# US 2026/0066286 A1 · Metal composite hydroxide and method for producing same, positive electrode active material for non-aqueous electrolyte secondary battery and method for producing same, and non-aqueous electrolyte secondary battery using same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0066286 A1
- Document ID: US20260066286A1
- Status: Published application
- Kind: A1
- Application number: 19/381,277
- Filed: 2025-11-06
- Published: 2026-03-05
- Earliest claimed: 2017-07-12
- Assignees: Sumitomo Metal Mining Co., Ltd.
- Applicants: Sumitomo Metal Mining Co., Ltd.
- Inventors: Tatsuya Takahashi; Hiroko Senba; Taira Aida
- Web page: https://patentgrep.com/patent/US20260066286A1

## CPC

- C01G 53/82: Compounds containing nickel, with or without oxygen or hydrogen, and containing two or more other elements
- H01M 4/505: of mixed oxides or hydroxides containing manganese for inserting or intercalating light metals, e.g. LiMn2O4 or LiMn2OxFy
- C01G 53/40: Complex oxides containing nickel and at least one other metal element
- C01G 53/502: containing lithium and cobalt
- H01M 4/36: Selection of substances as active materials, active masses, active liquids
- H01M 4/366: {as layered products}
- H01M 4/525: of mixed oxides or hydroxides containing iron, cobalt or nickel for inserting or intercalating light metals, e.g. LiNiO2, LiCoO2 or LiCoOxFy
- H01M 10/052: Li-accumulators
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- C01P 2002/52: containing elements as dopants
- C01P 2002/60: Compounds characterised by their crystallite size
- C01P 2002/72: by d-values or two theta-values, e.g. as X-ray diagram
- C01P 2004/45: Aggregated particles or particles with an intergrown morphology
- C01P 2004/50: Agglomerated particles
- C01P 2004/51: Particles with a specific particle size distribution
- C01P 2004/61: Micrometer sized, i.e. from 1-100 micrometer
- C01P 2004/84: one phase coated with the other
- C01P 2004/86: Thin layer coatings, i.e. the coating thickness being less than 0.1 time the particle radius
- C01P 2006/11: Powder tap density
- C01P 2006/40: Electric properties
- H01M 2004/028: {Positive electrodes}
- Y02E 60/10: Energy storage using batteries
- C01G: COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSES C01D OR C01F (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts or peroxyacids C01B15/00; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium, or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds containing nitrogen, other non-metals and metal C01B21/082}; metal amides C01B21/092; nitrites C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; compounds having molecular sieve properties but not having base-exchange properties C01B37/00; compounds having molecular sieve and base-exchange properties, e.g. crystalline zeolites, C01B39/00; cyanides C01C3/08; salts of cyanamide C01C3/16; thiocyanates C01C3/20)
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A method for producing a metal composite hydroxide, which includes a first crystallization process of obtaining first metal composite hydroxide particles by supplying a first raw material aqueous solution containing a metal element and an ammonium ion donor to a reaction tank, adjusting a pH of a reaction aqueous solution in the reaction tank, and performing a crystallization reaction and a second crystallization process of forming a tungsten-concentrated layer on a surface of the first metal composite hydroxide particles and obtaining second metal composite hydroxide particles by supplying a second raw material aqueous solution containing a metal element and a more amount of tungsten than the first raw material aqueous solution and an ammonium ion donor to a reaction aqueous solution containing the first metal composite hydroxide particles, adjusting a pH of the reaction aqueous solution, and performing a crystallization reaction, and the like.

## Claims

### Claim 1

A method for producing a metal composite hydroxide that contains nickel, manganese, and tungsten and optionally cobalt and element M and has a ratio of number of atoms of the respective metal elements represented by Ni:Mn:Co:W:M=x:y:z:a:b (x+y+z=1, 0.3≤x≤0.95, 0.05≤y≤0.55, 0≤z≤0.4, 0<a≤0.1, 0≤b≤0.1, and M is one or more elements selected from Mg, Ca, Al, Ti, V, Cr, Zr, Nb, Mo, Hf, and Ta), the method comprising:
a first crystallization process of obtaining first metal composite hydroxide particles by supplying a first raw material aqueous solution containing at least one among the metal elements and an ammonium ion donor to a reaction tank, adjusting a pH of a reaction aqueous solution in the reaction tank, and performing a crystallization reaction; and
a second crystallization process of forming a tungsten-concentrated layer on a surface of the first metal composite hydroxide particles and obtaining second metal composite hydroxide particles by supplying a second raw material aqueous solution containing at least one among the metal elements and a more amount of tungsten than the first raw material aqueous solution and an ammonium ion donor to a reaction aqueous solution containing the first metal composite hydroxide particles, adjusting a pH of the reaction aqueous solution, and performing a crystallization reaction.

### Claim 2 (depends on 1)

The method for producing a metal composite hydroxide according to claim 1, wherein
the first crystallization process includes a nuclear generation process of performing nuclear generation and a particle growth process of performing particle growth, and the second crystallization process includes performing particle growth following the particle growth process in the first crystallization process, and
the particle growth in the first crystallization process and the second crystallization process includes adjusting a pH of the reaction aqueous solution to be lower than a pH value of the reaction aqueous solution in the nuclear generation process and is performed in a non-oxidizing atmosphere having an oxygen concentration of 1 vol % or less.

