# US 2026/0071434 A1 · Epdm roofing membranes reinforced with short fiber aramids

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0071434 A1
- Document ID: US20260071434A1
- Status: Published application
- Kind: A1
- Application number: 19/311,470
- Filed: 2025-08-27
- Published: 2026-03-12
- Earliest claimed: 2024-09-09
- Assignees: Carlisle Construction Materials, LLC
- Applicants: Carlisle Construction Materials, LLC
- Inventors: Majid KARIMI NEJAD
- Web page: https://patentgrep.com/patent/US20260071434A1

## CPC

- E04D 12/002: {Sheets of flexible material, e.g. roofing tile underlay}
- C08K 5/3477: Six-membered rings
- C08K 5/34922: {Melamine; Derivatives thereof}
- C08K 5/548: containing sulfur {(C08K5/5477 takes precedence)}
- C08K 7/02: Fibres or whiskers
- C08L 9/00: Compositions of homopolymers or copolymers of conjugated diene hydrocarbons
- C08L 23/16: Ethylene-propylene or ethylene-propylene-diene copolymers
- C08L 77/10: Polyamides derived from aromatically bound amino and carboxyl groups of amino-carboxylic acids or of polyamines and polycarboxylic acids
- C08L 2207/04: Thermoplastic elastomer
- E04D: ROOF COVERINGS; SKY-LIGHTS; GUTTERS; ROOF-WORKING TOOLS (coverings of outer walls by plaster or other porous material E04F13/00)
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)

## Abstract

An EPDM roofing membrane with improved hail resistance formed from a block of EPDM material with short aramid fibers added to the block of EPDM material at a concentration of 5 to 35 PHR, a weak alkaline accelerator added to the block of EPDM material at a concentration of 2 to 8 PHR, a thermoplastic elastomer added to the block of EPDM material at a concentration of 2 to 10 PHR, polysulfide silane added to the block of EPDM material at a concentration of 2 to 10 PHR; and a hemiaminal ether crosslinking agent added to the block of EPDM material at a concentration of 2 to 10 PHR.

## Claims

### Claim 1

An EPDM roofing membrane, comprising:
a block of EPDM material;
short aramid fibers added to the block of EPDM material at a concentration of 5 to 35 PHR;
a weak alkaline accelerator added to the block of EPDM material at a concentration of 2 to 8 PHR;
a thermoplastic elastomer added to the block of EPDM material at a concentration of 2 to 10 PHR;
polysulfide silane added to the block of EPDM material at a concentration of 2 to 10 PHR; and
a hemiaminal ether crosslinking agent added to the block of EPDM material at a concentration of 2 to 10 PHR.

### Claim 2 (depends on 1)

The EPDM roofing membrane of claim 1, wherein the a weak alkaline accelerator is HEXA-80.

### Claim 3 (depends on 1)

The EPDM roofing membrane of claim 1, wherein the thermoplastic elastomer is MAH-G-EPDM.

### Claim 4 (depends on 1)

The EPDM roofing membrane of claim 1, wherein the hemiaminal ether crosslinking agent such is HMMM.