# US 2026/0077108 A1 · Medicament-Coated Balloon Coating Solution, Coating Material, Medicament-Coated Balloon, Preparation Method Therefor, and Use Thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0077108 A1
- Document ID: US20260077108A1
- Status: Published application
- Kind: A1
- Application number: 19/103,939
- Filed: 2023-11-10
- Published: 2026-03-19
- Earliest claimed: 2022-11-11
- Assignees: Cardio Navi Medtech (Wuhan) Co., Ltd.
- Applicants: Cardio Navi Medtech (Wuhan) Co., Ltd.
- Inventors: Dan XIONG; Shuangshuang LI; Meng LV; Chao LI; Ying ZHANG
- Web page: https://patentgrep.com/patent/US20260077108A1

## CPC

- A61L 29/08: Materials for coatings
- A61L 29/14: Materials characterised by their function or physical properties {, e.g. lubricating compositions}
- A61L 29/16: Biologically active materials, e.g. therapeutic substances {(A61L29/048 takes precedence)}
- A61M 25/10: Balloon catheters ({A61M25/0125 takes precedence; embolectomy A61B17/22032; retractors A61B17/02;} inflatable balloons for placing stents or stent-grafts A61F2/958 {; stomach balloons for treatment of obesity A61F5/0003; oesophagal tubes A61J15/00})
- A61L 2300/416: Anti-neoplastic or anti-proliferative or anti-restenosis or anti-angiogenic agents, e.g. paclitaxel, sirolimus
- A61L 2300/624: Nanocapsules
- A61L 2300/626: Liposomes, micelles, vesicles
- A61L 2420/02: Methods for coating medical devices
- A61M 2025/105: {having a balloon suitable for drug delivery, e.g. by using holes for delivery, drug coating or membranes}
- A61L: METHODS OR APPARATUS FOR STERILISING MATERIALS OR OBJECTS IN GENERAL; DISINFECTION, STERILISATION OR DEODORISATION OF AIR; CHEMICAL ASPECTS OF BANDAGES, DRESSINGS, ABSORBENT PADS OR SURGICAL ARTICLES; MATERIALS FOR BANDAGES, DRESSINGS, ABSORBENT PADS OR SURGICAL ARTICLES (preservation of bodies or disinfecting characterised by the agents employed A01N; preserving, e.g. sterilising, food or foodstuffs A23; preparations for medical, dental or toiletry purposes A61K)
- A61M: DEVICES FOR INTRODUCING MEDIA INTO, OR ONTO, THE BODY (introducing media into or onto the bodies of animals A61D7/00; means for inserting tampons A61F13/26; devices for administering food or medicines orally A61J; containers for collecting, storing or administering blood or medical fluids A61J1/05); DEVICES FOR TRANSDUCING BODY MEDIA OR FOR TAKING MEDIA FROM THE BODY (surgery A61B; chemical aspects of surgical articles A61L); DEVICES FOR PRODUCING OR ENDING SLEEP OR STUPOR {(Electrotherapy, e.g. producing anaesthesia by the use of alternating or intermittent currents A61N1/36021)}

## Abstract

Provided are a medicament-coated balloon coating solution, a coating material, a medicament-coated balloon, a preparation method therefor, and use thereof. The medicament-coated balloon coating solution comprises an aqueous-phase solvent. The coating solution further comprises a plurality of core-shell structures formed by wrapping a medicament in a phospholipid bilayer. The core-shell structures are dispersed in the aqueous-phase solvent. A core of each core-shell structure comprises a plurality of particles loaded with the medicament. A shell of each core-shell structure is the phospholipid bilayer. The phospholipid bilayer comprises a hydrophilic group in an outer layer and a hydrophobic group in an inner layer. The plurality of particles loaded with the medicament comprise a plurality of nanocrystalline particles comprising the medicament. Nanocrystalline is combined with liposome, such that advantages of two types of medicament carriers are combined. The formed phospholipid bilayer increases the solubility of a poorly soluble medicament on the medicament-coated balloon, the medicament loading capacity is high, the stability of the medicament carriers is good, and the medicament crystal form is stable, such that the medicament release rate is controllable.

