# US 2026/0074219 A1 · Cathode active material for lithium secondary batteries, method of preparing same, cathode including the same, and lithium secondary battery including cathode

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0074219 A1
- Document ID: US20260074219A1
- Status: Published application
- Kind: A1
- Application number: 19/388,147
- Filed: 2025-11-13
- Published: 2026-03-12
- Earliest claimed: 2021-08-18
- Assignees: Samsung SDI Co., Ltd.
- Applicants: Samsung SDI Co., Ltd.
- Inventors: Jangwook Lee; Wooyoung Yang; Ickkyu Choi
- Web page: https://patentgrep.com/patent/US20260074219A1

## CPC

- C01G 51/50: of the type (MnO2)n-, e.g. Li(CoxMn1-x)O2 or Li(MyCoxMn1-x-y)O2
- H01M 4/525: of mixed oxides or hydroxides containing iron, cobalt or nickel for inserting or intercalating light metals, e.g. LiNiO2, LiCoO2 or LiCoOxFy
- C01G 51/42: containing alkali metals, e.g. LiCoO2
- C01G 51/82: Compounds containing cobalt, with or without oxygen or hydrogen, and containing two or more other elements
- H01M 4/0404: {by coating on electrode collectors}
- H01M 4/0471: {involving thermal treatment, e.g. firing, sintering, backing particulate active material, thermal decomposition, pyrolysis}
- H01M 4/366: {as layered products}
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- C01P 2002/74: by peak-intensities or a ratio thereof only
- C01P 2004/03: obtained by SEM
- C01P 2004/34: hollow
- C01P 2004/61: Micrometer sized, i.e. from 1-100 micrometer
- C01P 2006/12: Surface area
- C01P 2006/16: Pore diameter
- C01P 2006/20: Powder free flowing behaviour
- C01P 2006/40: Electric properties
- H01M 2004/021: {Physical characteristics, e.g. porosity, surface area}
- H01M 2004/028: {Positive electrodes}
- Y02E 60/10: Energy storage using batteries
- C01G: COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSES C01D OR C01F (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts or peroxyacids C01B15/00; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium, or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds containing nitrogen, other non-metals and metal C01B21/082}; metal amides C01B21/092; nitrites C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; compounds having molecular sieve properties but not having base-exchange properties C01B37/00; compounds having molecular sieve and base-exchange properties, e.g. crystalline zeolites, C01B39/00; cyanides C01C3/08; salts of cyanamide C01C3/16; thiocyanates C01C3/20)
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A cathode active material for lithium secondary batteries, a method of preparing the same, a cathode including the same, and a lithium secondary battery including the cathode are provided. The cathode active material includes nickel-based lithium metal oxide secondary particles each including a plurality of large primary particles, the nickel-based lithium metal oxide secondary particles having a hollow structure having pores therein, each of the plurality of large primary particles having a size of about 2 μm to about 6 μm, and each of the nickel-based lithium metal oxide secondary particles having a size of about 10 μm to about 18 μm; and a cobalt compound-containing coating layer on surfaces of the nickel-based lithium metal oxide secondary particles.

## Claims

### Claim 1

A cathode active material for lithium secondary batteries, the cathode active material comprising:
nickel-based lithium metal oxide secondary particles each comprising a plurality of primary particles, the nickel-based lithium metal oxide secondary particles having a hollow structure having pores therein, and
a cobalt compound-containing coating layer on surfaces of the nickel-based lithium metal oxide secondary particles,
wherein a peak intensity ratio (I(003)/I(104)) of the cathode active material, is in a range of 1.2 to 4.0.

### Claim 2 (depends on 1)

The cathode active material of claim 1, wherein at least one of the surfaces or grain boundaries of the plurality of primary particles comprises the cobalt compound-containing coating layer.

### Claim 3 (depends on 1)

The cathode active material of claim 1, wherein a content of a cobalt compound in the cobalt compound-containing coating layer is about 0.1 mol % to about 5.0 mol % based on a total content of the cathode active material.

### Claim 4 (depends on 1)

The cathode active material of claim 1, wherein the cobalt compound-containing coating layer has a thickness of about 1 nm to about 50 nm.

