# US 2026/0074203 A1 · Lithium-metal secondary battery and method for manufacturing the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0074203 A1
- Document ID: US20260074203A1
- Status: Published application
- Kind: A1
- Application number: 19/394,881
- Filed: 2025-11-20
- Published: 2026-03-12
- Earliest claimed: 2022-03-29
- Assignees: Honda Motor Co., Ltd.
- Applicants: Honda Motor Co., Ltd.
- Inventors: Kazuki SAIMEN; Ken BABA
- Web page: https://patentgrep.com/patent/US20260074203A1

## CPC

- H01M 4/382: {Lithium (H01M4/405 takes precedence)}
- H01M 4/0445: {Forming after manufacture of the electrode, e.g. first charge, cycling}
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- H01M 50/46: Separators, membranes or diaphragms characterised by their combination with electrodes
- H01M 2004/021: {Physical characteristics, e.g. porosity, surface area}
- H01M 2004/027: {Negative electrodes}
- Y02E 60/10: Energy storage using batteries
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

A lithium-metal secondary battery, which includes a highly reduction-resistant electrolytic solution, including 2 to 6 mol of electrolyte per L of solvent and also having a lithium deposition dissolution efficiency of 98.5% or more, which lithium deposition dissolution efficiency is the proportion of the amount of redissolution of lithium to the amount thereof deposited on the copper surface, wherein the relative density of a lithium metal layer in a negative electrode is 40 to 85%. In addition, a lithium-metal secondary battery, which includes a highly oxidation-resistant electrolytic solution, including 2 to 6 mol of electrolyte per L of solvent and also having a voltage of 5.5 V or more when the current density is 0.4 mA/cm2 using lithium as a counter electrode and platinum as a working electrode, wherein the relative density of a lithium metal layer in a negative electrode is 70 to 95%.

## Claims

### Claim 1

A lithium-metal secondary battery, comprising,
a positive electrode,
a negative electrode having a lithium metal layer,
a separator positioned between the positive electrode and the negative electrode, and
a highly oxidation-resistant electrolytic solution,
comprising 2 to 6 mol of electrolyte per L of solvent and also having a voltage of 5.5 V or more when a current density is 0.4 mA/cm2 using lithium as a counter electrode and platinum as a working electrode,
wherein a relative density of the lithium metal layer is 70 to 95%.