### Claim 3 (depends on 1)

The method for producing a metal composite hydroxide according to claim 1, wherein the nuclear generation in the first crystallization process is performed in an oxidizing atmosphere having an oxygen concentration of more than 1 vol %.

### Claim 4 (depends on 1)

The method for producing a metal composite hydroxide according to claim 1, wherein supply of the second raw material aqueous solution in the second crystallization process is performed after the metal element in the first raw material aqueous solution is supplied to the reaction tank in a range of 50 mass % or more and 95 mass % or less with respect to a total amount of metal added in the first crystallization process and the second crystallization process.

### Claim 5 (depends on 1)

The method for producing a metal composite hydroxide according to claim 1, wherein the second crystallization process includes forming the tungsten-concentrated layer so as to have a thickness of 100 nm or less in a direction from a surface of the second metal composite hydroxide particles toward a center.

### Claim 6 (depends on 1)

The method for producing a metal composite hydroxide according to claim 1, wherein addition of the second raw material aqueous solution in the second crystallization process is performed at a time point at which 50% or more and 95% or less of entire time during which particle growth is performed elapses in the first and second crystallization processes.

### Claim 7 (depends on 1)

The method for producing a metal composite hydroxide according to claim 1, wherein supply of the second raw material aqueous solution is performed by separately supplying the first raw material aqueous solution and an aqueous solution containing tungsten to the reaction aqueous solution.

### Claim 8 (depends on 7)

The method for producing a metal composite hydroxide according to claim 7, wherein a tungsten concentration in the aqueous solution containing tungsten is 0.1 mol/L or more.

### Claim 9

A metal composite hydroxide comprising: nickel, manganese, and tungsten and optionally cobalt and element M, and having a ratio of number of atoms of the respective metal elements represented by Ni:Mn:Co:W:M=x:y:z:a:b (x+y+z=1, 0.3≤x≤0.95, 0.05≤y≤0.55, 0≤z≤0.4, 0<a≤0.1, 0≤b≤0.1, and M is one or more elements selected from Mg, Ca, Al, Ti, V, Cr, Zr, Nb, Mo, Hf, and Ta), wherein
the metal composite hydroxide has a tungsten-concentrated layer on a surface layer.

### Claim 10 (depends on 9)

The metal composite hydroxide according to claim 9, wherein a thickness of the tungsten-concentrated layer is 100 nm or less.

### Claim 11 (depends on 9)

The metal composite hydroxide according to claim 9, wherein an average particle size of the metal composite hydroxide is 4.0 μm or more and 9.0 μm or less and [(d90−d10)/average particle size], which is an index indicating spread of particle size distribution, is 0.65 or less.

### Claim 12 (depends on 9)

The metal composite hydroxide according to claim 9, wherein the metal composite hydroxide includes secondary particles formed by aggregation of a plurality of primary particles, the secondary particles have a hollow structure, and a tap density of the metal composite hydroxide is 1.2 g/cm3 or more and 1.9 g/cm3 or less.

### Claim 13

A method for producing the positive electrode active material for non-aqueous electrolyte secondary battery, the method comprising:
a first process of producing a metal composite hydroxide that contains nickel, manganese, and tungsten and optionally cobalt and element M and has a ratio of number of atoms of the respective metal elements represented by Ni:Mn:Co:W:M=x:y:z:a:b (x+y+z=1, 0.3≤x≤0.95, 0.05≤y≤0.55, 0≤z≤0.4, 0<a≤0.1, 0≤b≤0.1, and M is one or more elements selected from Mg, Ca, Al, Ti, V, Cr, Zr, Nb, Mo, Hf, and Ta), the first process comprising:
a first crystallization process of obtaining first metal composite hydroxide particles by supplying a first raw material aqueous solution containing at least one among the metal elements and an ammonium ion donor to a reaction tank, adjusting a pH of a reaction aqueous solution in the reaction tank, and performing a crystallization reaction, and
a second crystallization process of forming a tungsten-concentrated layer on a surface of the first metal composite hydroxide particles and obtaining second metal composite hydroxide particles by supplying a second raw material aqueous solution containing at least one among the metal elements and a more amount of tungsten than the first raw material aqueous solution and an ammonium ion donor to a reaction aqueous solution containing the first metal composite hydroxide particles, adjusting a pH of the reaction aqueous solution, and performing a crystallization reaction;
a second process of obtaining a lithium mixture by mixing a lithium compound with at least either of the metal composite hydroxide obtained by the first process or a metal composite oxide obtained by subjecting the metal composite hydroxide to a thermal treatment; and
a third process of obtaining a lithium-metal composite oxide by firing the lithium mixture.

### Claim 14 (depends on 13)

The method for producing the positive electrode active material for non-aqueous electrolyte secondary battery according to claim 13, wherein a value of (d50 of the lithium-metal composite oxide/d50 of the metal composite hydroxide), which is an index indicating degree of aggregation of lithium-metal composite oxide particles, is adjusted to be 0.95 or more and 1.05 or less.