# US 2026/0063583 A1 · Electrode and electrochemical measurement system

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0063583 A1
- Document ID: US20260063583A1
- Status: Published application
- Kind: A1
- Application number: 19/381,288
- Filed: 2025-11-06
- Published: 2026-03-05
- Earliest claimed: 2023-05-11
- Assignees: Murata Manufacturing Co., Ltd.; Ryukoku University
- Applicants: Murata Manufacturing Co., Ltd.; Ryukoku University
- Inventors: Akira OSAKI; Shuichi Kawata; Yasuo Fujii; Yoshifumi Aoi; Megumi Kasuno
- Web page: https://patentgrep.com/patent/US20260063583A1

## CPC

- G01N 27/301: {Reference electrodes}
- G01N 27/30: Electrodes, e.g. test electrodes; Half-cells (G01N27/414 takes precedence)
- G01N 27/308: {at least partially made of carbon}
- G01N 27/48: using polarography, i.e. measuring changes in current under a slowly-varying voltage
- G01N: INVESTIGATING OR ANALYSING MATERIALS BY DETERMINING THEIR CHEMICAL OR PHYSICAL PROPERTIES (measuring or testing apparatus or processes other than immunoassay, involving enzymes or microorganisms C12M, C12Q)

## Abstract

An electrode that includes a carbon film having an sp2 bond and an sp3 bond, the carbon film having a proportion of the sp3 bond of from 0.3 to 0.45 and a full width at half maximum of a G band of from 135 cm−1 to 220 cm−1.

## Claims

### Claim 1

An electrode comprising:
a carbon film having an sp2 bond and an sp3 bond,
the carbon film having a proportion of the sp3 bond of from 0.3 to 0.45 and a full width at half maximum of a G-band of from 135 cm−1 to 220 cm−1.

### Claim 2 (depends on 1)

The electrode according to claim 1, wherein the proportion of the sp3 bond is from 0.3 to 0.42.

### Claim 3 (depends on 1)

The electrode according to claim 1, wherein the full width at half maximum of the G band is from 135 cm−1 to 210 cm−1.

### Claim 4 (depends on 1)

The electrode according to claim 1, wherein, in the carbon film, the proportion of the sp3 bond is from 0.3 to 0.42 and the full width at half maximum of the G band is from 135 cm−1 to 210 cm−1.

### Claim 5 (depends on 1)

The electrode according to claim 1, wherein the proportion of the sp3 bond is from 0.34 to 0.37.

### Claim 6 (depends on 1)

The electrode according to claim 1, wherein the full width at half maximum of the G band is from 185 cm−1 to 210 cm−1.

### Claim 7 (depends on 1)

The electrode according to claim 1, wherein, in the carbon film, the proportion of the sp3 bond is from 0.34 to 0.37 and the full width at half maximum of the G band is from 185 cm−1 to 210 cm−1.

### Claim 8 (depends on 1)

The electrode according to claim 1, wherein a thickness of the carbon film is from 5 nm to 500 nm.

### Claim 9 (depends on 1)

The electrode according to claim 1, wherein a thickness of the carbon film is from 10 nm to 300 nm.

### Claim 10 (depends on 1)

The electrode according to claim 1, further comprising:
an underlying substrate,
wherein the carbon film is on a surface of the underlying substrate.

### Claim 11 (depends on 10)

The electrode according to claim 10, wherein the underlying substrate has electrical conductivity.

### Claim 12 (depends on 10)

The electrode according to claim 10, wherein the underlying substrate includes a conductive inorganic substrate.

### Claim 13 (depends on 10)

The electrode according to claim 10, wherein the underlying substrate includes a conductive silicon substrate.

### Claim 14 (depends on 10)

The electrode according to claim 10, wherein a thickness of the underlying substrate is from 2 μm to 1000 μm.

### Claim 15 (depends on 10)

The electrode according to claim 10, wherein a thickness of the underlying substrate is from 20 μm to 500 μm.

### Claim 16 (depends on 10)

The electrode according to claim 10, wherein a thickness of the underlying substrate is from 2 μm to 1000 μm, and a thickness of the carbon film is from 5 nm to 500 nm.

### Claim 17 (depends on 10)

The electrode according to claim 10, wherein a thickness of the underlying substrate is from 20 μm to 500 μm, and a thickness of the carbon film is from 10 nm to 300 nm.

### Claim 18 (depends on 1)

An electrochemical measurement system comprising the electrode according to claim 1.

### Claim 19 (depends on 18)

The electrochemical measurement system according to claim 18, wherein the electrode is constructed as a working electrode for stripping voltammetry.

### Claim 20 (depends on 19)

The electrochemical measurement system according to claim 19, further comprising:
a reference electrode;
a counter electrode; and
a potentiostat constructed to control potentials of the working electrode, the reference electrode and the counter electrode.