# US 2026/0075938 A1 · Methods of forming semiconductor devices

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0075938 A1
- Document ID: US20260075938A1
- Status: Published application
- Kind: A1
- Application number: 19/392,524
- Filed: 2025-11-18
- Published: 2026-03-12
- Earliest claimed: 2021-01-15
- Assignees: Taiwan Semiconductor Manufacturing Company, Ltd.
- Applicants: Taiwan Semiconductor Manufacturing Co., Ltd.
- Inventors: Wan-Yi Kao; Szu-Ping Lee; Che-Hao Chang; Chun-Heng Chen; Yung-Cheng Lu; Chi On Chui
- Web page: https://patentgrep.com/patent/US20260075938A1

## CPC

- H10D 84/0188: {Manufacturing their isolation regions}
- H10D 84/853: {comprising FinFETs}
- H10D 30/024: {of fin field-effect transistors [FinFET]}
- H10D 30/6211: {having fin-shaped semiconductor bodies integral with the bulk semiconductor substrates}
- H10D 62/115: {Dielectric isolations, e.g. air gaps}
- H10D 84/013: {Manufacturing their source or drain regions, e.g. silicided source or drain regions}
- H10D 84/0158: {the components including FinFETs}
- H10D 84/0193: {the components including FinFETs}
- H10D 84/038: {using silicon technology, e.g. SiGe}
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

In an embodiment, a method includes: forming a first fin and a second fin extending from a semiconductor substrate; depositing a liner layer along a first sidewall of the first fin, a second sidewall of the second fin, and a top surface of the semiconductor substrate, the liner layer formed of silicon oxynitride having a nitrogen concentration; depositing a fill material on the liner layer, the fill material formed of silicon; annealing the liner layer and the fill material, the annealing converting the fill material to silicon oxide, the annealing decreasing the nitrogen concentration of the liner layer; and recessing the liner layer and the fill material to form an isolation region between the first fin and the second fin.

## Claims

### Claim 1

A method comprising:
forming an isolation region between a first channel region and a second channel region by:
depositing a liner material, the liner material having a first nitrogen concentration;
depositing a semiconductor material over the liner material;
converting the semiconductor material and an upper portion of the liner material to a fill material, the fill material having a second nitrogen concentration, the second nitrogen concentration being less than the first nitrogen concentration; and
recessing the fill material and the liner material; and
forming a gate structure extending along a top surface of the isolation region, a first sidewall of the first channel region, and a second sidewall of the second channel region.

### Claim 2 (depends on 1)

The method of claim 1, wherein the first nitrogen concentration is in a range of 5% to 30%, and the second nitrogen concentration is in a range of 1% to 5%.

### Claim 3 (depends on 1)

The method of claim 1, wherein the liner material is silicon oxynitride, the semiconductor material is silicon, and the fill material is silicon oxide.

### Claim 4 (depends on 1)

The method of claim 1, wherein depositing the liner material comprises performing an atomic layer deposition process, depositing the semiconductor material comprises performing a chemical vapor deposition process, and converting the semiconductor material and the upper portion of the liner material comprises performing a wet anneal process.

### Claim 5 (depends on 1)

The method of claim 1, wherein the liner material has a first thickness before converting the semiconductor material and the upper portion of the liner material, the liner material has a second thickness after converting the semiconductor material and the upper portion of the liner material, and the second thickness is less than the first thickness.

### Claim 6 (depends on 1)

The method of claim 1, wherein after recessing the fill material and the liner material, a top surface of the fill material is coplanar with a top surface of the liner material.

### Claim 7 (depends on 1)

The method of claim 1, wherein forming the gate structure comprises:
depositing a gate dielectric layer over the first channel region, the second channel region, and the top surface of the isolation region, a dielectric constant of the gate dielectric layer being greater than a dielectric constant of the fill material; and
depositing a gate electrode layer over the gate dielectric layer.

### Claim 8 (depends on 1)

The method of claim 1, further comprising:
forming a first fin and a second fin extending from a substrate, the first fin comprising the first channel region, the second fin comprising the second channel region.

### Claim 9

A method comprising:
forming an isolation region over a substrate by:
depositing a liner material having a nitrogen concentration of at least 5%;
depositing a semiconductor material over the liner material;
performing an anneal process that converts the semiconductor material to a fill material and decreases the nitrogen concentration of the liner material to less than 5%; and
recessing the fill material and the liner material; and
forming a gate structure over the isolation region, the gate structure comprising a gate dielectric and a gate electrode over the gate dielectric, a dielectric constant of the gate dielectric being greater than a dielectric constant of the fill material.

### Claim 10 (depends on 9)

The method of claim 9, wherein the liner material is deposited to a thickness in a range of 15 Å to 50 Å, and the anneal process decreases the thickness of the liner material to be in a range of 1 Å to 10 Å.

### Claim 11 (depends on 9)

The method of claim 9, wherein recessing the fill material and the liner material comprises etching the fill material and the liner material at substantially the same rate.

### Claim 12 (depends on 11)

The method of claim 11, wherein the liner material is silicon oxynitride, the semiconductor material is silicon, the fill material is silicon oxide, and the etching comprises performing a wet etch using dilute hydrofluoric acid.

### Claim 13 (depends on 9)

The method of claim 9, wherein the isolation region is formed between a first channel region and a second channel region, and the gate structure extends between the first channel region and the second channel region.

### Claim 14 (depends on 9)

The method of claim 9, further comprising:
forming a gate spacer adjacent to the gate structure;
forming a source/drain region adjacent to the gate spacer;
depositing an inter-layer dielectric over the source/drain region; and
forming a source/drain contact extending through the inter-layer dielectric, the source/drain contact being coupled to the source/drain region, the source/drain contact being spaced apart from the gate structure by the inter-layer dielectric and the gate spacer.

### Claim 15

A method comprising:
forming an isolation region adjacent to a channel region by:
depositing a liner material;
depositing a semiconductor material over the liner material;
performing an anneal process that converts the semiconductor material to a fill material and decreases an etching selectivity between the liner material and the fill material relative to an etching process; and
recessing the liner material and the fill material by etching the liner material and the fill material with the etching process; and
forming a gate structure over the isolation region and the channel region;
forming a gate spacer adjacent to the gate structure;
forming a source/drain region adjacent to the gate spacer and the channel region;
depositing an inter-layer dielectric over the source/drain region; and
forming a source/drain contact extending through the inter-layer dielectric, the source/drain contact being coupled to the source/drain region, the source/drain contact being spaced apart from the gate structure by the inter-layer dielectric and the gate spacer.

### Claim 16 (depends on 15)

The method of claim 15, wherein the liner material is deposited with a nitrogen concentration in a range of 5% to 30%, and the anneal process decreases the nitrogen concentration of the liner material to be in a range of 1% to 5%.

### Claim 17 (depends on 15)

The method of claim 15, wherein the liner material is deposited to a thickness in a range of 15 Å to 50 Å, and the anneal process decreases the thickness of the liner material to be in a range of 1 Å to 10 Å.

### Claim 18 (depends on 15)

The method of claim 15, wherein the liner material is deposited having an effective oxide charge with respect to the channel region, and the anneal process decreases the effective oxide charge.

### Claim 19 (depends on 15)

The method of claim 15, wherein depositing the liner material comprises depositing silicon oxynitride by atomic layer deposition, and depositing the semiconductor material comprises depositing silicon by chemical vapor deposition.

### Claim 20 (depends on 15)

The method of claim 15, wherein after the etching process, a top surface of the liner material is coplanar with a top surface of the fill material, and the gate structure extends across the top surface of the liner material and the top surface of the fill material.