# US 2026/0074254 A1 · Fluorocarbon molecular additives for perfluorosulfonic acid based membranes

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0074254 A1
- Document ID: US20260074254A1
- Status: Published application
- Kind: A1
- Application number: 18/883,340
- Filed: 2024-09-12
- Published: 2026-03-12
- Earliest claimed: 2024-09-12
- Assignees: GM Global Technology Operations LLC
- Applicants: GM Global Technology Operations LLC
- Inventors: Nagappan Ramaswamy; Richard Wehbe; Yunzhu Zhang
- Web page: https://patentgrep.com/patent/US20260074254A1

## CPC

- H01M 8/1051: Non-ion-conducting additives, e.g. stabilisers, SiO2 or ZrO2
- H01M 8/1004: characterised by membrane-electrode assemblies [MEA] (H01M8/12 takes precedence)
- H01M 8/1023: having only carbon, e.g. polyarylenes, polystyrenes or polybutadiene-styrenes
- H01M 8/1039: halogenated, e.g. sulfonated polyvinylidene fluorides
- H01M 8/1048: Ion-conducting additives, e.g. ion-conducting particles, heteropolyacids, metal phosphate or polybenzimidazole with phosphoric acid
- H01M 8/1053: consisting of layers of polymers with at least one layer being ionically conductive
- H01M 8/1067: characterised by their physical properties, e.g. porosity, ionic conductivity or thickness
- H01M 8/1081: starting from solutions, dispersions or slurries exclusively of polymers
- H01M 2008/1095: {Fuel cells with polymeric electrolytes}
- H01M 2250/20: Fuel cells in motive systems, e.g. vehicle, ship, plane
- Y02E 60/50: Fuel cells
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A proton exchange membrane for an energy conversion device, a hydrogen fuel cell stack for a vehicle, and a method of forming a proton exchange membrane. The proton exchange membrane includes a first layer of a perfluorosulfonic acid ionomer. In addition, the perfluorosulfonic acid ionomer includes a first methoxy-nonafluorobutane coated additive. The hydrogen fuel cell stack includes one or more membrane electrode assemblies, each including a proton exchange membrane.

## Claims

### Claim 1

A proton exchange membrane for an energy conversion device, comprising:
a first layer of a perfluorosulfonic acid ionomer,
wherein the perfluorosulfonic acid ionomer includes a first methoxy-nonafluorobutane coated additive.

### Claim 2 (depends on 1)

The proton exchange membrane of claim 1, wherein the methoxy-nonafluorobutane coated additive includes a recombination catalyst.

### Claim 3 (depends on 2)

The proton exchange membrane of claim 2, wherein the first methoxy-nonafluorobutane coated additive includes platinum on carbon and a weight ratio of the perfluorosulfonic acid ionomer to the first methoxy-nonafluorobutane coated additive is in the range of 1:10 to 1:2000.

### Claim 4 (depends on 1)

The proton exchange membrane of claim 1, wherein the first methoxy-nonafluorobutane coated additive includes an inert particle.

### Claim 5 (depends on 1)

The proton exchange membrane of claim 1, wherein the first methoxy-nonafluorobutane coated additive includes at least one additive selected from the group consisting of silica, carbon black, graphene, and carbon nanotubes.

### Claim 6 (depends on 1)

The proton exchange membrane of claim 1, further comprising an expanded polytetrafluoroethylene membrane including a first side and a second side, wherein the first layer of the perfluorosulfonic acid ionomer contacts the first side of the expanded polytetrafluoroethylene membrane.

### Claim 7 (depends on 6)

The proton exchange membrane of claim 6, further comprising a second layer of the perfluorosulfonic acid ionomer contacting a second side of the expanded polytetrafluoroethylene membrane, wherein the second layer of the perfluorosulfonic acid includes a second methoxy-nonafluorobutane coated additive and contacts a second side of the expanded polytetrafluoroethylene membrane.

### Claim 8 (depends on 7)

The proton exchange membrane of claim 7, wherein the first methoxy-nonafluorobutane coated additive and the second methoxy-nonafluorobutane coated additive are the same.

### Claim 9 (depends on 7)

The proton exchange membrane of claim 7, wherein the first layer of the perfluorosulfonic acid ionomer exhibits a first thickness in the range of 4 micrometers to 28 micrometers and the second layer of perfluorosulfonic acid ionomer exhibits a second thickness in the range of 2 micrometers to 28 micrometers.

### Claim 10 (depends on 9)

The proton exchange membrane of claim 9, wherein the expanded polytetrafluoroethylene membrane exhibits a third thickness in the range of 1 micrometers to 10 micrometers.

