# US 2026/0066340 A1 · Method for preparing solid state electrolyte membrane structure

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0066340 A1
- Document ID: US20260066340A1
- Status: Published application
- Kind: A1
- Application number: 18/822,018
- Filed: 2024-08-30
- Published: 2026-03-05
- Earliest claimed: 2024-08-30
- Assignees: Microvast, Inc.
- Applicants: Microvast, Inc.
- Inventors: Huijie GUO; Bryan Thomas Yonemoto
- Web page: https://patentgrep.com/patent/US20260066340A1

## CPC

- H01M 10/0562: Solid materials
- H01M 10/052: Li-accumulators
- H01M 10/056: characterised by the materials used as electrolytes, e.g. mixed inorganic/organic electrolytes
- H01M 50/403: Manufacturing processes of separators, membranes or diaphragms
- H01M 2300/0068: inorganic
- H01M 2300/0071: Oxides
- H01M 2300/0094: in the form of layered products, e.g. coatings
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A method for preparing a solid-state electrolyte membrane structure. The method includes: S1, proportionally mixing raw materials of a solid-state electrolyte to obtain a mixed powder; S2, mixing the mixed powder, a binder and a solvent together to obtain a solid-state electrolyte precursor slurry; S3, coating the solid-state electrolyte precursor slurry on a substrate to obtain a solid-state electrolyte precursor coating layer; and S4, subjecting the solid-state electrolyte precursor coating layer to a laser treatment to obtain the solid-state electrolyte membrane structure.

## Claims

### Claim 1

A method for preparing a solid-state electrolyte membrane structure, comprising
step S1, proportionally mixing raw materials of a solid-state electrolyte to obtain a mixed powder;
step S2, mixing the mixed powder, a binder and a solvent together to obtain a solid-state electrolyte precursor slurry;
step S3, coating the solid-state electrolyte precursor slurry on a substrate to obtain a solid-state electrolyte precursor coating layer; and
step S4, subjecting the solid-state electrolyte precursor coating layer to a laser treatment to obtain the solid-state electrolyte membrane structure.

### Claim 2 (depends on 1)

The method of claim 1, wherein the raw materials of the solid-state electrolyte comprises a lithium source and a second metal source, and a second metal of the second metal source is selected from the group consisting of Al, Ti, Zr, La, Ta, Nb, and any combination thereof.

### Claim 3 (depends on 2)

The method of claim 2, wherein the lithium source is selected from the group consisting of lithium salts, Li2O, LiOH, and any combination thereof; and the second metal source is selected from the group consisting of second metal salts, second metal oxide, second metal hydroxide, and any combination thereof.

### Claim 4 (depends on 2)

The method of claim 2, wherein the lithium source is selected from the group consisting of Li2SO4, LiNO3, LiCl, Li2O, LiOH, and any combination thereof; and the second metal source is selected from the group consisting of Al2O3, TiO2, ZrO2, La2O3, Ta2O5, Nb2O5, La(NO3)3, and any combination thereof.

### Claim 5 (depends on 2)

The method of claim 2, wherein the raw materials of the solid-state electrolyte further comprises a phosphorus source, the phosphorus source comprises a phosphate group, the phosphate group is selected from the group consisting of NH4H2PO4, (NH4)3PO4, (NH4)2HPO4, and any combination thereof.

### Claim 6 (depends on 1)

The method of claim 1, wherein in step S1, proportionally mixing raw materials of the solid-state electrolyte to obtain the mixed powder comprises grinding the raw materials of the solid-state electrolyte to obtain the mixed powder, and an average particle size of the mixed powder is smaller than or equal to 300 nm.

### Claim 7 (depends on 1)

The method of claim 1, wherein in step S2, a mass ratio of the binder to the mixed powder is in a range of 1:100 to 5:95.

### Claim 8 (depends on 1)

The method of claim 1, wherein in step S2, a viscosity of the solid-state electrolyte precursor slurry is in a range of 2000 cPs to 9000 cPs.

### Claim 9 (depends on 1)

The method of claim 1, wherein in step S3, the substrate comprises a current collector or an electrode plate.

### Claim 10 (depends on 1)

The method of claim 1, wherein step S4, before the step of subjecting the solid-state electrolyte precursor coating layer to the laser treatment, further comprises a sstep of subjecting the solid-state electrolyte precursor coating layer to a preheating treatment, a temperature of the preheating treatment is lower than a temperature at which the solid-state electrolyte precursor coating layer reacts chemically, and a temperature difference between the temperature of the preheating treatment and the temperature at which the solid-state electrolyte precursor coating layer reacts chemically is smaller than or equal to 400° C.

### Claim 11 (depends on 10)

The method of claim 10, wherein the temperature of the preheating treatment is in a range of 400° C. to 800° C.

### Claim 12 (depends on 10)

The method of claim 10, wherein the preheating treatment is a gradient preheating treatment.

### Claim 13 (depends on 12)

The method of claim 12, wherein the gradient preheating treatment comprises: heating the solid-state electrolyte precursor coating layer at a first heating rate in a range of 1° C./min to 20° C./min, and then heating the solid-state electrolyte precursor coating layer at a second heating rate in a range of 20° C./min to 50° C./min to the temperature of the preheating treatment.

### Claim 14 (depends on 10)

The method of claim 10, wherein step S4, after a temperature of the solid-state electrolyte precursor coating layer reaches the temperature of the preheating treatment, holding the solid-state electrolyte precursor coating layer for 1 minute to 10 minutes, and then subjecting the solid-state electrolyte precursor coating layer to the laser treatment.

### Claim 15 (depends on 1)

The method of claim 1, wherein step S4, before the step of subjecting the solid electrolyte precursor coating layer to the laser treatment, further comprises a step of drying the solid-state electrolyte precursor coating layer and applying a pressure to the solid-state electrolyte precursor coating layer.

### Claim 16 (depends on 1)

The method of claim 1, wherein in step S4, before the step of subjecting the solid electrolyte precursor coating layer to the laser treatment, a porosity of the solid-state electrolyte precursor coating layer is in a range of 5% to 40%.

### Claim 17 (depends on 1)

The method of claim 1, wherein in step S4, before the step of subjecting the solid electrolyte precursor coating layer to the laser treatment, a thickness of the solid-state electrolyte precursor coating layer is in a range of 5 μm to 100 μm.

### Claim 18 (depends on 1)

The method of claim 1, wherein in step S4, a wavelength of a laser for the laser treatment is in a range of 900 nm to 1200 nm, and a power of the laser for the laser treatment is in a range of 20 W to 150 W.

### Claim 19 (depends on 1)

The method of claim 1, wherein in step S4, the solid-state electrolyte structure comprises the substrate and a solid-state electrolyte membrane fixed on the substrate;
after the step of obtaining the solid-state electrolyte membrane structure, the method further comprises repeating a step of coating the solid-state electrolyte precursor slurry on the solid-state electrolyte membrane to obtain the solid-state electrolyte precursor coating layer and a step of subjecting the solid-state electrolyte precursor coating layer to the laser treatment to accomplish a chemical reaction of the solid-state electrolyte precursor coating layer, so as to increase a thickness of the solid-state electrolyte membrane.