# US 2026/0071076 A1 · Cementitious cooling paint and cementitious cooling construction material

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0071076 A1
- Document ID: US20260071076A1
- Status: Published application
- Kind: A1
- Application number: 19/104,905
- Filed: 2023-09-21
- Published: 2026-03-12
- Earliest claimed: 2022-09-21
- Assignees: Nanyang Technological University
- Applicants: Nanyang Technological University
- Inventors: Hong LI; Jipeng FEI
- Web page: https://patentgrep.com/patent/US20260071076A1

## CPC

- C09D 1/06: cement
- C09D 1/08: with organic additives
- C09D 5/004: {Reflecting paints; Signal paints}
- C09D 7/61: inorganic
- C09D 7/63: organic
- C09D 7/65: macromolecular (C09D7/41-C09D7/48 take precedence)
- C09D 7/68: {Particle size between 100-1000 nm}
- C09D 7/69: {Particle size larger than 1000 nm}
- C08K 3/013: Fillers, pigments or reinforcing additives
- C08K 3/16: Halogen-containing compounds
- C09D: COATING COMPOSITIONS, e.g. PAINTS, VARNISHES OR LACQUERS; FILLING PASTES; CHEMICAL PAINT OR INK REMOVERS; INKS; CORRECTING FLUIDS; WOODSTAINS; PASTES OR SOLIDS FOR COLOURING OR PRINTING; USE OF MATERIALS THEREFOR (cosmetics A61K; processes for applying liquids or other fluent materials to surfaces, in general, B05D; staining wood B27K5/02; glazes or vitreous enamels C03C; natural resins, French polish, drying-oils, driers, turpentine, per se, C09F; polishing compositions other than French polish, ski waxes C09G; adhesives or use of materials as adhesives C09J; materials for sealing or packing joints or covers C09K3/10; materials for stopping leaks C09K3/12; processes for the electrolytic or electrophoretic production of coatings C25D)
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)

## Abstract

A cementitious cooling paint is provided. The cementitious cooling paint comprises a composite cement; a structural filler; a water-absorbing polymer; a water capture material; and water wherein the water to composite cement ratio is from 0.4 to 1.2 by mass; the composite cement to structural filler ratio is from 0.4 to 0.7 by mass; the composite cement to water-absorbing polymer ratio is from 0.01 to 0.03 by mass; and the composite cement to water capture material ratio is from 0.05 to 0.3. The cementitious cooling paint may further include a dispersant, wherein the composite cement to dispersant ratio is from 20 to 50 by mass. A cementitious cooling construction material and a cement-based building product comprising the cementitious cooling construction material are also provided.

## Claims

### Claim 1

A cementitious cooling paint comprising:
a composite cement;
a structural filler;
a water-absorbing polymer;
a water capture material; and
water;
wherein
the water to composite cement ratio is from 0.4 to 1.2 by mass;
the composite cement to structural filler ratio is from 0.4 to 0.7 by mass;
the composite cement to water-absorbing polymer ratio is from 0.01 to 0.03 by mass; and
the composite cement to water capture material ratio is from 0.05 to 0.3 by mass; and
wherein the cementitious cooling paint exhibits dual passive cooling mechanisms including radiative cooling and evaporative cooling.

### Claim 2 (depends on 1)

The cementitious cooling paint according to claim 1, further comprising: a dispersant, wherein the composite cement to dispersant ratio is from 20 to 50 by mass.

### Claim 3 (depends on 1)

The cementitious cooling paint according to claim 1, wherein the composite cement is at least one selected from the group consisting of various types and grades of Portland cement and geopolymer cement.

### Claim 4 (depends on 1)

The cementitious cooling paint according to claim 1, wherein the structural filler is at least one selected from the group consisting of silicon dioxide (SiO2), barium sulfate (BaSO4), calcium carbonate (CaCO3), zinc oxide (ZnO), aluminum oxide (Al2O3), zirconium dioxide (ZrO2), titanium dioxide (TiO2), iron(III) oxide (Fe2O3), hydrated goethite (α-FeOOH) and Prussian Blue.

### Claim 5 (depends on 1, 4)

The cementitious cooling paint according to claim 1 or 4, wherein the structural filler comprises nanoparticles having an average particle size ranging from 0.3 μm to 2 μm.

