# US 2026/0071032 A1 · Method of producing powdered polyamide

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0071032 A1
- Document ID: US20260071032A1
- Status: Published application
- Kind: A1
- Application number: 19/110,970
- Filed: 2023-09-21
- Published: 2026-03-12
- Earliest claimed: 2022-09-28
- Assignees: Asahi Kasei Kabushiki Kaisha
- Applicants: Asahi Kasei Kabushiki Kaisha
- Inventors: Kenichi YAKIGAYA; Ryo MIYATAKE; Yutaro YAMADA; Noko HONDA; Shoji OTANI; Naoyuki KUSUYAMA
- Web page: https://patentgrep.com/patent/US20260071032A1

## CPC

- C08J 3/14: by precipitation from solutions {(C08J3/122 takes precedence)}
- B29B 17/00: Recovery of plastics or other constituents of waste material containing plastics; ({volume reduction of waste plastics, e.g. by mechanical compacting or melting disposal of solid waste B09B;} chemical recovery C08J11/00)
- B29B 17/02: Separating plastics from other materials
- C08G 69/46: Post-polymerisation treatment
- C08J 3/11: from solid polymers
- C08J 3/126: {Polymer particles coated by polymer, e.g. core shell structures}
- C08J 11/08: using selective solvents for polymer components
- C08K 3/16: Halogen-containing compounds
- C08K 3/20: Oxides; Hydroxides {(graphene oxides C08K3/042)}
- C08L 77/00: Compositions of polyamides obtained by reactions forming a carboxylic amide link in the main chain (of polyhydrazides C08L79/06; of polyamideimides or polyamide acids C08L79/08); Compositions of derivatives of such polymers
- C08L 77/06: Polyamides derived from polyamines and polycarboxylic acids (C08L77/10 takes precedence)
- C08J 2377/06: Polyamides derived from polyamines and polycarboxylic acids (C08J2377/10 takes precedence)
- C08J 2431/08: of phthalic acid
- Y02W 30/62: Plastics recycling; Rubber recycling
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)
- B29B: PREPARATION OR PRETREATMENT OF THE MATERIAL TO BE SHAPED; MAKING GRANULES OR PREFORMS; RECOVERY OF PLASTICS OR OTHER CONSTITUENTS OF WASTE MATERIAL CONTAINING PLASTICS
- C08G: MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- Y02W: CLIMATE CHANGE MITIGATION TECHNOLOGIES RELATED TO WASTEWATER TREATMENT OR WASTE MANAGEMENT

## Abstract

A method of producing powdered polyamide includes: a step 1 of heating and dissolving a polyamide resin composition in a metal chloride alcohol solution containing a metal chloride and an alcohol to obtain a polyamide thermal dissolution liquid; a step 2 of diluting the polyamide thermal dissolution liquid with an alcohol to obtain an alcohol dilution; and a step 3 of cooling the alcohol dilution to cause precipitation of powdered polyamide. The mass proportion of metal chloride relative to 100 mass % of the metal chloride alcohol solution in step 1 is 23 mass % to 35 mass %, the polyamide thermal dissolution liquid contains 0.2 mol to 2.5 mol of water relative to 1 mol of metal chloride in step 1, and the polyamide thermal dissolution liquid is diluted without dropping below a temperature of 50° C. in step 2.

## Claims

### Claim 1

A method of producing powdered polyamide comprising:
step 1: a step of heating and dissolving a polyamide resin composition in a metal chloride alcohol solution containing a metal chloride and an alcohol to obtain a polyamide thermal dissolution liquid;
step 2: a step of diluting the polyamide thermal dissolution liquid with an alcohol to obtain an alcohol dilution; and
step 3: a step of cooling the alcohol dilution to cause precipitation of powdered polyamide, wherein
a mass proportion of metal chloride relative to 100 mass % of the metal chloride alcohol solution in the step 1 is not less than 23 mass % and not more than 35 mass %, the polyamide thermal dissolution liquid contains not less than 0.2 mol and not more than 2.5 mol of water relative to 1 mol of metal chloride in the step 1, and the polyamide thermal dissolution liquid is diluted without dropping below a temperature of 50° C. in the step 2.

