# US 2026/0074216 A1 · Positive electrode for all-solid-state battery, all-solid-state battery including the same, and method of manufacturing the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0074216 A1
- Document ID: US20260074216A1
- Status: Published application
- Kind: A1
- Application number: 19/275,745
- Filed: 2025-07-21
- Published: 2026-03-12
- Earliest claimed: 2024-09-12
- Assignees: Samsung SDI Co., Ltd.
- Applicants: Samsung SDI Co., Ltd.
- Inventors: Jinhee KIM; Hoseon YOU; Dongwoo KANG; Daeyang OH
- Web page: https://patentgrep.com/patent/US20260074216A1

## CPC

- H01M 4/525: of mixed oxides or hydroxides containing iron, cobalt or nickel for inserting or intercalating light metals, e.g. LiNiO2, LiCoO2 or LiCoOxFy
- H01M 4/0404: {by coating on electrode collectors}
- H01M 4/131: Electrodes based on mixed oxides or hydroxides, or on mixtures of oxides or hydroxides, e.g. LiCoOx
- H01M 4/136: Electrodes based on inorganic compounds other than oxides or hydroxides, e.g. sulfides, selenides, tellurides, halogenides or LiCoFy
- H01M 4/1391: of electrodes based on mixed oxides or hydroxides, or on mixtures of oxides or hydroxides, e.g. LiCoOx
- H01M 4/622: {being polymers}
- H01M 4/623: {fluorinated polymers}
- H01M 4/625: {Carbon or graphite}
- H01M 10/0562: Solid materials
- H01M 10/0585: of accumulators having only flat construction elements, i.e. flat positive electrodes, flat negative electrodes and flat separators
- H01M 2004/028: {Positive electrodes}
- H01M 2300/0068: inorganic
- H01M 2300/008: Halides
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

Disclosed are positive electrodes, all-solid-state batteries, and fabrication methods thereof. The positive electrode includes a positive electrode current collector, and a positive electrode active material layer on the positive electrode current collector. The positive electrode active material layer includes a sulfide-based solid electrolyte, a binder that includes a first non-aqueous binder and a second non-aqueous binder, and a positive electrode active material. The first non-aqueous binder includes a fluorine-based binder. The second non-aqueous binder includes an acrylate-based binder.

## Claims

### Claim 1

A positive electrode for an all-solid-state battery, the positive electrode comprising:
a positive electrode current collector; and
a positive electrode active material layer on the positive electrode current collector,
wherein the positive electrode active material layer comprises:
a sulfide-based solid electrolyte;
a binder that comprises a first non-aqueous binder and a second non-aqueous binder; and
a positive electrode active material,
wherein the first non-aqueous binder comprises a fluorine-based binder, and
wherein the second non-aqueous binder comprises an acrylate-based binder.

### Claim 2 (depends on 1)

The positive electrode of claim 1, wherein the binder in the positive electrode active material layer is present in an amount in a range of about 1 wt % to about 1.5 wt % relative to 100 wt % of the positive electrode active material layer.

### Claim 3 (depends on 1)

The positive electrode of claim 1, wherein an amount of the first non-aqueous binder in the binder is equal to or greater than an amount of the second non-aqueous binder in the binder.

### Claim 4 (depends on 1)

The positive electrode of claim 1, wherein:
the first non-aqueous binder in the binder is present in an amount in a range of about 50 wt % to about 90 wt % relative to 100 wt % of the binder, and
the second non-aqueous binder in the binder is present in an amount in a range of about 10 wt % to about 50 wt % relative to 100 wt % of the binder.

### Claim 5 (depends on 1)

The positive electrode of claim 1, wherein the first non-aqueous binder comprises at least one of poly(vinylidenefluoride-co-hexafluoropropylene) (P(VDF-HFP)), poly(vinylidenefluoride-co-trifluoroethylene) (P(VDF-TrFE)), poly(vinylidenefluoride-co-chlorotrifluoroethylene) (P(VDF-CTFE)), poly(vinylidenefluoride-co-tetrafluoroethylene) (P(VDF-TFE)), and poly(vinylidenefluoride-co-hexafluoropropylene-co-trifluoroethylene) (P(VDF-HFP-TrFE)).

### Claim 6 (depends on 1)

The positive electrode of claim 1, wherein the second non-aqueous binder comprises at least one of polyacrylic acid (PAA), polymethyl methacrylate (PMMA), poly(butyl acrylate), poly(ethyl acrylate), and poly(2-ethylhexyl acrylate).

### Claim 7 (depends on 1)

The positive electrode of claim 1, wherein an adhesive force between the positive electrode active material layer and the positive electrode current collector is in a range of about 0.5 gf/mm to about 2.5 gf/mm.