### Claim 11 (depends on 1)

The proton exchange membrane of claim 1, further comprising:
an expanded polytetrafluoroethylene membrane including a first side and a second side, wherein the expanded polytetrafluoroethylene membrane exhibits a thickness in the range of 1 micrometer to 10 micrometers, wherein the first layer of the perfluorosulfonic acid ionomer exhibits a thickness in the range of 4 micrometers to 15 micrometers and contacts the first side of the expanded polytetrafluoroethylene membrane; and
a second layer of the perfluorosulfonic acid ionomer including a second methoxy-nonafluorobutane coated additive dispersed through the second layer of the perfluorosulfonic acid ionomer, wherein the second layer of the perfluorosulfonic acid exhibits a thickness in the range of 2 micrometers to 6 micrometers and contacts a second side of the expanded polytetrafluoroethylene membrane,
wherein the first methoxy-nonafluorobutane coated additive and the second methoxy-nonafluorobutane coated additive include platinum on carbon, the weight ratio of the first layer of perfluorosulfonic acid ionomer to the first methoxy-nonafluorobutane coated additive is in the range of 1:10 to 1:2000, and the weight ratio of the second layer of perfluorosulfonic acid ionomer to the second methoxy-nonafluorobutane coated additive is in the range of 1:10 to 1:2000.

### Claim 12

A hydrogen fuel cell stack for a vehicle, comprising:
one or more membrane electrode assemblies, each membrane electrode assembly including:
a proton exchange membrane including first layer of a perfluorosulfonic acid ionomer, wherein the perfluorosulfonic acid ionomer includes a first methoxy-nonafluorobutane coated additive present at a weight ratio of the perfluorosulfonic acid ionomer to the first methoxy-nonafluorobutane coated additive is in the range of 1:10 to 1:2000;
an anode including a first gas diffusion layer and a first catalyst disposed on the first gas diffusion layer, wherein the first catalyst contacts a first surface of the proton exchange membrane; and
a cathode including a second gas diffusion layer and a second catalyst disposed on the second gas diffusion layer, wherein the second catalyst contacts a second surface of the proton exchange membrane.

### Claim 13 (depends on 12)

The hydrogen fuel cell stack of claim 12, wherein the first methoxy-nonafluorobutane coated additive is platinum on carbon.

### Claim 14 (depends on 12)

The hydrogen fuel cell stack of claim 12, wherein the first methoxy-nonafluorobutane coated additive an inert particle.

### Claim 15 (depends on 12)

The hydrogen fuel cell stack of claim 12, wherein the first methoxy-nonafluorobutane coated additive includes at least one additive selected from the group consisting of silica, carbon black, graphene, and carbon nanotubes.

### Claim 16 (depends on 12)

The hydrogen fuel cell stack of claim 12, further comprising an expanded polytetrafluoroethylene membrane, the expanded polytetrafluoroethylene membrane including a first side and a second side, wherein the first layer of the perfluorosulfonic acid ionomer contacts the first side of the expanded polytetrafluoroethylene membrane.

### Claim 17 (depends on 16)

The hydrogen fuel cell stack of claim 16, further comprising a second layer of a perfluorosulfonic acid ionomer contacting the second side of the expanded polytetrafluoroethylene membrane, wherein the perfluorosulfonic acid ionomer includes a second methoxy-nonafluorobutane coated additive.

### Claim 18 (depends on 17)

The hydrogen fuel cell stack of claim 17, wherein the first layer of the perfluorosulfonic acid ionomer exhibits a first thickness in the range of 4 micrometers to 15 micrometers, the expanded polytetrafluoroethylene membrane exhibits a second thickness in the range of 2 micrometers to 10 micrometers, and the second layer of perfluorosulfonic acid ionomer exhibits a third thickness in the range of 2 micrometers to 15 micrometers, wherein the first thickness is greater than the third thickness.

### Claim 19 (depends on 12)

The hydrogen fuel cell stack of claim 12, further comprising sealing gaskets positioned on either side of each membrane electrode assembly; a bi-polar plate positioned on either side of the membrane electrode assembly, wherein each sealing gaskets is positioned between the membrane electrode assembly and one of the bi-polar plates; and a current collector plate positioned on adjacent each bi-polar plate externally to the membrane electrode assembly.

### Claim 20

A method of forming a proton exchange membrane, comprising:
dispersing an additive in methoxy-nonafluorobutane;
coating the additive with methoxy-nonafluorobutane while dispersing;
separating the coated additive from excess methoxy-nonafluorobutane;
drying the coated additive;
combining the coated additive and a perfluorosulfonic acid ionomer solution in a solution of alcohol and water to form an ionomer dispersion;
forming the ionomer dispersion into the proton exchange membrane;
drying the proton exchange membrane; and
validating the proton conductivity of the proton exchange membrane using four probe electrochemical impedance spectroscopy at one or more relative humidities in the range of 40 percent to 100 percent.