# US 2026/0074113 A1 · LAYERED STRUCTURE OF TiO2 THIN FILM HAVING RUTILE CRYSTAL STRUCTURE AND METHOD FOR FORMING TiO2 THIN FILM HAVING RUTILE CRYSTAL STRUCTURE AND METHOD FOR MANUFACTURING CAPACITOR USING THE SAME

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0074113 A1
- Document ID: US20260074113A1
- Status: Published application
- Kind: A1
- Application number: 19/312,123
- Filed: 2025-08-27
- Published: 2026-03-12
- Earliest claimed: 2024-09-06
- Assignees: Korea Institute of Science and Technology
- Applicants: Korea Institute of Science and Technology
- Inventors: Jihoon JEON; Sunghoon HUR; Ji-Soo JANG; Hyun-Cheol SONG; Seung Hyub BAEK; Chong Yun KANG; Ji-Won CHOI; Jin Sang KIM; Seong Keun KIM
- Web page: https://patentgrep.com/patent/US20260074113A1

## CPC

- H01G 4/1218: {based on titanium oxides or titanates (H01G4/1245 takes precedence)}
- C23C 16/01: on temporary substrates, e.g. substrates subsequently removed by etching
- C23C 16/0281: {of metallic sub-layers (C23C16/029 takes precedence)}
- C23C 16/405: {of refractory metals or yttrium}
- C23C 16/45525: {Atomic layer deposition [ALD]}
- H01G 4/008: Selection of materials
- H01G 4/33: Thin- or thick-film capacitors {(thin- or thick-film circuits; capacitors without a potential-jump or surface barrier specially adapted for integrated circuits, details thereof, multistep manufacturing processes therefor)}
- H01G: CAPACITORS; CAPACITORS, RECTIFIERS, DETECTORS, SWITCHING DEVICES, LIGHT-SENSITIVE OR TEMPERATURE-SENSITIVE DEVICES OF THE ELECTROLYTIC TYPE (selection of specified materials as dielectric H01B3/00; capacitors having potential barriers H10D1/62, H10K10/10)
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)

## Abstract

The present invention relates to a layered structure of a TiO2 thin film having a rutile crystal structure, a method for forming a TiO2 thin film having a rutile crystal structure, and a method for manufacturing a capacitor using the same, which are capable of achieving both deposition of rutile TiO2 at a temperature of 400° C. or less and miniaturization of a device by depositing rutile TiO2 using a material having structural consistency with rutile TiO2, while preventing a material having structural consistency with rutile TiO2 from remaining between a substrate and rutile TiO2.

## Claims

### Claim 1

A layered structure of a TiO2 thin film having a rutile crystal structure, comprising:
a substrate; and
a rutile TiO2 thin film laminated on the substrate,
wherein a crystal structure of the substrate and a crystal structure of the rutile TiO2 thin film are different from each other, and the rutile TiO2 thin film is formed by an atomic layer deposition (ALD) process at 400 ° C. or less.

### Claim 2 (depends on 1)

The layered structure of claim 1, wherein the substrate is one of a semiconductor substrate, a conductive substrate, or an insulating substrate.

### Claim 3 (depends on 1)

The layered structure of claim 1, wherein the substrate is a lower electrode of a capacitor or has a structure in which an insulating layer is provided on the lower electrode.

### Claim 4 (depends on 3)

The layered structure of claim 3, wherein the lower electrode of the capacitor is made of one of TiN, TiAlN, Si, NbN, TaN, or MoN, and the insulating layer is made of one of ZrO2, HfO2, Al2O2, LaOx, TaOx, or NbOx.

### Claim 5 (depends on 3)

The layered structure of claim 3, wherein an upper electrode of the capacitor is further provided on the rutile TiO2 thin film.

### Claim 6

A method for forming a TiO2 thin film having a rutile crystal structure, comprising:
a first step of laminating an ultra-thin film sacrificial layer on a substrate; and
a second step of depositing a rutile TiO2 thin film on the substrate through an atomic layer deposition (ALD) process,
wherein,
in the second step,
a reaction in which the rutile TiO2 thin film is formed on the ultra-thin film sacrificial layer in the form of a metal oxide having structural consistency with rutile TiO2, and a reaction in which the ultra-thin film sacrificial layer in the form of the metal oxide reacts with an oxidizing agent to be converted into a volatile oxide and removed, are carried out.

### Claim 7 (depends on 6)

The method of claim 6, wherein the ultra-thin film sacrificial layer is capable of existing as a metal oxide having structural consistency with rutile TiO2 and is capable of being converted into a volatile oxide, which is a gaseous material, when reacting with an oxidizing agent.

### Claim 8 (depends on 6)

The method of claim 6, wherein a crystal structure of the substrate and a crystal structure of the rutile TiO2 thin film are different from each other.

### Claim 9 (depends on 6)

The method of claim 6, wherein the ultra-thin film sacrificial layer is made of a metal or a metal oxide.

### Claim 10 (depends on 9)

The method of claim 9, wherein the metal is one of Ru, Ir, Mo, V, Sn, or Nb, and the metal oxide is one of RuO2, IrO2, MoO2, VO2, SnO2, or NbO2.

### Claim 11 (depends on 6)

The method of claim 6, wherein, when the ultra-thin film sacrificial layer is made of a metal,
in the second step,
a process in which the metal reacts with an oxidizing agent to be converted into a metal oxide having structural consistency with rutile TiO2, a process in which the rutile TiO2 thin film is formed on the metal oxide having structural consistency with rutile TiO2, and a process in which the metal oxide having structural consistency with rutile TiO2 reacts with the oxidizing agent to be converted into a volatile oxide and removed, are carried out.

### Claim 12 (depends on 6)

The method of claim 6, wherein, when the ultra-thin film sacrificial layer is made of a metal oxide,
in the second step,
a process in which the rutile TiO2 thin film is formed on the metal oxide having structural consistency with rutile TiO2, and a process in which the metal oxide having structural consistency with rutile TiO2 reacts with an oxidizing agent to be converted into a volatile oxide and removed, are carried out.

### Claim 13 (depends on 6)

The method of claim 6, wherein the substrate is one of a semiconductor substrate, a conductive substrate, or an insulating substrate.

### Claim 14 (depends on 6)

The method of claim 6, wherein the substrate is a lower electrode of a capacitor or has a structure in which an insulating layer is provided on the lower electrode.

### Claim 15 (depends on 14)

The method of claim 14, wherein the lower electrode of the capacitor is made of one of TiN, TiAlN, Si, NbN, TaN, or MoN, and the insulating layer is made of one of ZrO2, HfO2, Al2O2, LaOx, TaOx, or NbOx.

### Claim 16 (depends on 6)

The method of claim 6, wherein the ultra-thin film sacrificial layer has a thickness of 6 nm or less.

### Claim 17 (depends on 6)

The method of claim 6, wherein the ultra-thin film sacrificial layer has a thickness of 3 nm or less.

### Claim 18 (depends on 6)

The method of claim 6, wherein the ultra-thin film sacrificial layer has a thickness of 2.5 nm or less.

### Claim 19 (depends on 6)

The method of claim 6, wherein the atomic layer deposition (ALD) process of the second step is carried out at a temperature of 400 °C or less.

### Claim 20 (depends on 6)

The method of claim 6, wherein the atomic layer deposition (ALD) process of the second step comprises:
repeating a titanium precursor supply process and an oxidizing agent supply process, and
wherein the oxidizing agent is supplied by the oxidizing agent supply process, and the oxidizing agent is O3 or O2 plasma.