# US 2026/0066403 A1 · Self-assembled cast polypropylene (cpp) base film of aluminum-plastic film for new energy pouch batteries and preparation method thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0066403 A1
- Document ID: US20260066403A1
- Status: Published application
- Kind: A1
- Application number: 19/249,705
- Filed: 2025-06-25
- Published: 2026-03-05
- Earliest claimed: 2024-09-04
- Assignees: Guizhou Institute of Metallurgy and Chemical Engineering; Guizhou Nanomaterials Engineering Center; Guizhou tianrunda technology co., ltd
- Applicants: Guizhou Institute of Metallurgy and Chemical Engineering; Guizhou Nanomaterials Engineering Center; Guizhou tianrunda technology co., ltd
- Inventors: Shu Zeng; Xiaoxiao HUANG; Kang Yang; Yi Zhang; Yulong MA; Juheng WANG; Anlan ZHONG
- Web page: https://patentgrep.com/patent/US20260066403A1

## CPC

- H01M 50/124: having a layered structure
- B29C 71/04: by wave energy or particle radiation {, e.g. for curing or vulcanising preformed articles (during moulding, e.g. in a mould B29C35/08)}
- H01M 50/105: Pouches or flexible bags
- H01M 50/119: Metals
- H01M 50/121: Organic material
- B29C 48/154: Coating solid articles, i.e. non-hollow articles
- B29C 48/21: the layers being joined at their surfaces
- B29K 2023/12: {PP, i.e. polypropylene}
- B29K 2705/02: Aluminium
- B29L 2031/3468: {Batteries, accumulators or fuel cells (battery cases B29L2031/7146)}
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- B29C: SHAPING OR JOINING OF PLASTICS; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDED FOR; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING (making preforms B29B11/00; making laminated products by combining previously unconnected layers which become one product whose layers will remain together B32B37/00 - B32B41/00)
- B29K: INDEXING SCHEME ASSOCIATED WITH SUBCLASSES B29B, B29C OR B29D, RELATING TO MOULDING MATERIALS OR TO MATERIALS FOR {MOULDS, } REINFORCEMENTS, FILLERS OR PREFORMED PARTS, e.g. INSERTS
- B29L: INDEXING SCHEME ASSOCIATED WITH SUBCLASS B29C, RELATING TO PARTICULAR ARTICLES
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

Disclosed is a self-assembled cast polypropylene (CPP) base film of an aluminum-plastic film for new energy pouch batteries and a preparation method thereof. The base film comprises a self-assembled heat sealing layer, a support layer and a composite layer. The preparation process includes charging the raw materials of three layers into a three-layer co-extrusion casting machine and setting the relevant parameters for preparation, then performing a corona treatment. The present disclosure utilizes an organic hybrid micro-nano thermal conductive material to induce the heat sealing layer to produce a self-assembly function in a high temperature environment after heat sealing, thereby effectively preventing the pouch batteries from short circuit or explosion in a high temperature environment.

## Claims

### Claim 1

A self-assembled cast polypropylene (CPP) base film of an aluminum-plastic film for new energy pouch batteries, comprising a self-assembled heat sealing layer, a support layer and a composite layer arranged in sequence; wherein a thickness of the CPP base film is 20 μm to 90 μm, and a thickness ratio of the self-assembled heat sealing layer, the support layer and the composite layer is (1-3): (4-8): (1-3);
wherein the self-assembled heat sealing layer comprises, by weight percentage, 69% to 96% of ternary random copolymer polypropylene, 0% to 20% of binary random copolymer polypropylene, 3% to 6% of opening slipping agent and 1% to 5% of organic hybrid micro-nano thermal conductive material;
wherein the organic hybrid micro-nano thermal conductive material is prepared by a sol-gel method using one or more of silicon dioxide, calcium carbonate, calcium silicate, and barium sulfate and an organic surface modifier, and a method for preparing the organic hybrid micro-nano thermal conductive material comprises:
mixing the organic surface modifier with an inorganic nanomaterial at a mass ratio of 1:99 to 5:95, and then preparing by a sol-gel method, wherein a temperature is controlled at −10° C. to 120° C., a pressure is 1.0 MPa to 3.0 MPa, and a reaction time is 1 h to 10 h; and the organic surface modifier is one or more of silane coupling agent, titanate coupling agent, aluminate coupling agent, and borate coupling agent;
wherein the support layer comprises, by weight percentage, 50% to 90% of block copolymer polypropylene, 0% to 10% of binary random copolymer polypropylene, 0% to 10% of ternary random copolymer polypropylene, 5% to 10% of polyolefin elastomer, and 5% to 20% of acidified polypropylene;
wherein the composite layer comprises, by weight percentage, 50% to 89% of binary random copolymer polypropylene, 5% to 15% of block copolymer polypropylene, 5% to 30% of acidified polypropylene, and 1% to 5% of vinyl acetate; and
wherein the acidified polypropylene is maleic anhydride grafted modified polypropylene, with a grafting rate of ≥2%, and a melt index of 3-12 g/10 min.

