)
- C01P 2004/61: Micrometer sized, i.e. from 1-100 micrometer
- C01P 2006/12: Surface area
- C01P 2006/80: Compositional purity
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS

## Abstract

Silicon chunks with reduced surface metal content and methods for producing the same. Where the method for producing the silicon chunks include the steps of (a) comminuting a silicon ingot or block into silicon chunks, (b) contacting the silicon chunks with at least one preliminary etching bath, comprising 6.6% to 12% by weight of hydrofluoric acid and 40% to 65% by weight of nitric acid, and (c) contacting the silicon chunks with at least one main etching bath, comprising 5.3% to 6.5% by weight of hydrofluoric acid and 40% to 65% by weight of nitric acid.

## Claims

### Claim at position 1

1-17. (canceled)

### Claim 18

A method for producing silicon chunks with reduced surface metal content, comprising the steps of:
a) comminuting a silicon ingot or block into silicon chunks;
b) contacting the silicon chunks with at least one preliminary etching bath, comprising 6.6% to 12% by weight of hydrofluoric acid and 40% to 65% by weight of nitric acid;
c) contacting the silicon chunks with at least one main etching bath, comprising 5.3% to 6.5% by weight of hydrofluoric acid and 40% to 65% by weight of nitric acid.

### Claim 19 (depends on 18)

The method of claim 18, wherein the preliminary etching bath comprises 6.6% to 12%, preferably 7% to 10%, by weight of hydrofluoric acid.

### Claim 20 (depends on 18)

The method of claim 18, wherein the contact time in the preliminary etching bath is 1 to 30 s, preferably 2 to 25 s, more preferably 4 to 20 s.

### Claim 21 (depends on 18)

The method of claim 18, wherein the preliminary etching bath has a temperature of 1 to 60° C., preferably 5 to 50° C., more preferably 8 to 40° C.

### Claim 22 (depends on 18)

The method of claim 18, wherein the temperature of the preliminary etching bath is set in dependence on the chunk size of the silicon chunks, with the temperature being
from 1 to 10° C. for chunk size 2,
from 8 to 60° C. for chunk size 3, and
from 5 to 15° C. for chunk size 4.

### Claim 23 (depends on 18)

The method of claim 18, wherein the at least one main etching bath has a temperature of 1 to 15° C., preferably of 2 to 12° C., more preferably of 4 to 10° C.

### Claim 24 (depends on 18)

The method of claim 18, wherein the silicon chunks are contacted in step c) with a main etching bath, this bath comprising preferably 53% to 65% by weight of nitric acid.

### Claim 25 (depends on 18)

The method of claim 18, wherein the silicon chunks are contacted in step c) with a first and a second main etching bath, the second main etching bath having a higher content of nitric acid.

### Claim 26 (depends on 25)

The method of claim 25, wherein the first main etching bath comprises 40% to 65% by weight of nitric acid and the second main etching bath comprising 53% to 65% by weight of nitric acid.

### Claim 27 (depends on 18)

The method of claim 18, wherein after step c) a further step d) of contacting the silicon chunks with a hydrophilizing bath comprising an ozone-water mixture with 5 to 30 ppm, preferably 7 to 15 ppm, of ozone.

### Claim 28 (depends on 18)

The method of claim 18, wherein after each step or after each of the individual steps a) to c) and/or after step d), the silicon chunks are contacted with an ultrapure water bath.

### Claim 29 (depends on 27)

The method of claim 27, wherein the silicon chunks after step d) are contacted with an ultrapure water bath which has a temperature of 50 to 95° C., preferably of 60 to 90° C.

### Claim 30 (depends on 18)

The method of claim 18, wherein a drying step in which the silicon chunks are dried by convection drying and/or vacuum drying.

### Claim 31 (depends on 30)

The method of claim 30, wherein the drying step comprises a convection drying at 60 to 100° C., preferably at 70 to 90° C., followed by a vacuum drying at 2 to 8 kPa, preferably at 3 to 5 kPa.

### Claim 32

A silicon chunk, comprising:
wherein the silicon chunk has a specific surface area of 1200 to 3500 cm2/kg and a grain size in a range from 4 to 150 mm, which has a surface metal content of <11 pptw, the metals under consideration being as follows: Fe, Cr, Ni, Al, Ca, Ag, Zn, As, Co, Cu, Na, K, Ti, Mg, Mo, Mn, Sn, Ba, Bi, Cd, Li, Pb, Sb, Sr, Tl, U, V, W, Y, Zr and the tungsten content being ≤0.3 pptw.

### Claim 33 (depends on 32)

The silicon chunk of claim 32, wherein the content of Fe, Cr, Ni and W is ≤3 pptw.