# US 2026/0066307 A1 · Anode for secondary battery, manufacturing method thereof, and lithium secondary battery including the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0066307 A1
- Document ID: US20260066307A1
- Status: Published application
- Kind: A1
- Application number: 19/310,934
- Filed: 2025-08-27
- Published: 2026-03-05
- Earliest claimed: 2024-09-02
- Assignees: SK On Co., Ltd.
- Applicants: SK On Co., Ltd.
- Inventors: Won Joon JANG
- Web page: https://patentgrep.com/patent/US20260066307A1

## CPC

- H01M 4/626: {Metals}
- H01M 4/0404: {by coating on electrode collectors}
- H01M 4/133: Electrodes based on carbonaceous material, e.g. graphite-intercalation compounds or CFx
- H01M 4/1393: of electrodes based on carbonaceous material, e.g. graphite-intercalation compounds or CFx
- H01M 4/587: for inserting or intercalating light metals
- H01M 4/622: {being polymers}
- H01M 10/052: Li-accumulators
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- H01M 2004/021: {Physical characteristics, e.g. porosity, surface area}
- H01M 2004/027: {Negative electrodes}
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

An anode for a secondary battery includes an anode current collector, an anode mixture layer disposed on at least one surface of the anode current collector and including an anode active material and an anode binder, and at least one gap that is open on a surface of the anode mixture layer and extends toward the anode current collector. An angle (θ) between the gap and a surface of the anode current collector is 70° to 110°. A method of manufacturing an anode for a secondary battery includes coating by applying an anode slurry containing an anode active material, a binder, and a magnetic material to at least one surface of an anode current collector, recovering the magnetic material contained in the anode slurry using a magnet spaced apart on the anode slurry, and drying the anode slurry and manufacturing an anode mixture layer.

## Claims

### Claim 1

An anode for a secondary battery, comprising:
an anode current collector;
an anode mixture layer disposed on at least one surface of the anode current collector and including an anode active material and an anode binder; and
at least one gap open on a surface of the anode mixture layer and extending toward the anode current collector,
wherein an angle (θ) between the gap and a surface of the anode current collector is 70° to 110°.

### Claim 2 (depends on 1)

The anode for a secondary battery of claim 1, wherein the anode mixture layer includes two or more gaps, and an angle (θ) between each of the gaps is 0° to 20°.

### Claim 3 (depends on 1)

The anode for a secondary battery of claim 1, wherein an upper end diameter of the gap is 100 nm to 100 μm.

### Claim 4 (depends on 1)

The anode for a secondary battery of claim 1, wherein a difference between the upper end diameter and the lower end diameter of the gap is 0% to 20%.

### Claim 5 (depends on 1)

The anode for a secondary battery of claim 1, wherein a ratio of a height of the gap to a thickness of the anode mixture layer is 1:0.2 to 1:1.

### Claim 6 (depends on 1)

The anode for a secondary battery of claim 1, wherein the anode mixture layer further includes a magnetic material.

### Claim 7 (depends on 6)

The anode for a secondary battery of claim 6, wherein the magnetic material is at least one selected from the group consisting of Fe3O4, Alnico, Mn—Al—C, Fe—Cr—Co, and Ni—Fe.

### Claim 8 (depends on 1)

The anode for a secondary battery of claim 1, wherein the anode active material includes a carbon-based material.

### Claim 9 (depends on 8)

The anode for a secondary battery of claim 8, wherein the carbon-based material has an OI value of 0.4 to 1.0 according to Equation 1, OI=I004/I110, where OI is an orientation Index measured by XRD, I004 is a peak intensity of the (004) plane measured by XRD for the carbon-based material, and I110 is a peak intensity of the (110) plane measured by XRD for the carbon-based material.

### Claim 10 (depends on 1)

The anode for a secondary battery of claim 1, wherein the anode binder is an aqueous binder.

### Claim 11 (depends on 10)

The anode for a secondary battery of claim 10, wherein the aqueous binder is at least one selected from the group consisting of styrene-butadiene rubber (SBR) and carboxymethyl cellulose (CMC).

### Claim 12

A method of manufacturing an anode for a secondary battery, comprising:
(a) applying a first anode slurry containing an anode active material, a binder, and a magnetic material to at least one surface of an anode current collector and forming a coating layer;
(b) recovering the magnetic material contained in the first anode slurry using a magnet spaced apart on the coating layer; and
(c) drying the anode slurry and manufacturing an anode mixture layer.

### Claim 13 (depends on 12)

The method of claim 12, wherein the (a) applying, the (b) recovering and the (c) drying are performed by conveying the substrate using a conveying section, and a conveying speed thereof is 30 m/min to 180 m/min.

### Claim 14 (depends on 12)

The method of claim 12, after the (a) applying, further comprising applying a second anode slurry containing an anode active material and a binder and not containing a magnetic material, onto the coating layer with the first anode slurry having been applied thereto.

### Claim 15 (depends on 14)

The method of claim 14, wherein a thickness ratio of the second anode slurry to the applied first anode slurry is 1:0.2 to 1:1.

### Claim 16 (depends on 12)

The method of claim 12, wherein the magnetic material is at least one selected from the group consisting of Fe3O4, Alnico, Mn—Al—C, Fe—Cr—Co, and Ni—Fe.

### Claim 17 (depends on 12)

The method of claim 12, wherein a strength of the magnet is 4,000 to 20,000 Gauss.

### Claim 18 (depends on 1)

A lithium secondary battery comprising the anode for a secondary battery according to claim 1.