# US 2026/0075824 A1 · Semiconductor device, semiconductor memory device, and method for manufacturing semiconductor device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0075824 A1
- Document ID: US20260075824A1
- Status: Published application
- Kind: A1
- Application number: 19/393,020
- Filed: 2025-11-18
- Published: 2026-03-12
- Earliest claimed: 2021-09-17
- Assignees: Kioxia Corporation
- Applicants: Kioxia Corporation
- Inventors: Yusuke NAKAJIMA; Akira TAKASHIMA; Tsunehiro INO; Yasushi NAKASAKI; Koji USUDA; Masaki NOGUCHI
- Web page: https://patentgrep.com/patent/US20260075824A1

## CPC

- H10B 43/27: the channels comprising vertical portions, e.g. U-shaped channels
- H10B 41/10: characterised by the top-view layout
- H10B 41/27: the channels comprising vertical portions, e.g. U-shaped channels
- H10B 41/35: with a cell select transistor, e.g. NAND
- H10B 43/10: characterised by the top-view layout
- H10B 43/35: with cell select transistors, e.g. NAND
- H10D 64/037: {comprising charge-trapping insulators}
- H10B: ELECTRONIC MEMORY DEVICES
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

A semiconductor device of an embodiment includes a semiconductor layer, a gate electrode layer, and a first insulating layer provided between the semiconductor layer and the gate electrode layer, the first insulating layer including aluminum oxide including at least one crystal phase selected from the group consisting of alpha (α)-aluminum oxide and theta (θ)-aluminum oxide, the first insulating layer having a thickness of equal to or less than 2.5 nm in a first direction from the semiconductor layer toward the gate electrode layer.

## Claims

### Claim 1

A method for manufacturing a semiconductor device, the method comprising:
forming a first aluminum nitride film having a thickness of less than 2.5 nm; and
forming a first aluminum oxide film by oxidizing the first aluminum nitride film at a temperature of equal to or more than 900° C.

### Claim 2 (depends on 1)

The method for manufacturing the semiconductor device according to claim 1, wherein, in the forming the first aluminum oxide film, the first aluminum nitride film is oxidized in an atmosphere containing an oxygen gas and a hydrogen gas.

### Claim 3 (depends on 1)

The method for manufacturing the semiconductor device according to claim 1, wherein the first aluminum oxide film is formed on a silicon oxide film.

### Claim 4 (depends on 1)

The method for manufacturing the semiconductor device according to claim 1, further comprising:
forming a second aluminum nitride film having a thickness of less than 2.5 nm on the first aluminum oxide film; and
forming a second aluminum oxide film by oxidizing the second aluminum nitride film at a temperature of equal to or more than 900° C.

### Claim 5 (depends on 1)

The method for manufacturing the semiconductor device according to claim 1, further comprising:
forming a gate electrode layer after the forming the first aluminum oxide film,
wherein the first aluminum nitride film is formed on a semiconductor layer.

### Claim 6 (depends on 1)

The method for manufacturing the semiconductor device according to claim 1,
wherein the first aluminum oxide film includes aluminum oxide, and the aluminum oxide includes at least one crystal phase selected from the group consisting of alpha (α)-aluminum oxide and theta (θ)-aluminum oxide.

### Claim 7 (depends on 5)

The method for manufacturing the semiconductor device according to claim 5,
wherein the first aluminum oxide film includes aluminum oxide, and the aluminum oxide includes at least one crystal phase selected from the group consisting of alpha (α)-aluminum oxide and theta (θ)-aluminum oxide, and
the aluminum oxide in the first aluminum oxide film has a crystal axis in a direction within a range of ±10 degrees with respect to a first direction from the semiconductor layer toward the gate electrode layer.

### Claim 8 (depends on 7)

The method for manufacturing the semiconductor device according to claim 7, wherein the crystal axis is a c-axis.