# US 2026/0066338 A1 · Systems and methods for lithium metal deposition

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0066338 A1
- Document ID: US20260066338A1
- Status: Published application
- Kind: A1
- Application number: 19/196,599
- Filed: 2025-05-01
- Published: 2026-03-05
- Earliest claimed: 2021-02-11
- Assignees: Pure Lithium Corporation
- Applicants: Pure Lithium Corporation
- Inventors: Donald R. SADOWAY; Paul J. BURKE
- Web page: https://patentgrep.com/patent/US20260066338A1

## CPC

- H01M 10/056: characterised by the materials used as electrolytes, e.g. mixed inorganic/organic electrolytes
- C22B 7/001: {Dry processes}
- C22B 26/12: Obtaining lithium
- C25D 5/12: at least one layer being of nickel or chromium
- C25D 21/12: Process control or regulation (controlling or regulating in general G05)
- H01M 4/382: {Lithium (H01M4/405 takes precedence)}
- H01M 4/387: {Tin or alloys based on tin}
- H01M 10/052: Li-accumulators
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- H01M 2004/027: {Negative electrodes}
- H01M 2300/0022: Room temperature molten salts
- H01M 2300/0082: Organic polymers
- Y02W 30/84: Recycling of batteries or fuel cells
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- C22B: PRODUCTION AND REFINING OF METALS (electrolytic C25); PRETREATMENT OF RAW MATERIALS
- C25D: PROCESSES FOR THE ELECTROLYTIC OR ELECTROPHORETIC PRODUCTION OF COATINGS; ELECTROFORMING; APPARATUS THEREFOR
- Y02W: CLIMATE CHANGE MITIGATION TECHNOLOGIES RELATED TO WASTEWATER TREATMENT OR WASTE MANAGEMENT

## Abstract

Provided are a conformable polymer coated lithium metal electrode, a solid electrolyte, and an inorganic molten salt electrolyte for a rechargeable lithium metal battery. Systems and methods are also provided for controlling the electroplating of lithium metal onto negative electrodes to allow for more rapid recharging of lithium metal batteries while minimizing dendrite formation.

## Claims

### Claim at position 1

-39. (canceled)

### Claim 40

A rechargeable metal displacement battery comprising:
a negative electrode, wherein the negative electrode comprises a conductive substrate coated with a layer of a first metal having an inner face and an outer face, wherein the inner face is configured to contact the conductive substrate;
a positive electrode, wherein the positive electrode comprises a second metal;
a solid electrolyte comprising a conformable polymer that preferentially conducts ions of the first metal compared to ions of the second metal, and that coats the outer face of the layer of the first metal; and
a molten salt electrolyte, wherein the molten salt electrolyte is a mixture of inorganic salts comprising a first salt of the first metal and a salt of the second metal, wherein the melting temperature of the molten salt electrolyte is less than 140° C.,
wherein the molten salt electrolyte is disposed between the solid electrolyte and the positive electrode, and is in direct physical contact with both the solid electrolyte and the positive electrode, and
wherein the first metal is more electropositive than the second metal.

### Claim 41 (depends on 40)

The rechargeable metal displacement battery of claim 40, wherein the conformable polymer is a graft or block copolymer with a first segment and a second segment, wherein each segment of the first and second segments is above its respective glass transition temperature, Tg, wherein the first segment is formed from groups configured to solvate a second salt of the first metal and the second segment is immiscible with the first segment, and wherein the second salt of the first metal is dispersed within the solid electrolyte.

### Claim 42 (depends on 40)

The rechargeable metal displacement battery of claim 40, wherein the first metal is selected from the group consisting of an alkali metal, an alkaline earth metal, and aluminum.

### Claim 43 (depends on 40)

The rechargeable metal displacement battery of claim 40, wherein the second metal is selected from the group consisting of Fe, Ni, Bi, Pb, Zn, Sn, and Cu.

### Claim 44 (depends on 40)

The rechargeable metal displacement battery of claim 40, wherein the mixture of inorganic salts comprises one or more salts selected from the group consisting of aluminum salts, titanium salts, iron salts, alkali metal salts, alkaline earth metal salts, ammonium salts, and combinations thereof.

