# US 2026/0062839 A1 · Carbon fiber bundle and method for producing carbon fiber bundle

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0062839 A1
- Document ID: US20260062839A1
- Status: Published application
- Kind: A1
- Application number: 19/381,788
- Filed: 2025-11-06
- Published: 2026-03-05
- Earliest claimed: 2023-05-10
- Assignees: Mitsubishi Chemical Corporation
- Applicants: Mitsubishi Chemical Corporation
- Inventors: Naomasa MATSUYAMA; Kyu OTA; Mitsuhiro HAMADA; Hiroko MATSUMURA; Hiroki HAMAMOTO
- Web page: https://patentgrep.com/patent/US20260062839A1

## CPC

- D01F 6/18: from polymers of unsaturated nitriles, e.g. polyacrylonitrile, polyvinylidene cyanide
- D01F 9/22: from polyacrylonitriles
- D01D 5/04: Dry spinning methods {(D01D5/0038 takes precedence)}
- D01D 5/06: Wet spinning methods {(D01D5/0046 takes precedence)}
- D01F 6/38: comprising unsaturated nitriles as the major constituent
- D01F 9/225: {from stabilised polyacrylonitriles}
- D10B 2101/12: Carbon; Pitch
- D10B 2321/10: polymers of unsaturated nitriles, e.g. polyacrylonitrile, polyvinylidene cyanide
- D01F: CHEMICAL FEATURES IN THE MANUFACTURE OF ARTIFICIAL FILAMENTS, THREADS, FIBRES, BRISTLES OR RIBBONS; APPARATUS SPECIALLY ADAPTED FOR THE MANUFACTURE OF CARBON FILAMENTS
- D01D: MECHANICAL METHODS OR APPARATUS IN THE MANUFACTURE OF ARTIFICIAL FILAMENTS, THREADS, FIBRES, BRISTLES OR RIBBONS
- D10B: INDEXING SCHEME ASSOCIATED WITH SUBLASSES OF SECTION D, RELATING TO TEXTILES

## Abstract

Provided a carbon fiber bundle in which the average diameter of carbon fiber single-fibers is increased without reducing the strand strength and strand elastic modulus of the carbon fibers, and a method for producing the same. Also provided is a carbon fiber suitable for a carbon fiber composite material having excellent compressive strength in the fiber axial direction. The carbon fiber bundle of the present invention has a strand strength of 4.5 GPa or more, a strand elastic modulus of 320 GPa or more, substantially no twist, and an average diameter of carbon fiber single-fibers of 6.5 μm or more and 8.5 μm or less.

## Claims

### Claim 1

A carbon fiber bundle having a strand strength of 4.5 GPa or more and a strand elastic modulus of 320 GPa or more,
having substantially no twist, and
having an average diameter of carbon fiber single-fibers of 6.5 μm or more and 8.5 μm or less.

### Claim 2 (depends on 1)

The carbon fiber bundle according to claim 1, wherein the carbon fiber single-fibers each have a crystallite size Lc of 3.4 nm or more and 4.1 nm or less.

### Claim 3 (depends on 1)

The carbon fiber bundle according to claim 1, wherein the carbon fiber single-fibers have an average void length of 22.0 nm or less.

### Claim 4 (depends on 1)

The carbon fiber bundle according to claim 1, wherein the carbon fiber single-fibers have a fracture surface formation energy of 18 N/m or more.

### Claim 5 (depends on 1)

The carbon fiber bundle according to claim 1, wherein the carbon fiber single-fibers in the carbon fiber bundle have a coefficient of variation (CV %) in elastic modulus in a single-fiber tensile test of 17.5% or less.

### Claim 6 (depends on 1)

The carbon fiber bundle according to claim 1, wherein the carbon fiber bundle is non-entangled.

### Claim 7 (depends on 1)

The carbon fiber bundle according to claim 1, wherein a product of the average diameter (unit: μm) of the carbon fiber single-fibers and the strand strength (unit: GPa) of the carbon fiber bundle is 31 or more.

### Claim 8 (depends on 1)

The carbon fiber bundle according to claim 1, wherein the strand strength is 4.85 GPa or more, and the strand elastic modulus is 365 GPa or more.

### Claim 9 (depends on 1)

The carbon fiber bundle according to claim 1, wherein the average diameter of the carbon fiber single-fibers is 6.8 μm or more, the strand strength of the carbon fiber bundle is 4.65 GPa or more, and the strand elastic modulus of the carbon fiber bundle is 365 GPa or more and 403 GPa or less.

### Claim 10 (depends on 1)

The carbon fiber bundle according to claim 1, wherein the average diameter of the carbon fiber single-fibers is 7.5 μm or more.

### Claim 11 (depends on 1)

The carbon fiber bundle according to claim 1, wherein the carbon fiber bundle has a knot strength of 80 N/mm2 or more.

