# US 2026/0074196 A1 · Composite anode active material for all-solid-state-battery and manufacturing method thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0074196 A1
- Document ID: US20260074196A1
- Status: Published application
- Kind: A1
- Application number: 18/805,828
- Filed: 2024-08-15
- Published: 2026-03-12
- Earliest claimed: 2023-12-11
- Assignees: Hyundai Motor Company; Kia Corporation
- Applicants: Hyundai Motor Company; Kia Corporation
- Inventors: So Yeon Kim; Hong Suk Choi; Seon Hwa Kim; Dong Hyun Cho; Jae Seok Nam; Jae Min Lim; Hee Soo Kang
- Web page: https://patentgrep.com/patent/US20260074196A1

## CPC

- H01M 4/366: {as layered products}
- H01M 4/0404: {by coating on electrode collectors}
- H01M 4/0407: {by coating on an electrolyte layer}
- H01M 4/364: {as mixtures}
- H01M 4/386: {Silicon or alloys based on silicon}
- H01M 4/583: Carbonaceous material, e.g. graphite-intercalation compounds or CFx
- H01M 4/62: Selection of inactive substances as ingredients for active masses, e.g. binders, fillers
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- H01M 10/0562: Solid materials
- H01M 2004/021: {Physical characteristics, e.g. porosity, surface area}
- H01M 2004/027: {Negative electrodes}
- H01M 2300/0068: inorganic
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

An embodiment composite negative electrode active material for an all-solid-state battery includes a negative electrode active material including a silicon-based active material and a coating layer including a solid electrolyte and coating a portion of a surface of the negative electrode active material, wherein a ratio (E/T) of a Young's modulus (E) of the solid electrolyte to a thickness (T) of the coating layer satisfies 0.02<E/T<0.06.

## Claims

### Claim 1

A composite negative electrode active material for an all-solid-state battery, the composite negative electrode active material comprising:
a negative electrode active material comprising a silicon-based active material; and
a coating layer comprising a solid electrolyte and coating at least a portion of a surface of the negative electrode active material, wherein a ratio (E/T) of a Young's modulus (E) of the solid electrolyte to a thickness (T) of the coating layer satisfies 0.02<E/T<0.06.

### Claim 2 (depends on 1)

The composite negative electrode active material of claim 1, wherein a ratio (T/d) of the thickness (T) of the coating layer to a particle diameter (d) of the negative electrode active material satisfies 20<T/d<100.

### Claim 3 (depends on 2)

The composite negative electrode active material of claim 2, wherein the thickness of the coating layer is in a range of 200 nm to 750 nm.

### Claim 4 (depends on 2)

The composite negative electrode active material of claim 2, wherein the Young's modulus of the solid electrolyte is in a range of 8 GPa to 22 GPa.

### Claim 5 (depends on 2)

The composite negative electrode active material of claim 2, wherein the solid electrolyte coats an entirety of the surface of the negative electrode active material.

### Claim 6 (depends on 2)

The composite negative electrode active material of claim 2, wherein the solid electrolyte comprises a sulfide-based solid electrolyte.

### Claim 7 (depends on 2)

The composite negative electrode active material of claim 2, wherein the silicon-based active material comprises a material selected from the group consisting of a silicon particle, silicon oxide, a silicon alloy, and combinations thereof.

### Claim 8 (depends on 2)

The composite negative electrode active material of claim 2, wherein the silicon-based active material is a composite comprising a carbon-based material.

### Claim 9

A negative electrode active material layer for an all-solid-state battery, the negative electrode active material layer comprising:
a composite negative electrode active material comprising:
a negative electrode active material comprising a silicon-based active material; and
a coating layer comprising a solid electrolyte and coating a portion of a surface of the negative electrode active material, wherein a ratio (E/T) of a Young's modulus (E) of the solid electrolyte to a thickness (T) of the coating layer satisfies 0.02<E/T<0.06, and wherein a ratio (T/d) of the thickness (T) of the coating layer to a particle diameter (d; nm) of the negative electrode active material satisfies 20<T/d<100; and
an electrode solid electrolyte.

### Claim 10 (depends on 9)

The negative electrode active material layer of claim 9, wherein the thickness of the coating layer is in a range of 200 nm to 750 nm.

### Claim 11 (depends on 9)

The negative electrode active material layer of claim 9, wherein the Young's modulus of the solid electrolyte is in a range of 8 GPa to 22 GPa.

### Claim 12 (depends on 9)

The negative electrode active material layer of claim 9, wherein the solid electrolyte coats an entirety of the surface of the negative electrode active material.

### Claim 13 (depends on 9)

The negative electrode active material layer of claim 9, wherein the solid electrolyte comprises a sulfide-based solid electrolyte.

### Claim 14 (depends on 9)

The negative electrode active material layer of claim 9, wherein the silicon-based active material comprises a material selected from the group consisting of a silicon particle, silicon oxide, a silicon alloy, and combinations thereof.

### Claim 15 (depends on 9)

The negative electrode active material layer of claim 9, wherein the silicon-based active material is a composite comprising a carbon-based material.

### Claim 16

A method of forming a composite negative electrode active material layer for an all-solid-state battery, the method comprising:
synthesizing a composite negative electrode active material by introducing a negative electrode active material and a solid electrolyte into a mixer at a weight ratio in a range of 9:1 to 7:3 and then mixing the negative electrode active material and the solid electrolyte;
preparing a negative electrode active material slurry by mixing the composite negative electrode active material and an electrode solid electrolyte; and
forming a negative electrode active material layer by applying and drying the negative electrode active material slurry on a negative electrode current collector.

### Claim 17 (depends on 16)

The method of claim 16, wherein the composite negative electrode active material comprises:
the negative electrode active material comprising a silicon-based active material; and
a coating layer comprising the solid electrolyte and coating a portion of a surface of the negative electrode active material, wherein a ratio (E/T) of a Young's modulus (E) of the solid electrolyte to a thickness (T) of the coating layer satisfies 0.02<E/T<0.06.

### Claim 18 (depends on 17)

The method of claim 17, wherein a ratio (T/d) of the thickness (T) of the coating layer to a particle diameter (d) of the negative electrode active material satisfies 20<T/d<100.

### Claim 19 (depends on 16)

The method of claim 16, wherein the mixer comprises a resonant acoustic mixer (RAM).

### Claim 20 (depends on 16)

The method of claim 16, wherein:
the mixer comprises a plurality of metal balls having a diameter of 10 mm or less; and
a weight ratio of a sum of the negative electrode active material and the solid electrolyte in powder form to the metal balls is in a range of 1:7 to 1:9.