### Claim 5 (depends on 1)

The cathode active material of claim 1, wherein, in the cobalt compound-containing coating layer, a cobalt compound is cobalt oxide, lithium cobalt oxide, or a combination thereof.

### Claim 6 (depends on 5)

The cathode active material of claim 5, wherein the cobalt compound-containing coating layer further comprises at least one of boron, manganese, phosphorus, aluminum, zinc, zirconium, or titanium.

### Claim 7 (depends on 5)

The cathode active material of claim 5, wherein the pores have a size of 0.5 μm to 4 μm.

### Claim 8 (depends on 1)

The cathode active material of claim 1, wherein the nickel-based lithium metal oxide secondary particles comprise a compound represented by Formula 1 below:
wherein in Formula 1, M1 is at least one of Co, Mn, of Al,
M2 is at least one of boron (B), magnesium (Mg), calcium (Ca), strontium (Sr), barium (Ba), titanium (Ti), vanadium (V), chromium (Cr), iron (Fe), copper (Cu)), or zirconium (Zr), and
0.95≤a≤1.1, 0.6≤(1−x−y)<1, 0≤x<0.4, 0≤y<0.4, and 0≤α1≤0.1, and wherein a case in which both x and y are 0 is excluded.

### Claim 9 (depends on 1)

The cathode active material of claim 1, wherein the nickel-based lithium metal oxide secondary particles comprise a compound represented by Formula 2 below:
wherein in Formula 2, M3 is at least one of Mn or Al,
M4 is at least one of boron (B), magnesium (Mg), calcium (Ca), strontium (Sr), barium (Ba), titanium (Ti), vanadium (V), chromium (Cr), iron (Fe), copper (Cu), or zirconium (Zr), and
0.95≤a≤1.1, 0.6≤(1−x−y−z)<1, 0≤x<0.4, 0≤y<0.4, 0≤z<0.4, and 0≤α1≤0.1, and wherein a case in which all of x, y, and z are 0 is excluded.

### Claim 10 (depends on 1)

The cathode active material of claim 1, wherein the plurality of primary particles have a size of about 2 μm to about 4 μm, and the nickel-based lithium metal oxide secondary particles have a size of about 12 μm to about 18 μm.

### Claim 11 (depends on 1)

The cathode active material of claim 1, wherein an area ratio A(003)/A(104) of the cathode active material, measured by X-ray diffraction analysis, is about 1.1 to about 1.4.

### Claim 12

A method of preparing a cathode active material for lithium secondary batteries, the method comprising:
mixing a nickel precursor, at least one of an M1 precursor or an M2 precursor, and a basic solution to obtain a mixture,
subjecting the mixture to a co-precipitation reaction, and then drying the mixture to obtain a nickel-based metal precursor having pores therein;
obtaining a mixture of the nickel-based metal precursor having pores therein and a lithium precursor;
performing a primary heat treatment of the mixture to obtain a product of the primary heat treatment; and
adding a cobalt precursor to the product of the primary heat treatment without a pulverization process of the product, to obtain a mixture, and performing a secondary heat treatment of the mixture to prepare the cathode active material,
wherein the primary heat treatment is performed at a higher temperature than the secondary heat treatment,
the M1 precursor is at least one of a cobalt precursor, a manganese precursor, or an aluminum precursor,
the M2 precursor contains at least one of boron (B), magnesium (Mg), calcium (Ca), strontium (Sr), barium (Ba), titanium (Ti), vanadium (V), chromium (Cr), iron (Fe), copper (Cu), or zirconium (Zr), and
during the co-precipitation reaction, a pH of the mixture is adjusted in two steps, a second step is carried out at a lower pH than a first step, and a difference in pH between the first step and the second step is 0.1 to 1.5.

### Claim 13 (depends on 12)

The method of claim 12, wherein the nickel-based metal precursor has a pore region therein, and a size of the pore region is about 2 μm to about 7 μm.

### Claim 14 (depends on 12)

The method of claim 12, wherein the cobalt precursor is Co(OH)2, CoOOH, CoO, Co2O3, Co3O4, Co(OCOCH3)2·4H2O, CoCl2, Co(NO3)2·6H2O, CoSO4, Co(SO4)2·7H2O, or a combination thereof.