### Claim 2 (depends on 1)

The self-assembled CPP base film of an aluminum-plastic film for new energy pouch batteries according to claim 1, wherein the opening slipping agent is one or more of organic silicones, siloxane polymers, and high molecular weight silicone waxes.

### Claim 3 (depends on 1)

The self-assembled CPP base film of an aluminum-plastic film for new energy pouch batteries according to claim 1, wherein the polyolefin elastomer is one or more of a polypropylene elastomer, a polyethylene elastomer, an ethylene-propylene rubber, and an ultra-low density polyethylene; and the selected block polypropylene has a melting point of ≥163° C. and a melt index of 2-10 g/10 min.

### Claim 4 (depends on 1)

The self-assembled CPP base film of an aluminum-plastic film for new energy pouch batteries according to claim 1, wherein the melting point of the ternary random copolymer polypropylene is 125° C. to 135° C. and the melt index is 3 to 12 g/10 min.

### Claim 5 (depends on 1)

The self-assembled CPP base film of an aluminum-plastic film for new energy pouch batteries according to claim 1, wherein the binary random copolymer polypropylene has a melting point of ≥140° C. and a melt index of 3-12 g/10 min.

### Claim 6 (depends on 1)

The self-assembled CPP base film of an aluminum-plastic film for new energy pouch batteries according to claim 1, wherein the acetic acid content of the vinyl acetate is 20 wt % to 30 wt %, and the melt index is 10-30 g/10 min.

### Claim 7 (depends on 1)

The method for preparing a self-assembled CPP base film of an aluminum-plastic film for new energy pouch batteries according to claim 1, comprising the following steps:
(1) weighing the raw materials of the self-assembled heat sealing layer, the support layer and the composite layer by weight percentage;
(2) correspondingly charging the raw materials of the self-assembled heat sealing layer, the support layer and the composite layer separately into the extruders A, B and C corresponding to the three-layer co-extrusion casting machine, starting the machine after debugging the equipment according to the thickness ratio of the layers and the processing temperature of the extruder, preparing the thin film by the co-extrusion casting process, and then carrying out a corona treatment with a corona machine at an output power of 2-70 KW and an output frequency of 10-25 kHz to obtain the self-assembled CPP base film of an aluminum-plastic film for new energy pouch batteries.

### Claim 8 (depends on 2)

The method for preparing a self-assembled CPP base film of an aluminum-plastic film for new energy pouch batteries according to claim 2, comprising the following steps:
(1) weighing the raw materials of the self-assembled heat sealing layer, the support layer and the composite layer by weight percentage;
(2) correspondingly charging the raw materials of the self-assembled heat sealing layer, the support layer and the composite layer separately into the extruders A, B and C corresponding to the three-layer co-extrusion casting machine, starting the machine after debugging the equipment according to the thickness ratio of the layers and the processing temperature of the extruder, preparing the thin film by the co-extrusion casting process, and then carrying out a corona treatment with a corona machine at an output power of 2-70 KW and an output frequency of 10-25 kHz to obtain the self-assembled CPP base film of an aluminum-plastic film for new energy pouch batteries.

### Claim 9 (depends on 3)

The method for preparing a self-assembled CPP base film of an aluminum-plastic film for new energy pouch batteries according to claim 3, comprising the following steps:
(1) weighing the raw materials of the self-assembled heat sealing layer, the support layer and the composite layer by weight percentage;
(2) correspondingly charging the raw materials of the self-assembled heat sealing layer, the support layer and the composite layer separately into the extruders A, B and C corresponding to the three-layer co-extrusion casting machine, starting the machine after debugging the equipment according to the thickness ratio of the layers and the processing temperature of the extruder, preparing the thin film by the co-extrusion casting process, and then carrying out a corona treatment with a corona machine at an output power of 2-70 KW and an output frequency of 10-25 kHz to obtain the self-assembled CPP base film of an aluminum-plastic film for new energy pouch batteries.