## Claims

### Claim 1

A coating solution for drug-coated balloon, characterized in that the coating solution comprises an aqueous solvent, and the coating solution further comprises a plurality of core-shell structures formed by wrapping drugs in a phospholipid bilayer, and the core-shell structures are dispersed in the solvent in aqueous phase, wherein, a core of the core-shell structure comprises a plurality of particles loaded with drugs, and a shell of the core-shell structure is a phospholipid bilayer comprising a hydrophilic group in the outer layer and a hydrophobic group in the inner layer, the plurality of particles loaded with drugs comprises a plurality of nanocrystals particles comprising drugs.

### Claim 2 (depends on 1)

The coating solution according to claim 1, characterized in that the particle size of the core-shell structures is 200 to 900 nm;
preferably, the particle size d50 of the nanocrystals particles is 150 to 900 nm; wherein in the preparation process of nanocrystals particles, a surfactant is used;
preferably, the surfactant is selected from one or more of vitamin E polyethylene glycol succinate, Poloxamer 188, Poloxamer 407, Tyloxapol, docusate sodium, polyoxyl 15-hydroxystearate, polyoxyethylene (40) hydrogenated castor oil, polyoxyethylene (60) hydrogenated castor oil, polyoxyethylene (60) castor oil, polyoxyethylene (40) castor oil, polyoxyethylene (35) castor oil, polyoxyethylene (20) castor oil, polyoxyethylene (10) castor oil, polyethylene glycol hexadecyl octadecyl ether 20, polyethylene glycol hexadecyl octadecyl ether 12, polyoxyethylene monocetyl ether (Ceteth-10), polyoxyethylene (10) lauryl ether (Brij 56), polyoxyethylene (20) lauryl ether (Brij 58), polyoxyethylene (23) lauryl ether (Brij 35), polyoxyethylene (2) lauryl ether (Brij 52), polyoxyethylene (25) oleate (Myrj 49), polyoxyethylene (40) palmitate (Myrj 52), sodium dodecyl sulfate, Tween 80, Tween 60, Tween 40, propylene glycol monolaurate, polyoxyethylene (20) lauryl ether, and polyoxyethylene monocetyl ether;
preferably, the drugs include Sirolimus, Zotarolimus and Everolimus, Tacrolimus, Temsirolimus, Pimecrolimus, Deforolimus, and Ridaforolimus;
preferably, the raw materials for preparing the phospholipid bilayer include phospholipids and cholesterols;
preferably, the phospholipids include one or more of yolk lecithin, soybean phospholipid, hydrogenated yolk lecithin, hydrogenated soybean phospholipid, cephalin, phosphatidylethanolamine, dimyristyl phosphatidylcholine (DMPC), stearamide (SA), sunflower phospholipid, 1,2-diformyl-sn-glycero-3-phosphocholine, 1,2-dipalmitoyl-sn-glycero-3-phosphocholine, 1,2-distearoyl-sn-glycero-3-phosphocholine, 1,2-dioleoyl-sn-glycero-3-phosphocholine, 1,2-dierucoyl-sn-glycero-3-phosphocholine, 1-dipalmitoyl-dioleoyl-sn-glycero-3-phosphocholine, 1,2-diformyl-sn-glycero-3-phospho-rac-glycerol sodium salt, 1,2-dipalmitoyl-sn-glycero-3-phospho-rac-glycerol sodium salt, 1,2-distearoyl-sn-glycero-3-phospho-rac-glycerol sodium salt, 1,2-dioleoyl-sn-glycero-3-phospho-rac-glycerol sodium salt, 1-dipalmitoyl-dioleoyl-sn-glycero-3-phospho-rac-glycerol sodium salt, 1,2-diformyl-sn-glycero-3-phosphoethanolamine, 1,2-dipalmitoyl-sn-glycero-3-phosphoethanolamine, 1,2-distearoyl-sn-glycero-3-phosphoethanolamine, 1,2-dioleoyl-sn-glycero-3-phosphoethanolamine, 1,2-dioleoyl-sn-glycero-3-phospho-L-serine sodium salt, 1,2-dipalmitoyl-sn-glycero-3-phosphate monosodium salt, N-(carbonyl-methoxypolyethylene glycol-5000)-1,2-dipalmitoyl-sn-glycero-3-phosphoethanolamine sodium salt, N-(carbonyl-methoxypolyethylene glycol-2000)-1,2-distearoyl-sn-glycero-4-phosphoethanolamine sodium salt, and 1,2-dioleoyl-3-trimethylpropanyl ammonium chloride;
the cholesterols include cholesterol and DC cholesterol;
preferably, the mass ratio of the phospholipid to cholesterols is 40:1 to 1:2, and more preferably 30:1 to 1:1.