### Claim 15 (depends on 12)

The method of claim 12, wherein the nickel-based metal precursor is a compound represented by Formula 3 below, a compound represented by Formula 4 below, or a combination thereof:
wherein, in Formula 3, M1 is at least one of Co, Mn, or Al,
M2 is at least one of boron (B), magnesium (Mg), calcium (Ca), strontium (Sr), barium (Ba), titanium (Ti), vanadium (V), chromium (Cr), iron (Fe), copper (Cu), of zirconium (Zr), and
0.6≤(1−x−y)<1, 0≤x<0.4, and 0≤y<0.4, and wherein a case in which both x and y are 0 is excluded, and
wherein, in Formula 4, M1 is at least one of Co, Mn, or Al,
M2 is at least one of boron (B), magnesium (Mg), calcium (Ca), strontium (Sr), barium (Ba), titanium (Ti), vanadium (V), chromium (Cr), iron (Fe), copper (Cu), or zirconium (Zr), and
0.6≤(1−x−y)<1, 0≤x<0.4, and 0≤y<0.4, and wherein a case in which both x and y are 0 is excluded.

### Claim 16 (depends on 12)

The method of claim 12, wherein the nickel-based metal precursor is a compound represented by Formula 5 below, a compound represented by Formula 6 below, or a combination thereof:
wherein, in Formula 5, M3 is at least one of Mn or Al,
M4 is at least one of boron (B), magnesium (Mg), calcium (Ca), strontium (Sr), barium (Ba), titanium (Ti), vanadium (V), chromium (Cr), iron (Fe), copper (Cu), or zirconium (Zr), and
0.6≤(1−x−y−z)<1, 0≤x<0.4, 0≤y<0.4, and 0≤z<0.4, and wherein a case in which all of x, y, and z are 0 is excluded, and
wherein, in Formula 6, M3 is at least one of Mn or Al,
M4 is at least one of boron (B), magnesium (Mg), calcium (Ca), strontium (Sr), barium (Ba), titanium (Ti), vanadium (V), chromium (Cr), iron (Fe), copper (Cu), or zirconium (Zr), and
0.6≤(1−x−y−z)<1, 0≤x<0.4, 0≤y<0.4, and 0≤z<0.4, and wherein a case in which all of x, y, and z are 0 is excluded.

### Claim 17 (depends on 12)

The method of claim 12, wherein the nickel-based metal precursor and the lithium precursor are mixed such that a molar ratio of Li/Me, wherein Me is an element other than Li, O, and H, is 0.9 or more and less than 1.1.

### Claim 18 (depends on 12)

The method of claim 12, wherein the lithium precursor is lithium hydroxide, lithium carbonate, lithium sulfate, lithium nitrate, or a combination thereof.

### Claim 19 (depends on 12)

The method of claim 12, wherein the primary heat treatment is performed at a temperature of 800° C. to 1200° C. under an oxidizing gas atmosphere.

### Claim 20 (depends on 12)

The method of claim 12, wherein the secondary heat treatment is performed at a temperature of 600° C. to 850° C. under an oxidizing gas atmosphere.

### Claim 21 (depends on 1)

A cathode for lithium secondary batteries, the cathode comprising:
a cathode current collector, and
a cathode active material layer on the cathode current collector,
wherein the cathode active material layer comprises:
the cathode active material of claim 1; and
at least one of particles or aggregates thereof, the particles having the same composition as the cathode active material.

### Claim 22 (depends on 21)

The cathode of claim 21, wherein the pores has a size in a range of 0.5 μm to 4 μm.

### Claim 23 (depends on 21)

The cathode of claim 21, wherein a greater amount of the particles are in a surface portion of the cathode than in a central portion of the cathode, the central portion being adjacent to the cathode current collector.

### Claim 24 (depends on 21)

The cathode of claim 21, wherein a larger amount the cathode active material comprising the secondary particles having the hollow structure are in a central portion of the cathode than in a surface portion of the cathode, the central portion being adjacent to the cathode current collector.

### Claim 25 (depends on 21)

The cathode of claim 21, wherein the cathode active material layer has a single layer or two-layer structure.

### Claim 26 (depends on 21)

A lithium secondary battery comprising:
the cathode of claim 21;
an anode; and
an electrolyte between the cathode and the anode.