# US 2026/0074238 A1 · Metal Film and Method of Manufacturing the Metal Film

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0074238 A1
- Document ID: US20260074238A1
- Status: Published application
- Kind: A1
- Application number: 19/318,509
- Filed: 2025-09-04
- Published: 2026-03-12
- Earliest claimed: 2024-09-11
- Assignees: SK On Co., Ltd.
- Applicants: SK On Co., Ltd.
- Inventors: Chang Mook HWANG; Hyun Ji KIM; Jong Hyeok LEE; Yoon Ji JO
- Web page: https://patentgrep.com/patent/US20260074238A1

## CPC

- H01M 4/70: characterised by shape or form
- C25D 1/04: Wires; Strips; Foils
- C25D 3/38: of copper
- C25D 3/44: Aluminium
- H01M 4/661: {Metal or alloys, e.g. alloy coatings (H01M4/669 take precedence)}
- H01M 4/667: {in the form of layers, e.g. coatings}
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- C25D: PROCESSES FOR THE ELECTROLYTIC OR ELECTROPHORETIC PRODUCTION OF COATINGS; ELECTROFORMING; APPARATUS THEREFOR
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

The present disclosure can minimize the problem that the inner and outer surfaces deteriorate due to stress caused by compression and stress caused by elongation, respectively, during bending. Furthermore, the present disclosure can prevent surface cracking and lithium precipitation due to stresses applied during bending. Furthermore, the present disclosure can improve the problem of different electrode densities on the inner and outer surfaces. Furthermore, the present disclosure can prevent a reduction in the lifetime of the battery.

## Claims

### Claim 1

A metal film comprising:
a first surface; and
a second surface opposite to the first surface;
wherein the metal film has RaR defined by the following Equation 1 in the range of 100 to 2,000,
RaR=Ra1/Ra2×100, [Equation 1]
where the Ra1 denotes the arithmetic mean roughness of the first surface and the Ra2 denotes the arithmetic mean roughness of the second surface.

### Claim 2 (depends on 1)

The metal film according to claim 1, wherein the metal film is included in the current collector of a battery.

### Claim 3 (depends on 1)

The metal film according to claim 1, wherein the metal film has a tensile strength in the range of 10 kg/cm2 to 100 kg/cm2.

### Claim 4 (depends on 1)

The metal film according to claim 1, wherein the metal film has a bending number of at least 3,000 times until fracture.

### Claim 5 (depends on 1)

The metal film according to claim 1, further comprising: a halogen element.

### Claim 6 (depends on 5)

The metal film according to claim 5, wherein the halogen element comprises at least one selected from the group consisting of chlorine and iodine.

### Claim 7 (depends on 6)

The metal film according to claim 6, wherein the metal film comprises chlorine in the range of 1 wt % to 30 wt % by total weight.

### Claim 8 (depends on 6)

The metal film according to claim 6, wherein the metal film comprises iodine in the range of 0.001 wt % to 0.1 wt % by total weight.

### Claim 9 (depends on 1)

The metal film according to claim 1, wherein crystal grains are formed on the first and second surfaces.

### Claim 10 (depends on 1)

The metal film according to claim 1, further comprising: copper or aluminum.

### Claim 11

A method of manufacturing a metal film, comprising:
a step of contacting at least a portion of a metal sheet including a first surface and a second surface opposite to the first surface with a first electrolyte solution containing metal ions and withdrawing out the metal film;
wherein the metal film has RaR defined by the following Equation 1 in the range of 100 to 2,000,
RaR=Ra1/Ra2×100, [Equation 1]
where the Ra1 denotes the arithmetic mean roughness of a first surface of the metal film and the Ra2 denotes the arithmetic mean roughness of a second surface of the metal film.

### Claim 12 (depends on 11)

The method according to claim 11, wherein the first surface of the metal sheet reacts with the first electrolyte solution.

### Claim 13 (depends on 11)

The method according to claim 11, wherein the second surface of the metal sheet is not substantially reactive with the first electrolyte solution.

### Claim 14 (depends on 11)

The method according to claim 11, wherein the metal ions contained in the first electrolyte solution are aluminum ions or copper ions, the first electrolyte solution further comprises at least one selected from the group consisting of chlorine ions and iodine ions.

### Claim 15 (depends on 14)

The method according to claim 14, wherein the first electrolyte solution comprises chlorine ions in the range of 0.1 mg/L to 1 mg/L.

### Claim 16 (depends on 14)

The method according to claim 14, wherein the first electrolyte solution comprises iodine ions in the range of 1 mg/L to 10 mg/L.

### Claim 17 (depends on 11)

The method according to claim 11, wherein the metal sheet is prepared by electroplating with a second electrolyte solution containing metal ions.

### Claim 18 (depends on 17)

The method according to claim 17, wherein the second electrolyte solution further comprises gelatin.

### Claim 19 (depends on 1)

An electrode comprising:
a current collector; and
an active material layer formed on at least one surface of the current collector;
wherein the current collector comprises the metal film of claim 1.