# US 2026/0070788 A1 · A method for producing ferrous sulphate and phosphoric acid

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0070788 A1
- Document ID: US20260070788A1
- Status: Published application
- Kind: A1
- Application number: 18/846,676
- Filed: 2023-03-22
- Published: 2026-03-12
- Earliest claimed: 2022-03-29
- Assignees: Kemira Oyj
- Applicants: Kemira Oyj
- Inventors: Bengt HANSEN; Roger BÅRSTRÖM
- Web page: https://patentgrep.com/patent/US20260070788A1

## CPC

- C01B 25/222: with sulfuric acid, a mixture of acids mainly consisting of sulfuric acid or a mixture of compounds forming it in situ, e.g. a mixture of sulfur dioxide, water and oxygen
- C01G 49/14: Sulfates {(C01G49/0018 takes precedence)}
- C05B 13/04: from metallic phosphorus compounds, e.g. ferro-phosphorus
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- C01G: COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSES C01D OR C01F (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts or peroxyacids C01B15/00; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium, or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds containing nitrogen, other non-metals and metal C01B21/082}; metal amides C01B21/092; nitrites C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; compounds having molecular sieve properties but not having base-exchange properties C01B37/00; compounds having molecular sieve and base-exchange properties, e.g. crystalline zeolites, C01B39/00; cyanides C01C3/08; salts of cyanamide C01C3/16; thiocyanates C01C3/20)
- C05B: PHOSPHATIC FERTILISERS

## Abstract

There is provided a method for producing ferrous sulphate and phosphoric acid comprising treating ferrous phosphate with sulphuric acid for obtaining ferrous sulphate and phosphoric acid. Additionally, there is provided a use of sulphuric acid for treating ferrous phosphate for obtaining ferrous sulphate and phosphoric acid.

## Claims

### Claim 1

A method for producing ferrous sulphate and phosphoric acid comprising
treating ferrous phosphate with sulphuric acid for producing a mixture comprising ferrous sulphate and phosphoric acid;
cooling the mixture for precipitating ferrous sulphate; and
recovering ferrous sulphate, phosphoric acid, or ferrous sulphate and phosphoric acid from the cooled mixture.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the ferrous phosphate originates from manure, phosphate rich industrial side streams, phosphate rich industrial waste streams, wastewater treatment process, preferably from sludge, such as sewage sludge from wastewater treatment process.

### Claim 3 (depends on 1)

The method according to claim 1, wherein impurities are removed from the mixture before cooling the mixture, preferably by filtration.

### Claim 4 (depends on 1)

The method according to claim 1, wherein the mixture is cooled to a temperature range from 0° C. to 50° C., preferably from 0° C. to 30° C., more preferably from 1° C. to 15° C., even more preferably from 1° C. to 10° C., further even more preferably from 1° C. to 5° C.

### Claim 5 (depends on 1)

The method according to claim 1, wherein the precipitated ferrous sulphate is recovered from the mixture, preferably by filtration, sedimentation or centrifugation.

### Claim 6 (depends on 1)

The method according to claim 1, wherein the recovered precipitated ferrous sulphate is washed, preferably with sulphuric acid.

### Claim 7 (depends on 1)

The method according to claim 1, wherein ferrous phosphate is treated with excess amount of sulphuric acid.

### Claim 8 (depends on 1)

The method according to claim 1, wherein ratio of mol amount of sulphuric acid to mol amount of iron in the ferrous phosphate is from 0.5 to 10, preferably from 1 to 10, more preferably from 1 to 8, even more preferably from 1 to 5, more even preferably from 1 to 4.

### Claim 9 (depends on 1)

The method according to claim 1, wherein mixing is applied in the treatment.

### Claim 10 (depends on 1)

The method according to claim 1, wherein before the treatment the ferrous phosphate has at least 5% solid content, preferably from 10% to 90%, more preferably 20% to 80%.

### Claim 11 (depends on 5)

The method according to claim 5, wherein a filtrate comprising phosphoric acid from the filtration and/or a supernatant comprising phosphoric acid from the centrifugation is recovered.

### Claim 12 (depends on 1311)

The method according to claim 1311, wherein phosphoric acid is separated from the filtrate and/or from the supernatant, preferably in an acid regeneration process.

### Claim 13

A method of producing ferrous sulphate and phosphoric acid by using sulphuric acid for treating ferrous phosphate, wherein a ratio of mol amount of used sulphuric acid to mol amount of iron in the ferrous phosphate is 0.5 to 10, preferably from 1 to 10, more preferably from 1 to 8, even more preferably from 1 to 5, more even preferably from 1 to 4.

### Claim 14 (depends on 1)

Ferrous sulphate and/or phosphoric acid produced with the method according to claim 1.

### Claim 15 (depends on 1)

Use of ferrous sulphate produced with the method according to claim 1 in a coagulant process or phosphoric acid solution produced with the method of according to claim 1 as a fertilizer or for production of pure phosphoric acid and other phosphate salts.

### Claim 16 (depends on 1)

The method of claim 1, wherein the concentration of the sulphuric acid is in the range of 40%-98.3%.