### Claim 6 (depends on 1)

The cementitious cooling paint according to claim 1, wherein the water-absorbing polymer is at least one selected from the group consisting of sodium poly(acrylate), sodium carboxymethyl cellulose and sodium alginate, polyvinyl alcohol, hydroxypropyl methylcellulose and carboxymethyl cellulose.

### Claim 7 (depends on 1)

The cementitious cooling paint according to claim 1, wherein the water capture material is at least one selected from the group consisting of deliquescent salt such as lithium chloride (LiCI) and calcium chloride (CaCl2).

### Claim 8 (depends on 2)

The cementitious cooling paint according to claim 2, wherein the dispersant is at least one selected from the group consisting of sodium polyacrylic and superplasticizer such as sulfonated naphthalene formaldehyde condensate, sulfonated melamine formaldehyde condensate, acetone formaldehyde condensate and polycarboxylates ethers.

### Claim 9

A cementitious cooling construction material comprising:
a composite cement;
a structural filler;
a water-absorbing polymer;
a water capture material;
a dispersant; and
water; wherein
the water to the composite cement ratio is from 0.5 to 1.5 by mass.
the composite cement to structural filler ratio is from 0.4 to 0.7 by mass;
the composite cement to water-absorbing polymer ratio is from 0.01 to 0.03 by mass;
the composite cement to water capture material ratio is from 0.05 to 0.3 by mass; and
the composite cement to dispersant ratio is from 8 to 15; and
wherein the cementitious cooling construction material exhibits dual passive cooling mechanisms including radiative cooling and evaporative cooling.

### Claim 10 (depends on 9)

The cementitious cooling construction material according to claim 9, further comprising alkaline water for hydrating the cementitious cooling construction material and for preventing the cementitious cooling construction material from cracking.

### Claim 11 (depends on 9)

The cementitious cooling construction material according to claim 9, wherein the composite cement is at least one selected from the group consisting of various types and grades of Portland cement and geopolymer cement.

### Claim 12 (depends on 9)

The cementitious cooling construction material according to claim 9, wherein the structural filler is at least one selected from the group consisting of silicon dioxide (SiO2), barium sulfate (BaSO4), calcium carbonate (CaCO3), zinc oxide (ZnO), aluminum oxide (Al2O3), zirconium dioxide (ZrO2), titanium dioxide (TiO2), iron(III) oxide (Fe2O3), hydrated goethite (α-FeOOH) and Prussian Blue.

### Claim 13 (depends on 9, 12)

The cementitious cooling construction material according to claim 9 or 12, wherein the structural filler comprises nanoparticles having an average particle size ranging from 0.3 μm to 2 μm.

### Claim 14 (depends on 9)

The cementitious cooling construction material according to claim 9, wherein the water-absorbing polymer is at least one selected from the group consisting of sodium poly(acrylate), sodium carboxymethyl cellulose and sodium alginate, polyvinyl alcohol, hydroxypropyl methylcellulose and carboxymethyl cellulose.

### Claim 15 (depends on 9)

The cementitious cooling construction material according to claim 9, wherein the water capture material is at least one selected from the group consisting of deliquescent salt such as lithium chloride (LiCI) and calcium chloride (CaCl2).

### Claim 16 (depends on 9)

The cementitious cooling construction material according to claim 9, wherein the dispersant is at least one selected from the group consisting of sodium polyacrylic and superplasticizer such as sulfonated naphthalene formaldehyde condensate, sulfonated melamine formaldehyde condensate, acetone formaldehyde condensate and polycarboxylates ethers.

### Claim 17 (depends on 10)

The cementitious cooling construction material according to claim 10, wherein the cementitious cooling construction material has a viscosity suitable for fabricating cement-based building product selected from cooling tile, cooling brick, cooling concrete, cooling concrete block, cooling concrete slab and cooling cement wall.

### Claim 18 (depends on 9)

A cement-based building product comprising a cementitious cooling construction material as defined in claim 9, wherein the cement-based building product is one selected from cooling tile, cooling brick, cooling concrete, cooling concrete block, cooling concrete slab and cooling cement wall.

### Claim at position 19

19-28. (canceled)