### Claim 8 (depends on 1)

The positive electrode of claim 1, wherein the sulfide-based solid electrolyte comprises an argyrodite-type compound comprising Li7−aMaPS6−cXc (0≤a≤2 and 0≤c≤2),
wherein X comprises at least one of F, Br, Cl, and I, and
wherein M comprises at least one of scandium (Sc), yttrium (Y), titanium (Ti), zirconium (Zr), hafnium (Hf), vanadium (V), niobium (Nb), tantalum (Ta), chromium (Cr), molybdenum (Mo), tungsten (W), manganese (Mn), technetium (Tc), rhenium (Re), iron (Fe), ruthenium (Ru), osmium (Os), cobalt (Co), rhodium (Rh), iridium (Ir), nickel (Ni), palladium (Pd), platinum (Pt), copper (Cu), silver (Ag), gold (Au), zinc (Zn), cadmium (Cd), mercury (Hg), aluminum (Al), gallium (Ga), indium (In), thallium (Tl), silicon (Si), germanium (Ge), tin (Sn), lead (Pb), arsenic (As), antimony (Sb), and bismuth (Bi).

### Claim 9

A method of manufacturing a positive electrode for an all-solid-state battery, the method comprising:
preparing a slurry; and
coating the slurry on a positive electrode current collector to form a positive electrode active material layer,
wherein preparing the slurry comprises mixing a positive electrode active material, a sulfide-based solid electrolyte, and a binder, in a non-polar solvent, wherein the binder comprises:
a first non-aqueous binder comprising a fluorine-based binder; and
a second non-aqueous binder comprising an acrylate-based binder.

### Claim 10 (depends on 9)

The method of claim 9, wherein the binder in the positive electrode active material layer is present in an amount in a range of about 1 wt % to about 1.5 wt % relative to 100 wt % of the positive electrode active material layer.

### Claim 11 (depends on 9)

The method of claim 9, wherein an amount of the first non-aqueous binder in the binder is equal to or greater than an amount of the second non-aqueous binder in the binder.

### Claim 12 (depends on 9)

The method of claim 9, wherein:
the first non-aqueous binder in the binder is present in an amount in a range of about 50 wt % to about 90 wt % relative to 100 wt % of the binder, and
the second non-aqueous binder in the binder is present in an amount in a range of about 10 wt % to about 50 wt % relative to 100 wt % of the binder.

### Claim 13 (depends on 9)

The method of claim 9, wherein the first non-aqueous binder comprises at least one of poly(vinylidenefluoride-co-hexafluoropropylene) (P(VDF-HFP)), poly(vinylidenefluoride-co-trifluoroethylene) (P(VDF-TrFE)), poly(vinylidenefluoride-co-chlorotrifluoroethylene) (P(VDF-CTFE)), poly(vinylidenefluoride-co-tetrafluoroethylene) (P(VDF-TFE)), and poly(vinylidenefluoride-co-hexafluoropropylene-co-trifluoroethylene) (P(VDF-HFP-TrFE)).

### Claim 14 (depends on 9)

The method of claim 9, wherein the non-polar solvent comprises at least one of butylate, toluene, xylene, anisole, hexane, heptane, dibromomethane, dichloroethane, ethanol, glycol ether, and a combination thereof.

### Claim 15 (depends on 9)

The method of claim 9, wherein the slurry has a viscosity at a temperature of about 20° C. in a range of about 1,000 mPa·s to about 10,000 mPa·s.

### Claim 16 (depends on 9)

The method of claim 9, wherein an adhesive force between the positive electrode active material layer and the positive electrode current collector is in a range of about 0.5 gf/mm to about 2.5 gf/mm.

### Claim 17

An all-solid-state battery, comprising:
a positive electrode layer and a negative electrode layer that are opposite to each other; and
a solid electrolyte layer between the positive electrode layer and the negative electrode layer,
wherein the positive electrode layer comprises a positive electrode current collector and a positive electrode active material layer on the positive electrode current collector,
wherein the positive electrode active material layer comprises a positive electrode active material, a binder, and a sulfide-based solid electrolyte, and
wherein the binder comprises:
a first non-aqueous binder comprising a fluorine-based binder; and
a second non-aqueous binder comprising an acrylate-based binder.

### Claim 18 (depends on 17)

The all-solid-state battery of claim 17, wherein the binder in the positive electrode active material layer is present in an amount in a range of about 1 wt % to about 1.5 wt % relative to 100 wt % of the positive electrode active material layer.

### Claim 19 (depends on 17)

The all-solid-state battery of claim 17, wherein:
the first non-aqueous binder in the binder is present in an amount in a range of about 50 wt % to about 90 wt % relative to 100 wt % of the binder, and
the second non-aqueous binder in the binder is present in an amount in a range of about 10 wt % to about 50 wt % relative to 100 wt % of the binder.

### Claim 20 (depends on 17)

The all-solid-state battery of claim 17, wherein the first non-aqueous binder comprises at least one of poly(vinylidenefluoride-co-hexafluoropropylene) (P(VDF-HFP)), poly(vinylidenefluoride-co-trifluoroethylene) (P(VDF-TrFE)), poly(vinylidenefluoride-co-chlorotrifluoroethylene) (P(VDF-CTFE)), poly(vinylidenefluoride-co-tetrafluoroethylene) (P(VDF-TFE)), and poly(vinylidenefluoride-co-hexafluoropropylene-co-trifluoroethylene) (P(VDF-HFP-TrFE)).