### Claim 2

A method of producing powdered polyamide comprising:
step 1: a step of heating and dissolving a polyamide resin composition in a metal chloride alcohol solution containing a metal chloride and an alcohol to obtain a polyamide thermal dissolution liquid;
step 2: a step of diluting the polyamide thermal dissolution liquid with an alcohol to obtain an alcohol dilution; and
step 3: a step of cooling the alcohol dilution to cause precipitation of powdered polyamide, wherein
a mass proportion of metal chloride relative to 100 mass % of the metal chloride alcohol solution in the step 1 is not less than 23 mass % and not more than 35 mass %, the polyamide thermal dissolution liquid contains not less than 0.2 mol and not more than 2.5 mol of water relative to 1 mol of metal chloride in the step 1, and mass of polyamide that precipitates in the step 2 is 1 mass % or less relative to total mass of polyamide contained in the polyamide thermal dissolution liquid.

### Claim at position 3

3-6. (canceled)

### Claim 7 (depends on 1)

The method of producing powdered polyamide according to claim 1, further comprising
step 4: a step of washing the powdered polyamide obtained in the step 3 at least once using a solvent.

### Claim 8 (depends on 7)

The method of producing powdered polyamide according to claim 7, wherein a solvent used in a first washing in the step 4 is the same alcohol as the alcohol that is used in the step 1.

### Claim 9 (depends on 1)

The method of producing powdered polyamide according to claim 1, wherein a temperature of the heating and dissolving of the step 1 is not lower than 60° C. and not higher than 80° C.

### Claim 10 (depends on 1)

The method of producing powdered polyamide according to claim 1, further comprising
step 5: a step of heating the powdered polyamide that has precipitated in the step 3 to obtain a heated powdered polyamide.

### Claim 11 (depends on 10)

The method of producing powdered polyamide according to claim 10, further comprising, after the step 5,
step 6: a step of performing solid-liquid separation of the heated powdered polyamide obtained in the step 5 and washing a solid obtained thereby.

### Claim 12 (depends on 1)

The method of producing powdered polyamide according to claim 1, wherein the polyamide resin composition is a polyamide resin composition that contains polyamide coated with a silicone resin, and a concentration of polyamide in the polyamide thermal dissolution liquid in the step 1 is 5 mass % to 15 mass %.

### Claim 13 (depends on 1)

The method of producing powdered polyamide according to claim 1, wherein the polyamide resin composition is a polyamide resin composition that contains polyamide coated with a silicone resin, and viscosity at 25° C. of the polyamide thermal dissolution liquid in the step 1 is 10 mPa·s to 20,000 mPa·s.

### Claim 14

(canceled)

### Claim 15 (depends on 1)

The method of producing powdered polyamide according to claim 1, wherein the metal chloride alcohol solution is a metal chloride alcohol solution that contains a metal chloride in a concentration of not less than 23 mass % and not more than 35 mass %, a hydroxide of the same metal as a metal included in the metal chloride in a concentration of 0.001 mass % to 1 mass %, and water in a concentration of 0.001 mass % to 10 mass %.

### Claim 16 (depends on 1)

The method of producing powdered polyamide according to claim 1, wherein the method is a method of producing powdered polyamide containing 0.001 ppm to 1,500 ppm of calcium atoms and having a halogen atom molar content of less than 1 relative to calcium atom molar content.

### Claim 17 (depends on 1)

The method of producing powdered polyamide according to claim 1, wherein the polyamide resin composition contains at least polyamide and polyethylene terephthalate.

### Claim 18 (depends on 1)

The method of producing powdered polyamide according to claim 1, wherein the polyamide resin composition contains polyamide coated with a urethane resin.

### Claim 19 (depends on 1)

The method of producing powdered polyamide according to claim 1, comprising, after the steps 1 to 3:
step 7: a step of recovering powdered polyamide that has precipitated;
step 8: a washing step of washing the powdered polyamide that has been recovered; and
step 9: a drying step of thermally drying the powdered polyamide that is present after the washing, wherein
an amount of metal chloride that is attached to the powdered polyamide present after the thermal drying of the step 9 is 20 parts by mass or less relative to 100 parts by mass of the powdered polyamide.