# US 2026/0076176 A1 · Semiconductor device and manufacturing method thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0076176 A1
- Document ID: US20260076176A1
- Status: Published application
- Kind: A1
- Application number: 18/827,866
- Filed: 2024-09-09
- Published: 2026-03-12
- Earliest claimed: 2024-09-09
- Assignees: Nanya Technology Corporation
- Applicants: Nanya Technology Corporation
- Inventors: Cheng Yan JI
- Web page: https://patentgrep.com/patent/US20260076176A1

## CPC

- H10W 20/48: Insulating materials thereof
- H10P 14/6339: {deposition by cyclic CVD, e.g. ALD, ALE or pulsed CVD}
- H10P 14/6903: {containing silicon}
- H10W 10/014: {using trench refilling with dielectric materials, e.g. shallow trench isolations}
- H10W 10/17: formed using trench refilling with dielectric materials, e.g. shallow trench isolations
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

A manufacturing method of a semiconductor device includes depositing, using a first atomic layer deposition, a first thin poly silicon layer on an active area, in which the active area includes a trench; depositing, using a second atomic layer deposition, a second thin poly silicon layer on the active area; and depositing, using a chemical vapor deposition, a poly silicon layer on the active area to form a poly silicon structure, in which a gas for the chemical vapor deposition includes disilane, a thickness of the poly silicon layer in a bottom of the trenches is substantially zero.

## Claims

### Claim 1

A manufacturing method of a semiconductor device, comprising:
depositing, using a first atomic layer deposition, a first thin poly silicon layer on an active area, wherein the active area comprises a trench;
depositing, using a second atomic layer deposition, a second thin poly silicon layer on the active area; and
depositing, using a chemical vapor deposition, a poly silicon layer on the active area to form a poly silicon structure, wherein a gas for the chemical vapor deposition comprises disilane, a thickness of the poly silicon layer in a bottom of the trenches is substantially zero.

### Claim 2 (depends on 1)

The manufacturing method of the semiconductor device of claim 1, further comprising:
etching a substrate to form the active area.

### Claim 3 (depends on 1)

The manufacturing method of the semiconductor device of claim 1, further comprising:
filling the trenches with a dielectric material to form a shallow trench isolation.

### Claim 4 (depends on 1)

The manufacturing method of the semiconductor device of claim 1, wherein a ratio of a thickness of a top portion of a sidewall of the poly silicon structure to a thickness of a top plane of the poly silicon structure is in a range of 0.6 to 0.7.

### Claim 5 (depends on 1)

The manufacturing method of the semiconductor device of claim 1, wherein a ratio of a thickness of a middle portion of a sidewall of the poly silicon structure to a thickness of a top plane of the poly silicon structure is in a range of 0.6 to 0.7.

### Claim 6 (depends on 1)

The manufacturing method of the semiconductor device of claim 1, wherein a ratio of a thickness of a bottom portion of a sidewall of the poly silicon structure to a thickness of a top plane of the poly silicon structure is in a range of 0.35 to 0.45.

### Claim 7 (depends on 1)

The manufacturing method of the semiconductor device of claim 1, wherein a gas used in the first atomic layer deposition comprises dichlorosilane.

### Claim 8

A manufacturing method of a semiconductor device, comprising:
depositing, using a first atomic layer deposition, a first thin poly silicon layer on an active area, wherein the active area comprises a trench, a gas used in the first atomic layer deposition comprises dichlorosilane;
depositing, using a second atomic layer deposition, a second thin poly silicon layer on the active area; and
depositing, using a chemical vapor deposition, a poly silicon layer on the active area to form a poly silicon structure, wherein a gas for the chemical vapor deposition comprises disilane.

### Claim 9 (depends on 8)

The manufacturing method of the semiconductor device of claim 8, further comprising:
etching a substrate to form the active area.

### Claim 10 (depends on 8)

The manufacturing method of the semiconductor device of claim 8, further comprising:
filling the trenches with a dielectric material to form a shallow trench isolation.

### Claim 11 (depends on 8)

The manufacturing method of the semiconductor device of claim 8, wherein a ratio of a thickness of a top portion of a sidewall of the poly silicon structure to a thickness of a top plane of the poly silicon structure is in a range of 0.6 to 0.7.

### Claim 12 (depends on 8)

The manufacturing method of the semiconductor device of claim 8, wherein a ratio of a thickness of a middle portion of a sidewall of the poly silicon structure to a thickness of a top plane of the poly silicon structure is in a range of 0.6 to 0.7.

### Claim 13 (depends on 8)

The manufacturing method of the semiconductor device of claim 8, wherein a ratio of a thickness of a bottom portion of a sidewall of the poly silicon structure to a thickness of a top plane of the poly silicon structure is in a range of 0.35 to 0.45.

### Claim 14 (depends on 8)

The manufacturing method of the semiconductor device of claim 8, wherein a gas used in the second atomic layer deposition comprises disilane.

### Claim 15

A semiconductor device, comprising:
a substrate, wherein the substrate comprises an active area, the active area comprises a trench; and
a poly silicon layer located on the active area, wherein a thickness of the poly silicon layer gradually shrinks from a top portion of a sidewall of the poly silicon layer to a bottom portion of the sidewall of the poly silicon layer.

### Claim 16 (depends on 15)

The semiconductor device of claim 15, wherein a thickness of the poly silicon layer on a bottom of the trench is substantially zero.

### Claim 17 (depends on 15)

The semiconductor device of claim 15, wherein a ratio of a thickness of the top portion of the sidewall of the poly silicon layer to a thickness of a top plane of the poly silicon layer is in a range of 0.6 to 0.7.

### Claim 18 (depends on 15)

The semiconductor device of claim 15, wherein a ratio of a thickness of a middle portion of the sidewall of the poly silicon layer to a thickness of a top plane of the poly silicon layer is in a range of 0.6 to 0.7.

### Claim 19 (depends on 15)

The semiconductor device of claim 15, wherein a ratio of a thickness of the bottom portion of the sidewall of the poly silicon layer to a thickness of a top plane of the poly silicon layer is in a range of 0.35 to 0.45.

### Claim 20 (depends on 15)

The semiconductor device of claim 15, wherein the poly silicon layer is formed by a first atomic layer deposition, a second atomic layer deposition and a chemical vapor deposition.