# US 2026/0075825 A1 · Semiconductor device and semiconductor device manufacturing method

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0075825 A1
- Document ID: US20260075825A1
- Status: Published application
- Kind: A1
- Application number: 19/393,757
- Filed: 2025-11-19
- Published: 2026-03-12
- Earliest claimed: 2021-09-21
- Assignees: Kioxia Corporation
- Applicants: Kioxia Corporation
- Inventors: Tomotaka ARIGA; Masayuki KITAMURA; Hiroshi TOYODA
- Web page: https://patentgrep.com/patent/US20260075825A1

## CPC

- H10B 43/27: the channels comprising vertical portions, e.g. U-shaped channels
- H10D 64/037: {comprising charge-trapping insulators}
- H10D 64/665: {the conductor comprising a layer of elemental metal contacting the insulator, e.g. tungsten or molybdenum (having lateral variation H10D64/671)}
- H10B: ELECTRONIC MEMORY DEVICES
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

A semiconductor device that can have an improved data retention characteristic is provided. A semiconductor device includes a stacked body and a memory pillar formed in a memory hole of the stacked body. The memory pillar has a structure in which a semiconductor portion 61b, a tunnel insulating film 62a, and a charge storage layer 62b are sequentially stacked. A block insulating film 53 is provided between the charge storage layer 62b and a conductive layer 52. The conductive layer 52 contains molybdenum. The block insulating film 53 includes a silicon oxide film 53a and an aluminum oxide film 53b. A region from the conductive layer 52 to the aluminum oxide film 53b contains chlorine, which prevents OH diffusion. The concentration of chlorine at a second portion closer to the aluminum oxide film 53b than a first portion in the conductive layer 52 is higher than the concentration of impurities at the first portion in the conductive layer.

## Claims

### Claim 1

A semiconductor device manufacturing method comprising:
forming a block insulating film by sequentially forming a first film and a second film on a surface of a charge storage layer;
forming a material-containing film on a surface of the second film by causing material gas and first gas to alternately flow on the surface of the second film, the material gas includes at least one of silicon and titanium, and the first gas includes nitrogen; and
forming a material-containing conductive layer on the surface of the second film by causing the material gas and a second gas to alternately flow on the material-containing film, the second gas includes hydrogen.

### Claim 2 (depends on 1)

A semiconductor device manufacturing method according to claim 1, wherein the material gas is MoO2Cl2 gas and the first gas is ammonia gas.

### Claim 3 (depends on 1)

A semiconductor device manufacturing method according to claim 1, wherein the material-containing film includes molybdenum and nitrogen, and the material-containing conductive layer includes molybdenum.

### Claim 4 (depends on 1)

A semiconductor device manufacturing method according to claim 1, wherein the material gas is SiH4 gas or SiH6 gas.

### Claim 5 (depends on 1)

A semiconductor device manufacturing method according to claim 1, wherein the material gas is SiH4 gas or TiCl4 gas.

### Claim 6 (depends on 1)

A semiconductor device manufacturing method according to claim 1, wherein the first gas is ammonia gas.

### Claim 7 (depends on 1)

A semiconductor device manufacturing method according to claim 1, wherein the material-containing film is formed by using an atomic layer deposition method.

### Claim 8 (depends on 1)

A semiconductor device manufacturing method according to claim 1, wherein the material-containing conductive layer is formed by using an atomic layer deposition method.

### Claim 9 (depends on 1)

A semiconductor device manufacturing method according to claim 1, wherein the material-containing film is formed in an atmosphere at a first temperature, and the material-containing conductive layer is formed in an atmosphere at a second temperature higher than the first temperature.

### Claim 10 (depends on 9)

A semiconductor device manufacturing method according to claim 9, wherein the first temperature is 300° C. or higher and 400° C. or lower.

### Claim 11 (depends on 10)

A semiconductor device manufacturing method according to claim 10, wherein the second temperature is 600° C.

### Claim 12 (depends on 1)

A semiconductor device manufacturing method according to claim 1, wherein the reactivity of the first gas with respect to the material gas is lower than the reactivity of the second gas with respect to the material gas.

### Claim 13 (depends on 1)

A semiconductor device manufacturing method according to claim 1, wherein the material gas includes a specified element, and a concentration of the specified element in the second film is higher than a concentration of the specified element in the material-containing conductive layer.

### Claim 14 (depends on 13)

A semiconductor device manufacturing method according to claim 13, wherein the concentration of the specified element in the second film is higher than a concentration of the specified element in the first film.

### Claim 15 (depends on 13)

A semiconductor device manufacturing method according to claim 13, wherein the specified element is chlorine, silicon, or titanium.

### Claim 16 (depends on 13)

A semiconductor device manufacturing method according to claim 13, wherein the first film includes silicon and oxygen, and the second film includes aluminum and oxygen.