# US 2026/0074112 A1 · Multilayer ceramic capacitor and method of manufacturing the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0074112 A1
- Document ID: US20260074112A1
- Status: Published application
- Kind: A1
- Application number: 19/057,551
- Filed: 2025-02-19
- Published: 2026-03-12
- Earliest claimed: 2024-09-11
- Assignees: Samsung Electro-Mechanics Co., Ltd.
- Applicants: Samsung Electro-Mechanics Co., Ltd.
- Inventors: Sumin Shin; Sunghwan Lee; Hongseok Kim
- Web page: https://patentgrep.com/patent/US20260074112A1

## CPC

- H01G 4/0085: {Fried electrodes}
- H01G 4/008: Selection of materials
- H01G 4/012: Form of non-self-supporting electrodes
- H01G 4/1209: {characterised by the ceramic dielectric material (H01G4/1272, H01G4/1281 take precedence)}
- H01G 4/1227: {based on alkaline earth titanates}
- H01G 4/30: Stacked capacitors (H01G4/33 takes precedence)
- H01G: CAPACITORS; CAPACITORS, RECTIFIERS, DETECTORS, SWITCHING DEVICES, LIGHT-SENSITIVE OR TEMPERATURE-SENSITIVE DEVICES OF THE ELECTROLYTIC TYPE (selection of specified materials as dielectric H01B3/00; capacitors having potential barriers H10D1/62, H10K10/10)

## Abstract

A multilayer ceramic capacitor including a capacitor body including a dielectric layer and an internal electrode layer, and an external electrode disposed on an outer surface of the capacitor body, wherein the internal electrode layer includes nickel (Ni), and a space lattice edge length of the nickel (Ni) obtained from Equation 1 through X-ray diffraction analysis (XRD) of the internal electrode layer is about 3.522 Å to about 3.544 Å. α = λ · h 2 + k 2 + l 2 2 ⁢ sin ⁢ θ [ Equation ⁢ 1 ] In Equation 1, λ, h, k, l and θ are as defined in the specification.

## Claims

### Claim 1

A multilayer ceramic capacitor, comprising
a capacitor body including a dielectric layer and an internal electrode layer, and
an external electrode disposed on an outer surface of the capacitor body,
wherein the internal electrode layer includes nickel (Ni), and
a space lattice edge length of nickel (Ni) obtained from Equation 1 through X-ray diffraction analysis (XRD) of the internal electrode layer is 3.522 Å to 3.544 Å:
α
=
λ
·
h
2
+
k
2
+
l
2
2
⁢
sin
⁢
θ
[
Equation
⁢
1
]
wherein, in Equation 1:
λ is 1.5406 Å, which is Cu Kα,
h, k, and l are plane indices, and
θ is a Bragg angle.

### Claim 2 (depends on 1)

The multilayer ceramic capacitor of claim 1, wherein
the dielectric layer includes a barium titanate-based compound.

### Claim 3 (depends on 2)

The multilayer ceramic capacitor of claim 2, wherein
a difference between the space lattice edge length of nickel (Ni) in the internal electrode layer and a space lattice edge length of the barium titanate-based compound is 0.492 Å to 0.515 Å, and
the space lattice edge length of the barium titanate-based compound is obtained from Equation 1 through X-ray diffraction analysis (XRD) of the dielectric layer.

### Claim 4 (depends on 1)

The multilayer ceramic capacitor of claim 1, wherein
the internal electrode layer further includes germanium (Ge).

### Claim 5 (depends on 4)

The multilayer ceramic capacitor of claim 4, wherein
germanium (Ge) is disposed inside a lattice of nickel (Ni).

### Claim 6 (depends on 4)

The multilayer ceramic capacitor of claim 4, wherein
the internal electrode layer includes germanium (Ge) in an amount of 0.95 atomic % to 11.95 atomic % based on a total amount of nickel (Ni) and germanium (Ge).

### Claim 7 (depends on 1)

The multilayer ceramic capacitor of claim 1, wherein
the internal electrode layer further includes one or more selected from copper (Cu), silver (Ag), palladium (Pd), gold (Au), and an alloy thereof.

### Claim 8 (depends on 1)

The multilayer ceramic capacitor of claim 1, wherein
the dielectric layer includes germanium (Ge).

### Claim 9 (depends on 1)

The multilayer ceramic capacitor of claim 1, wherein
an average thickness of the internal electrode layer is 0.1 μm to 1 μm.

### Claim 10 (depends on 1)

The multilayer ceramic capacitor of claim 1, wherein
an average thickness of the dielectric layer is 0.1 μm to 8.0 μm.

