# US 2026/0066262 A1 · Solid electrolyte-electrode assembly, methods for making, and an all-solid-state battery thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0066262 A1
- Document ID: US20260066262A1
- Status: Published application
- Kind: A1
- Application number: 19/315,180
- Filed: 2025-08-29
- Published: 2026-03-05
- Earliest claimed: 2024-08-30
- Assignees: LG Energy Solution, Ltd.; The Regents of the University of California
- Applicants: LG Energy Solution, Ltd.; The Regents of the University of California
- Inventors: Jung-Pil LEE; Jiyoung KIM; Dong Ju LEE; Zheng CHEN; Min-Sang SONG
- Web page: https://patentgrep.com/patent/US20260066262A1

## CPC

- H01M 4/0435: {Rolling or calendering}
- H01M 10/052: Li-accumulators
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- H01M 10/0562: Solid materials
- H01M 10/0585: of accumulators having only flat construction elements, i.e. flat positive electrodes, flat negative electrodes and flat separators
- H01M 2004/021: {Physical characteristics, e.g. porosity, surface area}
- H01M 2004/028: {Positive electrodes}
- H01M 2300/0068: inorganic
- Y02E 60/10: Energy storage using batteries
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

A solid electrolyte-electrode assembly, as well as an all-solid-state battery including the assembly are described. For instance, a solid electrolyte-cathode assembly can be formed by co-rolling a plurality of cathode particles and a plurality of solid electrolyte particles, which results in the simultaneous production of the assembly and makes it possible to achieve improved interface resistance between the electrolyte membrane and electrode to improve battery performance. Also, the resulting electrolyte can be thin, which improves the energy density, while also maintaining excellent strength by using an electrode as a support.

## Claims

### Claim 1

A method for manufacturing a solid electrolyte-cathode assembly, comprising:
providing a plurality of cathode particles;
providing a solid electrolyte, wherein the solid electrolyte is provided in the form of particles having an average particle size less than 5 μm;
providing a binder; and
co-rolling the plurality of cathode particles, the solid electrolyte, and the binder, under conditions to form the solid electrolyte-cathode assembly,
wherein the solid electrolyte-cathode assembly comprises a cathode layer having a thickness less than 200 μm, wherein the cathode layer structurally supports the solid electrolyte layer;
wherein a ratio of a thickness of the cathode layer to a thickness of the solid electrolyte layer is from 1:1 to 20:1.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the amount of binder is less than 2% wt.

### Claim 3 (depends on 1)

The method according to claim 1, wherein the amount of binder is less than 1% wt.

### Claim 4 (depends on 1)

The method according to claim 1, wherein the cathode layer has a thickness of about 25 μm to about 200 μm.

### Claim 5 (depends on 1)

The method according to claim 1, wherein the cathode layer has a thickness of about 50 μm to about 150 μm.

### Claim 6 (depends on 1)

The method according to claim 1, wherein the solid electrolyte layer has a thickness less than about 100 μm.

### Claim 7 (depends on 1)

The method according to claim 1, wherein the solid electrolyte layer has a thickness less than about 50 μm.

### Claim 8 (depends on 1)

The method according to claim 1, wherein a weight ratio of the plurality of cathode particles to the solid electrolyte is from 1:1 to 10:1.

### Claim 9 (depends on 1)

The method according to claim 1, wherein a ratio of a thickness of the cathode layer to a thickness of the solid electrolyte layer is from 1:1 to 10:1.

### Claim 10 (depends on 1)

The method according to claim 1, wherein the method is carried out under dry processing conditions.

### Claim 11 (depends on 1)

The method according to claim 1, wherein the co-rolling of the cathode particles is carried out at a temperature of from about room temperature to about 120° C.

### Claim 12 (depends on 1)

The method according to claim 1, wherein the cathode particles have an average particle size of 0.1 μm to 20 μm.

### Claim 13

A method for manufacturing a solid electrolyte-cathode assembly, comprising:
providing a plurality of cathode particles, wherein the cathode particles have an average particle size of 0.1 μm to 20 μm;
providing a solid electrolyte, wherein the solid electrolyte is provided in the form of particles having an average particle size less than 5 μm;
providing a binder; and
co-rolling the plurality of cathode particles, the solid electrolyte, and the binder, under conditions to form the solid electrolyte-cathode assembly,
wherein the co-rolling process is conducted at a speed of about 1 m/min to 10 m/min,
wherein the co-rolling produces a network-reinforced interface between the solid electrolyte and the cathode in the solid electrolyte-cathode assembly,
wherein the solid electrolyte-cathode assembly comprises a cathode layer having a thickness of more than 10 μm and less than 200 μm;
wherein an amount of the binder is less than 1%, such that contact between the cathode layer and the solid electrolyte layer is increased; and
wherein a ratio of a thickness of the cathode layer to a thickness of the solid electrolyte layer is from 1:1 to 20:1.

### Claim 14 (depends on 13)

The method according to claim 13, wherein a weight ratio of the plurality of cathode particles to the solid electrolyte is from 1:1 to 10:1.

### Claim 15 (depends on 13)

The method according to claim 13, wherein a ratio of a thickness of the cathode layer to a thickness of the solid electrolyte layer is from 1:1 to 10:1.

### Claim 16

A solid electrolyte-cathode assembly, prepared by:
providing a plurality of cathode particles;
providing a solid electrolyte, wherein the solid electrolyte is provided in the form of particles having an average particle size less than 5 μm;
providing a binder; and
co-rolling the plurality of cathode particles, the solid electrolyte, and the binder, under conditions to form the solid electrolyte-cathode assembly,
wherein the solid electrolyte-cathode assembly comprises a cathode layer having a thickness of more than 10 μm and less than 200 μm;
wherein the solid electrolyte-cathode assembly does not have a current collector;
wherein an amount of the binder is less than 1%, such that contact between the cathode layer and the solid electrolyte layer is increased; and
wherein a ratio of a thickness of the cathode layer to a thickness of the solid electrolyte layer is from 1:1 to 20:1.

### Claim 17 (depends on 16)

The solid electrolyte-cathode assembly according to claim 16, wherein a weight ratio of the cathode particles to the solid electrolyte is from 1:1 to 10:1.

### Claim 18 (depends on 16)

The solid electrolyte-cathode assembly according to claim 16, wherein a ratio of a thickness of the cathode layer to a thickness of the solid electrolyte layer is from 1:1 to 10:1.

### Claim 19 (depends on 16)

An all-solid-state battery comprising the solid electrolyte-cathode assembly according to claim 16.

### Claim 20 (depends on 19)

An all-solid-state battery according to claim 19, wherein the all-solid-state battery operates at a stack pressure of about 2 MPa or lower.