### Claim 3

A coating material for drug-coated balloon, characterized in that the material comprises a plurality of core-shell structures formed by wrapping drugs in a phospholipid bilayer, wherein a core of the core-shell structures comprises a plurality of particles loaded with drugs, and a shell of the core-shell structures is the phospholipid bilayer comprising a hydrophilic group in the outer layer and a hydrophobic group in the inner layer, and the plurality of particles loaded with drugs comprise a plurality of nanocrystals particles comprising drugs.

### Claim 4 (depends on 3)

The material according to claim 3, characterized in that the particle size of the core-shell structures is 200 to 900 nm;
preferably, the particle size d50 of the nanocrystals particles is 150 to 900 nm; in the preparation process of nanocrystals particles, a surfactant is used;
preferably, the surfactant is selected from one or more of vitamin E polyethylene glycol succinate, Poloxamer 188, Poloxamer 407, Tyloxapol, docusate sodium, polyoxyl 15-hydroxystearate, polyoxyethylene (40) hydrogenated castor oil, polyoxyethylene (60) hydrogenated castor oil, polyoxyethylene (60) castor oil, polyoxyethylene (40) castor oil, polyoxyethylene (35) castor oil, polyoxyethylene (20) castor oil, polyoxyethylene (10) castor oil, Polyethylene glycol hexadecyl octadecyl ether 20, polyethylene glycol hexadecyl octadecyl ether 12, polyoxyethylene monocetyl ether (Ceteth-10), polyoxyethylene (10) lauryl ether (Brij 56), polyoxyethylene (20) lauryl ether (Brij 58), polyoxyethylene (23) lauryl ether (Brij 35), polyoxyethylene (2) lauryl ether (Brij 52), polyoxyethylene (25) oleate (Myrj 49), polyoxyethylene (40) palmitate (Myrj 52), sodium dodecyl sulfate, Tween 80, Tween 60, Tween 40, propylene glycol monolaurate, polyoxyethylene (20) lauryl ether, and polyoxyethylene monocetyl ether;
preferably, the drugs include Sirolimus, Zotarolimus and Everolimus, Tacrolimus, Temsirolimus, Pimecrolimus, Deforolimus, and Ridaforolimus;
preferably, the raw materials for preparing the phospholipid bilayer comprise phospholipid and cholesterols; preferably, the phospholipids include one or more of yolk lecithin, soybean phospholipid, hydrogenated yolk lecithin, hydrogenated soybean phospholipid, cephalin, phosphatidylethanolamine, dimyristyl phosphatidylcholine (DMPC), stearamide (SA), sunflower phospholipid, 1,2-diformyl-sn-glycero-3-phosphocholine, 1,2-dipalmitoyl-sn-glycero-3-phosphocholine, 1,2-distearoyl-sn-glycero-3-phosphocholine, 1,2-dioleoyl-sn-glycero-3-phosphocholine, 1,2-dierucoyl-sn-glycero-3-phosphocholine, 1-dipalmitoyl-dioleoyl-sn-glycero-3-phosphocholine, 1,2-diformyl-sn-glycero-3-phospho-rac-glycerol sodium salt, 1,2-dipalmitoyl-sn-glycero-3-phospho-rac-glycerol sodium salt, 1,2-distearoyl-sn-glycero-3-phospho-rac-glycerol sodium salt, 1,2-dioleoyl-sn-glycero-3-phospho-rac-glycerol sodium salt, 1-dipalmitoyl-dioleoyl-sn-glycero-3-phospho-rac-glycerol sodium salt, 1,2-diformyl-sn-glycero-3-phosphoethanolamine, 1,2-dipalmitoyl-sn-glycero-3-phosphoethanolamine, 1,2-distearoyl-sn-glycero-3-phosphoethanolamine, 1,2-dioleoyl-sn-glycero-3-phosphoethanolamine, 1,2-dioleoyl-sn-glycero-3-phospho-L-serine sodium salt, 1,2-dipalmitoyl-sn-glycero-3-phosphate monosodium salt, N-(carbonyl-methoxypolyethylene glycol-5000)-1,2-dipalmitoyl-sn-glycero-3-phosphoethanolamine sodium salt, N-(carbonyl-methoxypolyethylene glycol-2000)-1,2-distearoyl-sn-glycero-4-phosphoethanolamine sodium salt, and 1,2-dioleoyl-3-trimethylpropanyl ammonium chloride;
the cholesterols include cholesterol and DC cholesterol;
preferably, the mass ratio of phospholipid to cholesterols is 40:1 to 1:2, and more preferably 30:1 to 1:1.

