# US 2026/0066368 A1 · Method for charging rechargeable lithium battery

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0066368 A1
- Document ID: US20260066368A1
- Status: Published application
- Kind: A1
- Application number: 19/316,518
- Filed: 2025-09-02
- Published: 2026-03-05
- Earliest claimed: 2024-09-02
- Assignees: Samsung SDI Co., Ltd.; Postech Research and Business Development Foundation
- Applicants: Samsung SDI Co., Ltd.; Postech Research and Business Development Foundation
- Inventors: Seok Mun KANG; Jaesang YOON; Youngsun KONG; Young-Ki KIM; Yong-Tae KIM; Jaesub KWON; Kyu-Young PARK
- Web page: https://patentgrep.com/patent/US20260066368A1

## CPC

- H01M 4/52: of nickel, cobalt or iron
- H01M 10/44: Methods for charging or discharging (circuits for charging H02J7/00)
- C01G 53/42: containing alkali metals, e.g. LiNiO2
- C01G 53/50: of the type (MnO2)n-, e.g. Li(NixMn1-x)O2 or Li(MyNixMn1-x-y)O2
- H01M 4/525: of mixed oxides or hydroxides containing iron, cobalt or nickel for inserting or intercalating light metals, e.g. LiNiO2, LiCoO2 or LiCoOxFy
- H01M 10/052: Li-accumulators
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- H01M 10/446: {Initial charging measures}
- C01P 2002/54: one element only
- C01P 2004/03: obtained by SEM
- C01P 2004/50: Agglomerated particles
- C01P 2004/61: Micrometer sized, i.e. from 1-100 micrometer
- C01P 2006/40: Electric properties
- H01M 2004/028: {Positive electrodes}
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- C01G: COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSES C01D OR C01F (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts or peroxyacids C01B15/00; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium, or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds containing nitrogen, other non-metals and metal C01B21/082}; metal amides C01B21/092; nitrites C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; compounds having molecular sieve properties but not having base-exchange properties C01B37/00; compounds having molecular sieve and base-exchange properties, e.g. crystalline zeolites, C01B39/00; cyanides C01C3/08; salts of cyanamide C01C3/16; thiocyanates C01C3/20)
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

The present disclosure relates to a method for charging a rechargeable lithium battery including constant-current charging the rechargeable lithium battery at a current density of 4 C to 10 C; and constant-voltage charging the rechargeable lithium battery, wherein the rechargeable lithium battery includes a positive electrode active material including a lithium nickel-based composite oxide having a nickel content of greater than or equal to about 80 mol % based on 100 mol % of metals excluding lithium.

## Claims

### Claim 1

A method for charging a rechargeable lithium battery, the method comprising:
constant-current charging the rechargeable lithium battery at a current density of 4 C to 10 C; and constant-voltage charging the rechargeable lithium battery,
wherein the rechargeable lithium battery comprises a positive electrode active material comprising a lithium nickel-based composite oxide having a nickel content of greater than or equal to about 80 mol % based on 100 mol % of metals excluding lithium.

### Claim 2 (depends on 1)

The method as claimed in claim 1, wherein:
a current density in the constant-current charging is 5 C to 10 C.

### Claim 3 (depends on 1)

The method as claimed in claim 1, wherein
in the constant-current charging, the rechargeable lithium battery is charged to a charge cut-off voltage of about 4.2 V to about 5 V.

### Claim 4 (depends on 1)

The method as claimed in claim 1, wherein:
in a differential capacity (Dq/Dv)-voltage (V) graph evaluated under conditions of 1 C=200 mAh/g, 5 C, 3.6V to 4.3V after formation,
the rechargeable lithium battery exhibits a first peak that appears at a charging voltage of between about 3.8 V and about 3.9 V; a second peak that appears at a charging voltage of between about 4.0 V and about 4.1 V; and a third peak that appears at a charging voltage of between about 4.25 V and about 4.3 V.

### Claim 5 (depends on 4)

The method as claimed in claim 4, wherein:
the third peak is a peak where the positive electrode active material undergoes a phase transition from H2 (hexagonal 2) to H3 (hexagonal 3) during the charging process.

### Claim 6 (depends on 4)

The method as claimed in claim 4, wherein:
if an intensity of the first peak is I1, an intensity of the second peak is I2, and an intensity of the third peak is I3, I1>I2>I3 is satisfied.

### Claim 7 (depends on 1)

The method as claimed in claim 1, wherein:
in the constant-voltage charging, the rechargeable lithium battery is charged to a charging capacity of about 175 mAh/g to about 240 mAh/g.

### Claim 8 (depends on 1)

The method as claimed in claim 1, wherein:
the positive electrode active material is in a form of secondary particles formed by agglomeration of a plurality of primary particles.

### Claim 9 (depends on 1)

The method as claimed in claim 1, wherein:
an average particle diameter (D50) of the positive electrode active material is about 10 μm to about 18 μm.

### Claim 10 (depends on 1)

The method as claimed in claim 1, wherein:
the positive electrode active material comprises a high-nickel positive electrode active material in which the nickel content is greater than or equal to about 90 mol % based on 100 mol % of metal excluding lithium.

### Claim 11 (depends on 1)

The method as claimed in claim 1, wherein:
the positive electrode active material comprises a lithium nickel-based composite oxide represented by Chemical Formula 1:
wherein, in Chemical Formula 1, 0.9≤a1≤1.8, 0.8≤x1≤1, 0≤y1≤0.2, 0≤z1≤0.2, 0.9≤x1+y1+z1≤1.1, and 0≤b1≤0.1, M1 and M2 are each independently one or more elements selected from Al, B, Ba, Ca, Ce, Co, Cr, Cu, Fe, Mg, Mn, Mo, Nb, Si, Sr, Ti, V, W, and Zr, and X is one or more elements selected from F, P, and S.

### Claim 12 (depends on 1)

The method as claimed in claim 1, wherein:
the positive electrode active material comprises a lithium nickel-manganese-based composite oxide represented by Chemical Formula 2:
wherein, in Chemical Formula 2, 0.9≤a2≤1.8, 0.8≤x2<1, 0<y2≤0.2, 0≤z2≤0.2, 0.9≤x2+y2+z2≤1.1, and 0≤b2≤0.1, M3 is or more elements selected from Al, B, Ba, Ca, Ce, Cr, Fe, Mg, Co, Mo, Nb, Si, Sr, Ti, V, W, and Zr, and X is one or more elements selected from F, P, and S.

### Claim 13 (depends on 1)

The method as claimed in claim 1, wherein:
the positive electrode active material comprises a lithium nickel-cobalt-based composite oxide represented by Chemical Formula 3:
wherein, in Chemical Formula 3, 0.9≤a3≤1.8, 0.8≤x3<1, 0<y3≤0.2, 0≤z3≤0.2, 0.9≤x3+y3+z3≤1.1, and 0≤b3≤0.1, M4 is one or more elements selected from Al, B, Ba, Ca, Ce, Cr, Fe, Mg, Mn, Mo, Nb, Si, Sr, Ti, V, W, and Zr, and X is one or more elements selected from F, P, and S.

### Claim 14 (depends on 1)

The method as claimed in claim 1, wherein:
the rechargeable lithium battery comprises a positive electrode active material layer comprising the positive electrode active material, and
a loading level of the positive electrode active material layer is about 10 mg/cm2 to about 40 mg/cm2.

### Claim 15 (depends on 14)

The method as claimed in claim 14, wherein:
a density of the positive electrode active material layer is about 3.0 g/cc to about 3.7 g/cc.