### Claim 10 (depends on 4)

The method for preparing a self-assembled CPP base film of an aluminum-plastic film for new energy pouch batteries according to claim 4, comprising the following steps:
(1) weighing the raw materials of the self-assembled heat sealing layer, the support layer and the composite layer by weight percentage;
(2) correspondingly charging the raw materials of the self-assembled heat sealing layer, the support layer and the composite layer separately into the extruders A, B and C corresponding to the three-layer co-extrusion casting machine, starting the machine after debugging the equipment according to the thickness ratio of the layers and the processing temperature of the extruder, preparing the thin film by the co-extrusion casting process, and then carrying out a corona treatment with a corona machine at an output power of 2-70 KW and an output frequency of 10-25 kHz to obtain the self-assembled CPP base film of an aluminum-plastic film for new energy pouch batteries.

### Claim 11 (depends on 5)

The method for preparing a self-assembled CPP base film of an aluminum-plastic film for new energy pouch batteries according to claim 5, comprising the following steps:
(1) weighing the raw materials of the self-assembled heat sealing layer, the support layer and the composite layer by weight percentage;
(2) correspondingly charging the raw materials of the self-assembled heat sealing layer, the support layer and the composite layer separately into the extruders A, B and C corresponding to the three-layer co-extrusion casting machine, starting the machine after debugging the equipment according to the thickness ratio of the layers and the processing temperature of the extruder, preparing the thin film by the co-extrusion casting process, and then carrying out a corona treatment with a corona machine at an output power of 2-70 KW and an output frequency of 10-25 kHz to obtain the self-assembled CPP base film of an aluminum-plastic film for new energy pouch batteries.

### Claim 12 (depends on 6)

The method for preparing a self-assembled CPP base film of an aluminum-plastic film for new energy pouch batteries according to claim 6, comprising the following steps:
(1) weighing the raw materials of the self-assembled heat sealing layer, the support layer and the composite layer by weight percentage;
(2) correspondingly charging the raw materials of the self-assembled heat sealing layer, the support layer and the composite layer separately into the extruders A, B and C corresponding to the three-layer co-extrusion casting machine, starting the machine after debugging the equipment according to the thickness ratio of the layers and the processing temperature of the extruder, preparing the thin film by the co-extrusion casting process, and then carrying out a corona treatment with a corona machine at an output power of 2-70 KW and an output frequency of 10-25 kHz to obtain the self-assembled CPP base film of an aluminum-plastic film for new energy pouch batteries.

### Claim 13 (depends on 7)

The method for preparing a self-assembled CPP base film of an aluminum-plastic film for new energy pouch batteries according to claim 7, wherein in the step (2), an extrusion temperature of extruders A and C is 230° C., and the extrusion temperature of extruder B is 255° C.

### Claim 14 (depends on 8)

The method for preparing a self-assembled CPP base film of an aluminum-plastic film for new energy pouch batteries according to claim 8, wherein in the step (2), an extrusion temperature of extruders A and C is 230° C., and the extrusion temperature of extruder B is 255° C.

### Claim 15 (depends on 9)

The method for preparing a self-assembled CPP base film of an aluminum-plastic film for new energy pouch batteries according to claim 9, wherein in the step (2), an extrusion temperature of extruders A and C is 230° C., and the extrusion temperature of extruder B is 255° C.

### Claim 16 (depends on 10)

The method for preparing a self-assembled CPP base film of an aluminum-plastic film for new energy pouch batteries according to claim 10, wherein in the step (2), an extrusion temperature of extruders A and C is 230° C., and the extrusion temperature of extruder B is 255° C.

### Claim 17 (depends on 11)

The method for preparing a self-assembled CPP base film of an aluminum-plastic film for new energy pouch batteries according to claim 11, wherein in the step (2), an extrusion temperature of extruders A and C is 230° C., and the extrusion temperature of extruder B is 255° C.

### Claim 18 (depends on 12)

The method for preparing a self-assembled CPP base film of an aluminum-plastic film for new energy pouch batteries according to claim 12, wherein in the step (2), an extrusion temperature of extruders A and C is 230° C., and the extrusion temperature of extruder B is 255° C.