### Claim 5 (depends on 1, 2, 3, 4)

A drug-coated balloon, characterized in that the surface of the drug-coated balloon is coated with the coating solution of any of claims 1-2 or the material of any of claims 3-4.

### Claim 6 (depends on 5)

A use of the drug-coated balloon of claim 5 in the treatment of atherosclerosis, stenosis, and/or restenosis of coronary arteries, peripheral vessels, or intracranial artery vessels.

### Claim 7

A preparation method of a coating solution for drug-coated balloon, characterized in that the method comprises the following steps:
(1) preparing a plurality of nanocrystals particles loaded with drugs; the method for preparing the nanocrystals particles comprises: anti-solvent method, high pressure homogenization method or microfluidic method;
(2) accurately weigh cholesterols, phospholipids and solvents in aqueous phase, respectively, and obtain a milky white solution after magnetic stirring;
(3) add nanocrystals particles to the milky white solution, mix well by magnetic stirring to obtain the coating solution for drug-coated balloon;
wherein, the coating solution comprises an aqueous solvent, and the coating solution further comprises a plurality of core-shell structures formed by wrapping drugs in a phospholipid bilayer, the core-shell structures are dispersed in the solvent in aqueous phase, wherein, a core of the core-shell structures comprises a plurality of particles loaded with drugs, and a shell of the core-shell structures is a phospholipid bilayer comprising a hydrophilic group in the outer layer and a hydrophobic group in the inner layer.

### Claim 8 (depends on 7)

A method according to claim 7, characterized in that after Step (3), there is Step (4) for adding a thickener to the above-mentioned solution, and mixing well by magnetic stirring to obtain the coating solution for drug-coated balloon;
preferably, the thickener comprises sodium alginate;
preferably, in Step (2), after magnetic stirring, 5 to 10 times of homogenization are performed by a high pressure homogenizer or a microfluidic device to obtain a milky white solution;
preferably, the drugs in Step S1 include Sirolimus, and the organic solvents include methanol;
preferably, the mass ratio of Sirolimus to sodium dodecyl sulfate is 5:1 to 1:2;
preferably, the anti-solvent method comprises the following steps:
S1. Accurately weigh Sirolimus and organic solvent, respectively, and stir magnetically until a transparent and uniform phase A solution is obtained;
S2. Accurately weigh sodium dodecyl sulfate and solvent in aqueous phase, respectively, and stir magnetically until a transparent and uniform phase B solution is obtained;
S3. Add phase A solution to phase B solution quickly, and stir magnetically to obtain a nanocrystals suspension;
S4. Add water to the suspension and mix well, and then freeze-dry to obtain nanocrystals particles;
preferably, the particle size d50 of the nanocrystals particles is 150 to 900 nm, and the mass ratio of Sirolimus to sodium dodecyl sulfate is 5:1 to 1:2;
preferably, the high pressure homogenization method comprises the following steps:
S1. Accurately weigh Sirolimus, solvent in aqueous phase and sodium dodecyl sulfate, respectively, and stir magnetically to obtain a suspension;
S2. Perform several times of homogenization to the suspension through a high pressure homogenizer to obtain a nanocrystals suspension;
S3. Freeze-dry to obtain Sirolimus nanocrystals;
preferably, the particle size d50 of the nanocrystals particles is between 150 and 900 nm, the homogenization pressure is 1,000 to 2,000 bar, the homogenization is performed for 5 to 10 times, and the mass ratio of Sirolimus to sodium dodecyl sulfate is between 5:1 and 1:2;
preferably, the microfluidic method comprises the following steps:
S1. Accurately weigh Sirolimus, solvent in aqueous phase and sodium dodecyl sulfate, respectively, and stir magnetically to obtain a suspension;
S2. Perform several times of homogenization to the suspension through a microfluidic device to obtain a nanocrystals suspension;
S3. Freeze-dry to obtain Sirolimus nanocrystals;
preferably, the particle size d50 of the nanocrystals particles is 150 to 900 nm, the microfluidization pressure is 1,000 to 2,000 bar, the homogenization is performed for 5 to 10 times, and the mass ratio of Sirolimus to sodium dodecyl sulfate is 5:1 to 1:2.

