# US 2026/0063482 A1 · Strain gauge, strain measurement device, and strain measurement method

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0063482 A1
- Document ID: US20260063482A1
- Status: Published application
- Kind: A1
- Application number: 19/310,224
- Filed: 2025-08-26
- Published: 2026-03-05
- Earliest claimed: 2024-09-03
- Assignees: Research Institute For Electromagnetic Materials
- Applicants: Research Institute for Electromagnetic Materials
- Inventors: Nobukiyo KOBAYASHI; Yui HASEGAWA; Kenji IKEDA; Tadayoshi IWASA
- Web page: https://patentgrep.com/patent/US20260063482A1

## CPC

- G01L 1/2287: {constructional details of the strain gauges (adjustable resistors H01C10/00)}
- G01L 1/2262: {involving simple electrical bridges}
- G01L: MEASURING FORCE, STRESS, TORQUE, WORK, MECHANICAL POWER, MECHANICAL EFFICIENCY, OR FLUID PRESSURE (weighing G01G)

## Abstract

To provide a strain gauge that can achieve improvement of practicality. A nano-granular structure film constituting a resistor 2 formed on one main surface of a substrate 1 of a strain gauge has a composition represented by a general formula L100-a-b-cMaFbOc (L is one or more metal elements selected from Fe, Co, Ni, Pt, Au, Ag, and Cu; M is one or more elements selected from Li, Mg, Al, Ca, Sr, Ba, Gd, and Y: F is fluorine: O is oxygen; and 40.0≤(a+b+c)≤63.0). The resistor 2 is constituted of a nano-granular structure film in which metal particles Q1 represented by L and having an average particle diameter of 1.0 to 5.0 nm are distributed in an insulating matrix Q2 formed of a fluoride of M or a fluoride and an oxide of M.

## Claims

### Claim 1

A strain gauge comprising:
a substrate; and
a resistor formed on a surface of the substrate,
wherein the resistor is constituted of a nano-granular structure film which has a composition represented by a general formula L100-a-b-cMaFbOc, wherein L is one or more metal elements selected from Fe, Co, Ni, Pt, Au, Ag, and Cu; M is one or more elements selected from Li, Mg, Al, Ca, Sr, Ba, Gd, and Y; F is fluorine; O is oxygen; and 40.0≤(a+b+c)≤63.0, and in which metal particles represented by L and having an average particle diameter of 1.0 to 5.0 nm are distributed in an insulating matrix formed of a fluoride of M or a fluoride and an oxide of M.

### Claim 2 (depends on 1)

The strain gauge according to claim 1,
wherein a degree of crystallinity of the insulating matrix is 20% or more.

### Claim 3 (depends on 2)

The strain gauge according to claim 2,
wherein a degree of crystallinity of the insulating matrix is included in a range of 24% to 64%.

### Claim 4 (depends on 3)

The strain gauge according to claim 3,
wherein L is one or more magnetic metal elements selected from Fe, Co, and Ni,
the degree of crystallinity of the insulating matrix is included in a range of 38% to 64%, and
a+b+c is included in a range of 50.1% to 59.1%.

### Claim 5 (depends on 3)

The strain gauge according to claim 3,
wherein L is one or more nonmagnetic metal elements selected from Pt, Au, Ag, and Cu,
the degree of crystallinity of the insulating matrix is included in a range of 41% to 61%, and
a+b+c is included in a range of 54.5% to 58.1%.

### Claim 6 (depends on 1)

The strain gauge according to claim 1,
wherein a change in a gauge rate within a temperature range of 0 to 50° C. is ±1500 ppm/° C. or less.

### Claim 7 (depends on 1)

A strain measurement device comprising:
the strain gauge according to claim 1;
a circuit component constituting a bridge circuit including the strain gauge; and
a magnet configured to apply a magnetic field to the strain gauge.

### Claim 8 (depends on 1)

A strain measurement method comprising:
a step of attaching the strain gauge according to claim 1 to an object;
a step of applying a magnetic field to the strain gauge using a magnet; and
a step of detecting strain appearance of the object according to a change in electrical resistance of the strain gauge.