# US 2026/0074230 A1 · Modified electrode plate, preparation method thereof, secondary battery, and electric apparatus

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0074230 A1
- Document ID: US20260074230A1
- Status: Published application
- Kind: A1
- Application number: 19/365,237
- Filed: 2025-10-22
- Published: 2026-03-12
- Earliest claimed: 2023-09-22
- Assignees: Contemporary Amperex Technology Co., Limited
- Applicants: Contemporary Amperex Technology Co., Limited
- Inventors: Kai WU; Yuejuan WAN; Bingkun GUO; Xinxin ZHANG; Longchao XU
- Web page: https://patentgrep.com/patent/US20260074230A1

## CPC

- H01M 4/628: {Inhibitors, e.g. gassing inhibitors, corrosion inhibitors}
- H01M 10/054: Accumulators with insertion or intercalation of metals other than lithium, e.g. with magnesium or aluminium
- H01M 4/0402: {Methods of deposition of the material}
- H01M 4/0497: {Chemical precipitation}
- H01M 4/13: Electrodes for accumulators with non-aqueous electrolyte, e.g. for lithium-accumulators; Processes of manufacture thereof
- H01M 4/139: Processes of manufacture
- H01M 4/587: for inserting or intercalating light metals
- H01M 10/052: Li-accumulators
- H01M 10/4235: {Safety or regulating additives or arrangements in electrodes, separators or electrolyte (H01M10/4242 takes precedence)}
- H01M 2004/021: {Physical characteristics, e.g. porosity, surface area}
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A modified electrode plate includes an electrode plate, the electrode plate having element sodium or element lithium on its surface, and the electrode plate including a pre-lithiated negative electrode plate or a pre-sodiated negative electrode plate; a protective film, the protective film including a first group and a hydrophobic group, the first group being attached to the surface of the electrode plate, and the hydrophobic group being distal from the electrode plate and the hydrophobic group including a hydrophobic group and being exposed on a surface of the protective film. Disposing the protective film having the hydrophobic group on the surface of the electrode plate can effectively block water, oxygen, or carbon dioxide in the air so as to effectively prevent water, oxygen, or carbon dioxide from passing through the protective layer to react with active components in the electrode plate.

## Claims

### Claim 1

A modified electrode plate comprising:
an electrode plate, the electrode plate having element sodium or element lithium on its surface, and the electrode plate comprising a pre-lithiated negative electrode plate or a pre-sodiated negative electrode plate; and
a protective film, the protective film comprising a first group and a hydrophobic group, the first group being attached to the surface of the electrode plate, the hydrophobic group being distal from the electrode plate, and the hydrophobic group being exposed on a surface of the protective film.

### Claim 2 (depends on 1)

The modified electrode plate according to claim 1, wherein the first group comprises any one or more of a phosphate group, a halogenated silyl group, a siloxane group, a thiol group, a carboxylic acid group, or —N═N—; and/or
the hydrophobic group comprises any one or more of a C6-C20 aryl group, a C1-C50 alkyl group, or a C1-C50 halogenated alkyl group.

### Claim 3 (depends on 1)

The modified electrode plate according to claim 1, wherein the hydrophobic group comprises any one or more of a C6-C10 aryl group, a C1-C40 alkyl group, or a C1-C30 halogenated alkyl group.

### Claim 4 (depends on 1)

The modified electrode plate according to claim 1, wherein the protective film comprises any one or more of a C1-C50 alkyl phosphonate film, a C1-C50 alkyl chlorosilane film, a C1-C50 fluorinated alkyl siloxane film, a C1-C50 thiol film, or a benzotriazole film.

### Claim 5 (depends on 4)

The modified electrode plate according to claim 4, wherein the protective film comprises any one or more of a C1-C40 alkyl phosphonate film, a C1-C30 alkyl chlorosilane film, a C1-C30 fluorinated alkyl siloxane film, or a C1-C10 thiol film.

