- Number: US 2026/0074222 A1
- Document ID: US20260074222A1
- Status: Published application
- Kind: A1
- Application number: 18/830,821
- Filed: 2024-09-11
- Published: 2026-03-12
- Earliest claimed: 2024-09-11
- Assignees: Ford Global Technologies, LLC
- Applicants: Ford Global Technologies, LLC
- Inventors: Sookyung JEONG; Eun Young GOH; Sangil HAN; Keonseok OH; Michael LERNER; Chi PAIK
- Web page: https://patentgrep.com/patent/US20260074222A1

## CPC

- H01M 4/583: Carbonaceous material, e.g. graphite-intercalation compounds or CFx
- H01M 4/0404: {by coating on electrode collectors}
- H01M 4/133: Electrodes based on carbonaceous material, e.g. graphite-intercalation compounds or CFx
- H01M 4/1393: of electrodes based on carbonaceous material, e.g. graphite-intercalation compounds or CFx
- H01M 4/587: for inserting or intercalating light metals
- H01M 4/661: {Metal or alloys, e.g. alloy coatings (H01M4/669 take precedence)}
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- H01M 2004/021: {Physical characteristics, e.g. porosity, surface area}
- H01M 2004/027: {Negative electrodes}
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A battery including a positive electrode assembly and a negative electrode assembly with a porous matrix of graphite-based active material, and lithiophilic nanoparticles occupying pores defined by the porous matrix, is presented. The negative electrode assembly may be formed by loading nickel nanoparticles into graphite, hydrogenating the negative electrode assembly to create porosity within the negative electrode assembly, and galvanizing the negative electrode assembly with silver to replace the nickel nanoparticles.

## Claims

### Claim 1

A battery comprising:
a positive electrode assembly; and
a negative electrode assembly with a porous matrix of graphite-based active material, and lithiophilic nanoparticles occupying pores defined by the porous matrix.

### Claim 2 (depends on 1)

The battery of claim 1 wherein the lithiophilic nanoparticles are silver nanoparticles.

### Claim 3 (depends on 1)

The battery of claim 1 wherein the lithiophilic nanoparticles are configured to form a solid solution with lithium in the negative electrode assembly.

### Claim 4 (depends on 1)

The battery of claim 1 wherein the porous matrix of graphite-based active material has an increased edge surface area compared to non-porous graphite-based active material.

### Claim 5 (depends on 1)

The battery of claim 1 wherein the lithiophilic nanoparticles are in a range of 0.1 to 10 weight percent of the negative electrode assembly.

### Claim 6 (depends on 1)

The battery of claim 1 wherein the porous matrix has a porosity of 10 to 50 percent.

### Claim 7 (depends on 1)

The battery of claim 1 wherein the lithiophilic nanoparticles have an average diameter between 5 to 100 nanometers.

### Claim 8

An electrode assembly comprising:
a current collector; and
a graphite-based active material layer, with electrocatalytic nanoparticles interspersed between particles of the graphite-based active material layer, deposited on the current collector.

### Claim 9 (depends on 8)

The electrode assembly of claim 8 wherein the graphite-based active material layer has a porous structure.

### Claim 10 (depends on 8)

The electrode assembly of claim 8 wherein the electrocatalytic nanoparticles are silver nanoparticles.

### Claim 11 (depends on 8)

The electrode assembly of claim 8 wherein the electrocatalytic nanoparticles are present both on surfaces of the graphite-based active material layer and within pores of the graphite-based active material layer.

### Claim 12 (depends on 8)

The electrode assembly of claim 8 wherein the graphite-based active material layer has a thickness of 50 to 200 micrometers.

### Claim 13 (depends on 8)

The electrode assembly of claim 8 wherein the electrode assembly is a negative electrode assembly.

### Claim 14 (depends on 8)

The electrode assembly of claim 8 wherein the current collector is a copper foil.

### Claim 15

A method of forming an electrode comprising:
loading nickel nanoparticles into a graphite active material to form a nickel-loaded graphite active material;
hydrogenating the nickel-loaded graphite active material to form a porous graphite active material; and
galvanizing the porous graphite active material with a silver salt solution to replace nickel nanoparticles with silver nanoparticles to form the electrode.

### Claim 16 (depends on 15)

The method of claim 15 wherein the hydrogenating is performed at a temperature range of 600 to 900 degrees Celsius.

### Claim 17 (depends on 15)

The method of claim 15 wherein the galvanizing is performed at room temperature.

### Claim 18 (depends on 15)

The method of claim 15, further comprising controlling a radius of the silver nanoparticles by adjusting an amount of silver salt.

### Claim 19 (depends on 15)

The method of claim 15, further comprising depositing the formed electrode on a current collector.

### Claim 20 (depends on 15)

The method of claim 15 wherein the porous graphite active material has an increased surface area compared to the nickel-loaded graphite active material.