# US 2026/0066271 A1 · Cathode active material for lithium secondary battery, cathode for lithium secondary battery including the same and lithium secondary battery

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0066271 A1
- Document ID: US20260066271A1
- Status: Published application
- Kind: A1
- Application number: 19/305,799
- Filed: 2025-08-21
- Published: 2026-03-05
- Earliest claimed: 2024-08-28
- Assignees: SK On Co., Ltd.
- Applicants: SK On Co., Ltd.
- Inventors: Young Uk PARK; Min Cheol BEAK; Seung Hyun KIM; Min Suk KANG; Hyun Sung KANG; Ji Yae DO
- Web page: https://patentgrep.com/patent/US20260066271A1

## CPC

- H01M 4/364: {as mixtures}
- H01M 4/0404: {by coating on electrode collectors}
- H01M 4/525: of mixed oxides or hydroxides containing iron, cobalt or nickel for inserting or intercalating light metals, e.g. LiNiO2, LiCoO2 or LiCoOxFy
- H01M 4/5825: {Oxygenated metallic salts or polyanionic structures, e.g. borates, phosphates, silicates, olivines}
- H01M 10/052: Li-accumulators
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- H01M 2004/021: {Physical characteristics, e.g. porosity, surface area}
- H01M 2004/028: {Positive electrodes}
- H01M 2220/20: Batteries in motive systems, e.g. vehicle, ship, plane
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A cathode active material for a lithium secondary battery, a cathode for a lithium secondary battery including the same, and a lithium secondary battery are provided. The cathode active material for a lithium secondary battery includes: a first cathode active material including a lithium-nickel metal oxide in the form of a single particle; and a second cathode active material including lithium manganese iron phosphate. Accordingly, a lithium secondary battery with improved cell safety and high energy density per unit cell volume may be achieved.

## Claims

### Claim 1

A cathode active material for a lithium secondary battery comprising:
a first cathode active material comprising a lithium-nickel metal oxide in the form of a single particle; and
a second cathode active material comprising lithium manganese iron phosphate.

### Claim 2 (depends on 1)

The cathode active material for a lithium secondary battery according to claim 1, wherein the first cathode active material further comprises a lithium-nickel metal oxide in the form of a secondary particle, and the content ratio of the lithium-nickel metal oxide in the form of a single particle to the lithium-nickel metal oxide in the form of a secondary particle is 0.25 to 1.0.

### Claim 3 (depends on 1)

The cathode active material for a lithium secondary battery according to claim 1, wherein the first cathode active material further comprises a lithium-nickel metal oxide in the form of a secondary particle, and the content of the lithium-nickel metal oxide in the form of a single particle is 20% by weight to 50% by weight based on the total weight of the first cathode active material.

### Claim 4 (depends on 1)

The cathode active material for a lithium secondary battery according to claim 1, wherein the lithium manganese iron phosphate comprises 35 mol % to 75 mol % of manganese based on the total moles of elements excluding oxygen.

### Claim 5 (depends on 1)

The cathode active material for a lithium secondary battery according to claim 1, wherein the lithium-nickel metal oxide comprises 80 mol % or more of nickel, based on the total moles of elements excluding oxygen.

### Claim 6 (depends on 1)

The cathode active material for a lithium secondary battery according to claim 1, wherein the first cathode active material comprises a lithium-nickel metal oxide in the form of a single particle having a structure represented by Formula 1 below:
(in Formula 1, M1 comprises at least one selected from the group consisting of Fe, Na, Mg, Ca, Ti, V, Cr, Cu, Zn, Ge, Sr, Ag, Ba, Zr, Nb, Al, Mo, Ga, W, Y, La, Ta and B, and 0.5≤x≤1.0, 0≤y≤0.3, 0≤z≤0.3, 0≤k≤0.2, x+y+z+k=1, 0≤a≤0.5, 0.9≤b≤1.2).

### Claim 7 (depends on 1)

The cathode active material for a lithium secondary battery according to claim 1, wherein the second cathode active material comprises lithium manganese iron phosphate having a structure represented by Formula 2 below:
(in Formula 2, M3 is at least one selected from the group consisting of Ni, Co, Mg, Y, Zn, Ru, Ti, Nb, Mo, Cr, Cu, Zr, W, Ir and V, and 0.9≤f≤1.5, 0.01≤g≤0.65, 0.35≤h≤0.99, 0≤i≤0.1).

### Claim 8 (depends on 1)

The cathode active material for a lithium secondary battery according to claim 1, wherein the weight ratio of the first cathode active material based on the total weight of the cathode active material for a lithium secondary battery is 0.55 to 0.75.

### Claim 9 (depends on 1)

The cathode active material for a lithium secondary battery according to claim 1, wherein the weight ratio of the second cathode active material based on the total weight of the cathode active material for a lithium secondary battery is 0.25 to 0.45.

### Claim 10 (depends on 1)

The cathode active material for a lithium secondary battery according to claim 1, wherein the lithium-nickel metal oxide in the form of a single particle has a median particle diameter (D50) of 1 μm to 5 μm.

### Claim 11 (depends on 2)

The cathode active material for a lithium secondary battery according to claim 2, wherein the lithium-nickel metal oxide in the form of a secondary particle has a median particle diameter (D50) of 6 μm to 20 μm.

### Claim 12 (depends on 1)

A cathode for a lithium secondary battery:
a cathode current collector, and
a cathode active material layer disposed on the cathode current collector and comprising the cathode active material for a lithium secondary battery according to claim 1.

### Claim 13 (depends on 12)

The cathode for a lithium secondary battery according to claim 12, wherein a ratio of I(003)/I(104) measured on the surface of the cathode active material layer through X-ray diffraction (XRD) analysis is 2.5 to 18,
wherein I(003) represents the peak intensity of a (003) plane measured through X-ray diffraction (XRD) analysis, and I(104) represents the peak intensity of a (104) plane measured through X-ray diffraction (XRD) analysis.

### Claim 14 (depends on 13)

The cathode for a lithium secondary battery according to claim 13, wherein the ratio of I(003)/I(104) is 2.5 to 12.

### Claim 15 (depends on 12)

A lithium secondary battery comprising:
the cathode for a lithium secondary battery according to claim 12; and
an anode for a lithium secondary battery disposed to face the cathode for the lithium secondary battery.