# US 2026/0075858 A1 · Rinse process after forming fin-shaped structure

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0075858 A1
- Document ID: US20260075858A1
- Status: Published application
- Kind: A1
- Application number: 19/387,477
- Filed: 2025-11-12
- Published: 2026-03-12
- Earliest claimed: 2018-10-31
- Assignees: United Microelectronics Corp.
- Applicants: United Microelectronics Corp.
- Inventors: Po-Chang Lin; Bo-Han Huang; Chih-Chung Chen; Chun-Hsien Lin; Shih-Hung Tsai; Po-Kuang Hsieh
- Web page: https://patentgrep.com/patent/US20260075858A1

## CPC

- H10D 30/024: {of fin field-effect transistors [FinFET]}
- H10D 30/0245: {by further thinning the channel after patterning the channel, e.g. using sacrificial oxidation on fins}
- H10D 30/6211: {having fin-shaped semiconductor bodies integral with the bulk semiconductor substrates}
- H10D 30/6213: {having rounded corners}
- H10P 14/6309: {of silicon in uncombined form, i.e. pure silicon}
- H10P 14/6319: {Formation by plasma treatments, e.g. plasma oxidation of the substrate}
- H10P 70/23: {during, before or after processing of insulating materials}
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

A method for fabricating semiconductor device includes the steps of: forming fin-shaped structures on a substrate; using isopropyl alcohol (IPA) to perform a rinse process; performing a baking process; and forming a gate oxide layer on the fin-shaped structures. Preferably, a duration of the rinse process is between 15 seconds to 60 seconds, a temperature of the baking process is between 50° C. to 100° C., and a duration of the baking process is between 5 seconds to 120 seconds.

## Claims

### Claim 1

A method for fabricating semiconductor device, comprising:
forming fin-shaped structures on a substrate;
performing a first cleaning process to transform an angle between sidewalls of the fin-shaped structures made of planar surfaces to an angle made of a curved surface;
using isopropyl alcohol (IPA) to perform a rinse process;
performing a baking process; and
forming a gate oxide layer on the fin-shaped structures.

### Claim 2 (depends on 1)

The method of claim 1, further comprising:
performing a plasma treatment process to form an oxide layer on a bottom surface between the fin-shaped structures;
performing the first cleaning process to remove the oxide layer;
performing a second cleaning process to remove polymers; and
performing a third cleaning process to remove particles.

### Claim 3 (depends on 2)

The method of claim 2, further comprising using oxygen gas (O2) to perform the plasma treatment process.

### Claim 4 (depends on 3)

The method of claim 3, wherein a temperature of the plasma treatment process is between 135° C. to 165° C.

### Claim 5 (depends on 3)

The method of claim 3, wherein a pressure of the plasma treatment process is between 0.9 Torr to 1.1 Torr.

### Claim 6 (depends on 3)

The method of claim 3, wherein a duration of the plasma treatment process is between 2.7 minutes to 3.3 minutes.

### Claim 7 (depends on 2)

The method of claim 2, further comprising using diluted hydrofluoric acid (dHF) to perform the first cleaning process.

### Claim 8 (depends on 2)

The method of claim 2, further comprising using ozone (O3) to perform the second cleaning process.

### Claim 9 (depends on 2)

The method of claim 2, further comprising using Standard Clean 1 (SC1) to perform the third cleaning process.

### Claim 10 (depends on 1)

The method of claim 1, wherein a duration of the rinse process is between 15 seconds to 60 seconds.

### Claim 11 (depends on 1)

The method of claim 1, wherein a temperature of the baking process is between 50° C. to 100 ° C.

### Claim 12 (depends on 1)

The method of claim 1, wherein a duration of the baking process is between 5 seconds to 120 seconds.

### Claim 13 (depends on 1)

The method of claim 1, further comprising performing an in-situ steam generation (ISSG) process to form the gate oxide layer.

### Claim 14 (depends on 1)

The method of claim 1, wherein the fin-shaped structures comprise a ring-shaped fin-shaped structure, and the method further comprises performing a fin cut process to cut the ring-shaped fin-shaped structure after forming the gate oxide layer.