### Claim 45 (depends on 40)

The rechargeable metal displacement battery of claim 40, wherein the mixture of inorganic salts comprises aluminum salts, and wherein the molar percentage of the aluminum salts is at least 50%.

### Claim 46 (depends on 40)

The rechargeable metal displacement battery of claim 40, wherein the mixture of inorganic salts comprises iron salts, and wherein the molar percentage of the iron salts is at least 50%.

### Claim 47 (depends on 40)

The rechargeable metal displacement battery of claim 40, wherein the mixture of inorganic salts comprises anions chosen from the group consisting of halides, nitrates, nitrites, sulfates, sulfites, carbonates, hydroxides, and combinations thereof.

### Claim 48 (depends on 40)

The rechargeable metal displacement battery of claim 40, wherein the mixture of inorganic salts comprises aluminum chloride, wherein the molar percentage of aluminum chloride is at least 50%.

### Claim 49 (depends on 40)

The rechargeable metal displacement battery of claim 40, wherein the mixture of inorganic salts comprises ferric chloride, wherein the molar percentage of ferric chloride is at least 50%.

### Claim 50

A process for recycling battery scrap containing one or more transition metal oxides comprising:
submerging the battery scrap in a melt comprising a glass-forming oxide;
holding the melt at a temperature between about 600° C. and about 1100° C., thereby allowing the one or more transition metal oxides to dissolve in the melt;
disposing an anode and a first cathode in the melt; and
applying a voltage across the anode and the first cathode, thereby generating oxygen at the anode and electroplating a first transition metal onto the first cathode.

### Claim 51 (depends on 50)

The process for recycling battery scrap according to claim 50, wherein the voltage is applied in order to maintain a constant current.

### Claim 52 (depends on 51)

The process for recycling battery scrap according to claim 51, further comprising:
continuing to apply voltage to maintain a constant current until a rise in voltage indicates depletion of the first transition metal oxide from the melt; and
removing the first cathode with first electroplated transition metal from the melt.

### Claim 53

A system configured for monitoring and controlling electrolytic deposition of metal in an electrolytic cell, the electrolytic cell including a positive electrode, a negative electrode, and an electrolyte providing a source of metal ions for electrodeposition onto the negative electrode, the system comprising:
a variable direct current (dc) voltage source configured to receive a first control signal, and to provide a dc voltage across the positive electrode and the negative electrode based on the first control signal;
a variable alternating current source configured to receive a second control signal, and to provide alternating current across the positive electrode and the negative electrode based on the second control signal;
an electrochemical noise monitor configured to monitor current and voltage across the positive electrode and the negative electrode and to produce an output signal indicative of the current and voltage noise across the positive electrode and the negative electrode;
an analysis and control system configured to receive the output signal, and to analyze the output signal to calculate a power spectrum of the noise, and further configured to output the first control signal to the variable de voltage source, and the second control signal to the variable alternating current source, the first control signal and the second control signal being determined based on user-determined input parameters and on the power spectrum of the noise,
wherein the system is configured such that, during operation, the de voltage and the alternating current control the surface features of the metal electrodeposited on the negative electrode based on the first control signal and the second control signal, respectively.

### Claim 54 (depends on 53)

The system according to claim 53, the first control signal determining the magnitude and direction of the de voltage.

### Claim 55 (depends on 53)

The system according to claim 53, the second control signal determining the magnitude and frequency of the alternating current.

### Claim 56 (depends on 53)

The system according to claim 53, wherein the metal electrodeposited on the negative electrode comprises lithium.

### Claim 57 (depends on 53)

The system according to claim 53, wherein the electrolytic cell is a rechargeable lithium metal battery.

### Claim 58 (depends on 53)

The system according to claim 53, wherein, during operation, the dc voltage and the alternating current are controlled by the first control signal and the second control signal in order to reduce dendrite formation.

### Claim 59 (depends on 53)

The system according to claim 53, wherein, during operation, the dc voltage is reversed in order to reduce dendrite formation.