### Claim 11

A method of manufacturing a multilayer ceramic capacitor, comprising
mixing nickel (Ni) and a germanium (Ge)-based raw material to prepare a conductive paste;
manufacturing a dielectric green sheet from a dielectric slurry, and applying the conductive paste on a surface of the dielectric green sheet to form a conductive paste layer;
manufacturing a dielectric green sheet stack by stacking a plurality of the dielectric green sheet on which the conductive paste layer is formed;
manufacturing a capacitor body including a dielectric layer and an internal electrode layer by firing the dielectric green sheet stack; and
forming an external electrode on an outer surface of the capacitor body,
wherein the internal electrode layer includes nickel (Ni), and
a space lattice edge length of nickel (Ni) obtained from Equation 1 through X-ray diffraction analysis (XRD) of the internal electrode layer is 3.522 Å to 3.544 Å:
α
=
λ
·
h
2
+
k
2
+
l
2
2
⁢
sin
⁢
θ
[
Equation
⁢
1
]
wherein, in Equation 1:
λ is 1.5406 Å, which is Cu Kα,
h, k, and l are plane indices, and
θ is a Bragg angle.

### Claim 12 (depends on 11)

The method of claim 11, wherein
the germanium (Ge)-based raw material includes Ge, an oxide of Ge, a nitride of Ge, a salt compound of Ge, or a mixture thereof, or
the germanium (Ge)-based raw material includes a compound in a form of a sol in which Ge is dispersed in an organic solvent.

### Claim 13 (depends on 11)

The method of claim 11, wherein
the internal electrode layer includes germanium (Ge) in an amount of 0.95 atomic % to 11.95 atomic % based on a total amount of nickel (Ni) and germanium (Ge) in the internal electrode layer.

### Claim 14

A method of manufacturing a multilayer ceramic capacitor, comprising
preparing a conductive paste including nickel (Ni);
preparing a dielectric slurry including a barium titanate-based compound including barium (Ba), titanium (Ti), and germanium (Ge);
manufacturing a dielectric green sheet from a dielectric slurry, and applying the conductive paste on a surface of the dielectric green sheet to form a conductive paste layer;
manufacturing a dielectric green sheet stack by stacking a plurality of the dielectric green sheet on which the conductive paste layer is formed;
manufacturing a capacitor body including a dielectric layer and an internal electrode layer by firing the dielectric green sheet stack; and
forming an external electrode on an outer surface of the capacitor body,
the internal electrode layer includes nickel (Ni), and
a space lattice edge length of nickel (Ni) obtained from Equation 1 through X-ray diffraction analysis (XRD) of the internal electrode layer is 3.522 Å to 3.544 Å:
α
=
λ
·
h
2
+
k
2
+
l
2
2
⁢
sin
⁢
θ
[
Equation
⁢
1
]
wherein, in Equation 1:
λ is 1.5406 Å, which is Cu Kα,
h, k, and l are plane indices, and
θ is a Bragg angle.

### Claim 15

A method of manufacturing a multilayer ceramic capacitor, comprising
firing a dielectric green sheet stack in a reducing atmosphere that includes hydrogen at a concentration of up to 1% to manufacture a capacitor body including a dielectric layer and an internal electrode layer; and
forming an external electrode on an outer surface of the capacitor body,
wherein the dielectric green sheet stack includes a plurality of dielectric green sheets and a plurality of conductive paste layers,
a conductive paste layer among the plurality of conductive paste layers is disposed on a dielectric green sheet among the plurality of dielectric green sheets,
the plurality of conductive paste layers includes nickel (Ni), and a germanium (Ge)-based raw material,
the internal electrode layer includes nickel (Ni), and
a space lattice edge length of nickel (Ni) obtained from Equation 1 through X-ray diffraction analysis (XRD) of the internal electrode layer is 3.522 Å to 3.544 Å:
α
=
λ
·
h
2
+
k
2
+
l
2
2
⁢
sin
⁢
θ
[
Equation
⁢
1
]
wherein, in Equation 1:
λ is 1.5406 Å, which is Cu Kα,
h, k, and l are plane indices, and
θ is a Bragg angle.

### Claim 16 (depends on 15)

The method of claim 15, wherein
the germanium (Ge)-based raw material includes GeO2.

### Claim 17 (depends on 16)

The method of claim 16, wherein
the internal electrode layer includes germanium (Ge) in an amount of 0.95 atomic % to 11.95 atomic % based on a total amount of nickel (Ni) and germanium (Ge) in the internal electrode layer.

### Claim 18 (depends on 16)

The method of claim 16, wherein
the firing of the dielectric green sheet stack is performed at a temperature of 1100° C. to 1400° C., and
the reducing atmosphere has an oxygen partial pressure of 1.0×10−14 MPa to 1.0×10−10 MPa.

### Claim 19 (depends on 16)

The method of claim 16, wherein
the reducing atmosphere further includes nitrogen and moisture.

### Claim 20 (depends on 16)

The method of claim 16, wherein
the dielectric layer includes a barium titanate-based compound.

### Claim 21 (depends on 20)

The method of claim 20, wherein
a difference between the space lattice edge length of nickel (Ni) in the internal electrode layer and a space lattice edge length of the barium titanate-based compound is 0.492 Å to 0.515 Å, and
the space lattice edge length of the barium titanate-based compound is obtained from Equation 1 through X-ray diffraction analysis (XRD) of the dielectric layer.