# US 2026/0070845 A1 · Low-density high-strength concrete and related methods using foamed glass aggregates

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0070845 A1
- Document ID: US20260070845A1
- Status: Published application
- Kind: A1
- Application number: 19/320,079
- Filed: 2025-09-05
- Published: 2026-03-12
- Earliest claimed: 2024-09-06
- Assignees: Aero Aggregates of North America LLC
- Applicants: Aero Aggregates of North America, LLC
- Inventors: Archibald Filshill; Theresa A. Loux
- Web page: https://patentgrep.com/patent/US20260070845A1

## CPC

- C04B 28/04: Portland cements
- C04B 14/24: porous, e.g. foamed glass
- C04B 18/146: {Silica fume}
- C04B 2103/44: Thickening, gelling or viscosity increasing agents
- C04B 2103/58: {Shrinkage reducing agents}
- C04B 2111/00103: {Self-compacting mixtures}
- C04B 2111/00612: {as one or more layers of a layered structure}
- C04B 2111/28: Fire resistance, i.e. materials resistant to accidental fires or high temperatures
- C04B 2111/40: Porous or lightweight materials
- C04B 2201/20: for the density
- C04B 2201/50: for the mechanical strength
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE

## Abstract

The invention provides a low-density, high-strength concrete composition, which is self-compacting and lightweight, with a low weight-fraction of aggregate to total dry raw materials, and a highly homogenous distribution of an absorptive lightweight aggregate such as glass microspheres and, optionally, polymer beads, as well as the methods for providing the composition or components. Lightweight concrete formed by the disclosed concrete composition have low density, high strength-to-weight ratios, and high R-value. The concrete has strength like that ordinarily found in structural lightweight concrete. The concrete, at the density ordinarily found in structural lightweight concrete, has a higher strength and, at the strength ordinarily found in structural lightweight concrete, a lower density.

## Claims

### Claim 1

A lightweight concrete composition comprising:
one or more cementitious materials;
an aggregate mix composed of individual particles that are substantially volumetrically stable and non-absorbent, the aggregate mix comprising hollow glass microspheres;
a foaming agent; and, optionally,
an air detrainer;
a shrinkage reducer;
a viscosity modifier; and
combinations thereof
wherein the lightweight concrete composition has a weight of about 60 pounds per cubic foot and compressive strength after 28 days as measured by ASTM C39 of at least about 1750 psi.

### Claim 2 (depends on 1)

The lightweight concrete composition of claim 1, wherein the foaming agent comprises an air entrainment admixture.

### Claim 3 (depends on 1)

The lightweight concrete composition of claim 1, further comprising reinforcing fibers selected from the group consisting of glass fibers, carbon fibers, aramid fibers, steel fibers, and combinations thereof.
The lightweight concrete composition of claim 1, wherein the cementitious materials comprise Portland cement and silica fume.

### Claim 5 (depends on 1)

The lightweight concrete composition of claim 1, wherein the shrinkage reducer comprises a glycol-based compound.

### Claim 6 (depends on 1)

The lightweight concrete composition of claim 1, wherein the viscosity modifier is present in an amount of 2-16 ounces per 100 pounds of cementitious material.

### Claim 7 (depends on 1)

The lightweight concrete composition of claim 1, wherein the hollow glass microspheres are closed-cell microspheres having a particle size less than 150 micrometers.

### Claim 8

A method of preparing a lightweight concrete mix, comprising:
providing one or more cementitious materials;
providing an aggregate mix comprising hollow glass microspheres that are substantially volumetrically stable and non-absorbent;
combining the cementitious materials, the aggregate mix, and a foaming agent with water to form a concrete slurry; and
mixing the slurry under conditions sufficient to produce a substantially homogeneous distribution of the hollow glass microspheres,
wherein the resulting lightweight concrete has a density of about 60 to 120 pounds per cubic foot and a compressive strength after 28 days as measured by ASTM C39 of at least about 1750 psi.

### Claim 9 (depends on 8)

The method of claim 8, further comprising adding a viscosity modifier to increase suspension stability of the hollow glass microspheres.

### Claim 10 (depends on 8)

The method of claim 8, wherein the slurry is mixed in a drum-type mixer, a pan-type mixer, or a ribbon mixer.

### Claim 11 (depends on 8)

The method of claim 8, wherein the hollow glass microspheres replace at least 20% by volume of standard density aggregate.

### Claim 12 (depends on 8)

The method of claim 8, further comprising incorporating reinforcing fibers into the slurry prior to curing.

### Claim 13 (depends on 8)

The method of claim 8, wherein the water-to-cement ratio is maintained between about 0.22 and 0.40.

### Claim 14 (depends on 8)

The method of claim 8, further comprising curing the lightweight concrete under controlled moisture conditions to reduce autogenous shrinkage.

### Claim 15

A precast concrete product comprising:
a hardened lightweight concrete body formed from a mix including cementitious materials, hollow glass microspheres, and a foaming agent;
wherein the lightweight concrete body has a density of less than about 100 pounds per cubic foot, an R-value greater than that of normal weight concrete of equivalent thickness, and a compressive strength after 28 days as measured by ASTM C39 of at least about 2500 psi.

### Claim 16 (depends on 15)

The precast concrete product of claim 15, wherein the product is a structural beam, concrete block, or architectural panel.

### Claim 17 (depends on 15)

The precast concrete product of claim 15, further comprising a reinforcing mesh embedded within the hardened lightweight concrete body.

### Claim 18 (depends on 15)

The precast concrete product of claim 15, wherein the hollow glass microspheres are present in an amount of 10-50% by volume of the aggregate fraction.

### Claim 19 (depends on 15)

The precast concrete product of claim 15, wherein the product exhibits a modulus of rupture of at least about 400 psi.

### Claim 20 (depends on 15)

The precast concrete product of claim 15, wherein the hardened lightweight concrete body has a thermal conductivity at least 20% lower than that of conventional normal weight concrete.