### Claim 6 (depends on 5)

The modified electrode plate according to claim 5, wherein the C1-C40 alkyl phosphonate film comprises any one or more of a propyl phosphonate film, an octadecyl phosphonate film, or a dihexadecyl phosphonate film;
the C1-C30 alkyl chlorosilane film comprises any one or more of an n-propyltrichlorosilane film, an isopropyltrichlorosilane film, an n-butyltrichlorosilane film, a tert-butyltrichlorosilane film, an n-hexyltrichlorosilane film, an n-heptyltrichlorosilane film, a tridecyltrichlorosilane film, a tetradecyltrichlorosilane film, an octadecyltrichlorosilane film, or a tricosyltrichlorosilane film;
the C1-C30 fluorinated alkyl siloxane film comprises any one or more of a heptadecafluorodecyl-trimethoxysilane film or a trifluoropropyl-trimethoxysilane film; or
the C1-C10 thiol film comprises any one or more of an n-propylthiol film, an ethylthiol film, an isopropylthiol film, an n-butylthiol film, a tert-butylthiol film, an n-pentylthiol film, an n-hexylthiol film, or an n-decylthiol film.

### Claim 7 (depends on 1)

The modified electrode plate according to claim 1, wherein the modified electrode plate comprises a current collector and an active layer disposed on at least one surface of the current collector, the protective film being attached to the active layer,
the protective film comprises a C1-C50 alkyl phosphonate film, wherein a mass content of element P in the total elements of the active layer and the protective film of the modified electrode plate is 300 ppm to 500 ppm;
the protective film comprises a C1-C50 alkyl chlorosilane film, wherein a mass content of element Si in the total elements of the active layer and the protective film of the modified electrode plate is 250 ppm to 400 ppm, and a mass content of element Cl in the total elements of the active layer and the protective film of the modified electrode plate is 300 ppm to 500 ppm;
the protective film comprises a C1-C50 fluorinated alkyl siloxane film, wherein a mass content of element Si in the total elements of the active layer and the protective film of the modified electrode plate is 250 ppm to 400 ppm, and a mass content of element F in the total elements of the active layer and the protective film of the modified electrode plate is 500 ppm to 750 ppm; or
the protective film comprises a C1-C50 thiol film, wherein a mass content of element S in the total elements of the active layer and the protective film of the modified electrode plate is 100 ppm to 300 ppm.

### Claim 8 (depends on 1)

The modified electrode plate according to claim 1, wherein a water contact angle of the modified electrode plate is 65° to 85°.

### Claim 9 (depends on 1)

The modified electrode plate according to claim 1, wherein the protective film is a self-assembled monolayer film.

### Claim 10 (depends on 1)

The modified electrode plate according to claim 1, wherein the pre-lithiated negative electrode plate comprises any one or more of a metallic lithium pre-lithiated negative electrode plate, a lithium alloy pre-lithiated negative electrode plate, or an organic lithium pre-lithiated negative electrode plate; or
the pre-sodiated negative electrode plate comprises any one or more of a metallic sodium pre-sodiated negative electrode plate, an electrochemical pre-sodiated negative electrode plate, or an organic sodium pre-sodiated negative electrode plate.

### Claim 11 (depends on 1)

A preparation method of the modified electrode plate according to claim 1, wherein the preparation method comprises:
preparing a protective agent solution, the protective agent comprising a first group and a hydrophobic group; and
immersing an electrode plate in the protective agent solution for a predetermined time, the electrode plate having element sodium or element lithium on its surface, such that the first group is attached to the surface of the electrode plate, and the hydrophobic group is distal from the electrode plate to form a protective film, thereby obtaining the modified electrode plate.

### Claim 12 (depends on 11)

The preparation method according to claim 11, wherein a solvent of the protective agent solution comprises an ether solvent.

### Claim 13 (depends on 11)

The preparation method according to claim 11, wherein the ether solvent comprises ethylene glycol dimethyl ether, diethylene glycol dimethyl ether, triethylene glycol dimethyl ether, tetraethylene glycol dimethyl ether, tetrahydrofuran, methyl tetrahydrofuran, or 1,3-dioxolane.

### Claim 14 (depends on 11)

The preparation method according to claim 11, wherein a concentration of the protective agent solution is 0.01 wt % to 5 wt %.

### Claim 15 (depends on 14)

The preparation method according to claim 14, wherein the concentration of the protective agent solution is 0.5 wt % to 3 wt %.

### Claim 16 (depends on 11)

The preparation method according to claim 11, wherein the predetermined time is 2 min to 30 min.

### Claim 17 (depends on 16)

The preparation method according to claim 16, wherein the predetermined time is 10 min to 20 min.

### Claim 18 (depends on 1)

A secondary battery comprising a positive electrode plate, a negative electrode plate, and an electrolyte, wherein the positive electrode plate or the negative electrode plate comprises the modified electrode plate according to claim 1.

### Claim 19 (depends on 18)

An electric apparatus comprising a secondary battery, wherein the secondary battery comprises the secondary battery according to claim 18.