### Claim 9

A coating solution for drug-coated balloon, characterized in that the coating solution comprises an aqueous solvent, and the coating solution further comprises a plurality of core-shell structures formed by wrapping drugs in a phospholipid bilayer, the core-shell structures are dispersed in the solvent in aqueous phase, wherein, a core of the core-shell structures comprises a plurality of particles loaded with drugs, and a shell of the core-shell structures is a phospholipid bilayer comprising a hydrophilic group in the outer layer and a hydrophobic group in the inner layer, the plurality of particles loaded with drugs comprise a plurality of nanocrystals particles comprising drugs,
wherein, the raw materials for preparing the nanocrystals particles comprise a surfactant, and the surfactant is selected from one or more of vitamin E polyethylene glycol succinate, Poloxamer 188, Poloxamer 407, Tyloxapol, docusate sodium, polyoxyl 15-hydroxystearate, polyoxyethylene (40) hydrogenated castor oil, polyoxyethylene (60) hydrogenated castor oil, polyoxyethylene (60) castor oil, polyoxyethylene (40) castor oil, polyoxyethylene (35) castor oil, polyoxyethylene (20) castor oil, polyoxyethylene (10) castor oil, Polyethylene glycol hexadecyl octadecyl ether 20, polyethylene glycol hexadecyl octadecyl ether 12, polyoxyethylene monocetyl ether (Ceteth-10), polyoxyethylene (10) lauryl ether (Brij 56), polyoxyethylene (20) lauryl ether (Brij 58), polyoxyethylene (23) lauryl ether (Brij 35), polyoxyethylene (2) lauryl ether (Brij 52), polyoxyethylene (25) oleate (Myrj 49), polyoxyethylene (40) palmitate (Myrj 52), sodium dodecyl sulfate, Tween 80, Tween 60, Tween 40, propylene glycol monolaurate, polyoxyethylene (20) lauryl ether, and polyoxyethylene monocetyl ether.

### Claim 10 (depends on 9)

A coating solution according to claim 9, characterized in that the method for preparing the nanocrystals particles comprises: anti-solvent method, high pressure homogenization method or microfluidic method;
preferably, the anti-solvent method comprises the following steps:
S1. Accurately weigh Sirolimus and organic solvent, respectively, and stir magnetically until a transparent and uniform phase A solution is obtained;
S2. Accurately weigh the surfactant and the solvent in aqueous phase, respectively, and stir magnetically until a transparent and uniform phase B solution is obtained;
S3. Add phase A solution to phase B solution quickly, and stir magnetically to obtain a nanocrystals suspension;
S4. Add water to the suspension and mix well, and then freeze-dry to obtain nanocrystals particles;
preferably, the particle size d50 of the nanocrystals particles is between 150 and 900 nm, and the mass ratio of Sirolimus to surfactant is between 5:1 and 1:2;
preferably, the high pressure homogenization method comprises the following steps:
S1. Accurately weigh Sirolimus, solvent in aqueous phase and surfactant, respectively, and stir magnetically to obtain a suspension;
S2. Perform several times of homogenization to the suspension through a high pressure homogenizer to obtain a nanocrystals suspension;
S3. Freeze-dry to obtain Sirolimus nanocrystals;
preferably, the particle size d50 of the nanocrystals particles is between 150 and 900 nm, the homogenization pressure is 1,000 to 2,000 bar, the homogenization is performed for 5 to 10 times, and the mass ratio of Sirolimus to surfactant is between 5:1 and 1:2;
preferably, the microfluidic method comprises the following steps:
S1. Accurately weigh Sirolimus, solvent in aqueous phase and surfactant, respectively, and stir magnetically to obtain a suspension;
S2. Perform several times of homogenization to the suspension through a microfluidic device to obtain a nanocrystals suspension;
S3. Freeze-dry to obtain Sirolimus nanocrystals;
preferably, the particle size d50 of the nanocrystals particles is 150 to 900 nm, the microfluidization pressure is 1,000 to 2,000 bar, the homogenization is performed for 5 to 10 times, and the mass ratio of Sirolimus to surfactant is 5:1 to 1:2.

### Claim 11

A use of Sirolimus-coated balloon in intracranial artery stenosis, wherein the drug dose is less than or equal to 3 μg/mm2, and more preferably less than or equal to 1.5 μg/mm2.