### Claim 12 (depends on 1)

The carbon fiber bundle according to claim 1, wherein the carbon fiber single-fibers have a density of 1.79 g/cm3 or more.

### Claim 13

A method for producing a carbon fiber bundle, the method comprising heating a carbon fiber precursor acrylic fiber bundle in an oxidizing atmosphere to form a stabilized fiber bundle, and heating the stabilized fiber bundle in a non-oxidizing atmosphere to form a carbon fiber bundle, wherein
in the heating in the non-oxidizing atmosphere, a temperature rising rate when a temperature is raised from 1800° C. to 2200° C. is from 200 to 500° C./min, and
an average diameter of carbon fiber single-fibers contained in the produced carbon fiber bundle is 6.5 μm or more and 8.5 μm or less.

### Claim 14 (depends on 13)

A method for producing a carbon fiber bundle according to claim 13, the method comprising the following steps (1) and (2):
(1) a coagulation step of discharging an acrylonitrile-based polymer solution from a discharge hole into air by using a dry-wet spinning method, and then coagulating the acrylonitrile-based polymer solution in a coagulation bath including an aqueous solution having a temperature of 10° C. or lower and an organic solvent concentration of 80.0 mass % or more and 81.0 mass % or less to produce a coagulated yarn bundle containing the organic solvent; and
(2) a second stretching step of stretching the coagulated yarn bundle produced in the coagulation step at a stretching ratio of 2.0 times or more and 3.2 times or less in a hot aqueous solution having a temperature of 75° C. or higher and an organic solvent concentration of 40 mass % or more and 65 mass % or less to produce the carbon fiber precursor acrylic fiber bundle.

### Claim 15 (depends on 13)

The method for producing a carbon fiber bundle according to claim 13, the method further comprising a first stretching step of stretching the coagulated yarn bundle produced in the coagulation step in air at a stretching ratio of 1.00 times or more and 1.20 times or less between the coagulation step and the second stretching step, wherein the coagulated yarn bundle produced in the first stretching step is stretched in the second stretching step.

### Claim 16 (depends on 13)

The method for producing a carbon fiber bundle according to claim 13, wherein in the second stretching step, the coagulated yarn bundle is stretched, then the organic solvent is removed, the coagulated yarn bundle is shrunk or stretched at a ratio of 0.96 times or more and 1.30 times or less in hot water at a temperature of 90° C. or higher, and is stretched at a stretching ratio of 3.7 times or more and 4.2 times or less in a pressurized water vapor atmosphere to produce the carbon fiber precursor acrylic fiber bundle.

### Claim 17 (depends on 13)

The method for producing a carbon fiber bundle according to claim 13, wherein the concentration of the organic solvent in the aqueous solution used in the coagulation step is 80.2 mass % or more and 80.6 mass % or less.

### Claim 18 (depends on 13)

The method for producing a carbon fiber bundle according to claim 13, wherein the organic solvent is dimethylformamide.

### Claim 19 (depends on 13)

The method for producing a carbon fiber bundle according to claim 13, the method comprising the following steps (3) to (6):
(3) a stabilization step of heating a carbon fiber precursor acrylic fiber bundle or the carbon fiber precursor acrylic fiber bundle produced in the second stretching step in an oxidizing atmosphere having a temperature gradient within an ambient temperature range of 200° C. or higher and 260° C. or lower at an elongation percentage of 3.0% or more and 8.0% or less to produce a stabilized fiber bundle having a density of 1.33 g/cm3 or more and 1.36 g/cm3 or less;
(4) a first carbonization step of heating the stabilized fiber bundle produced in the stabilization step in a non-oxidizing atmosphere having a temperature gradient within an ambient temperature range of 300° C. or higher and 900° C. or lower at an elongation percentage of 4.0% or more and 5.0% or less;
(5) a second carbonization step of heating the fiber bundle while applying a tension of 0.15 cN/dtex or more and 0.21 cN/dtex or less to the fiber bundle in a non-oxidizing atmosphere having a temperature gradient within an ambient temperature range of 1000° C. or higher and 1800° C. or lower after the first carbonization step; and
(6) a third carbonization step of heating the fiber bundle while applying a tension of 0.15 cN/dtex or more and 0.23 cN/dtex or less to the fiber bundle in a non-oxidizing atmosphere having a temperature gradient within an ambient temperature range of 1700° C. or higher and 2300° C. or lower after the second carbonization step.

### Claim 20 (depends on 19)

The method for producing a carbon fiber bundle according to claim 19, wherein in the third carbonization step, a temperature rising rate when the ambient temperature is increased from 1800° C. to 2200° C. is 210° C./min or more and 340° C./min or less.

### Claim 21 (depends on 19)

The method for producing a carbon fiber bundle according to claim 19, wherein in the third carbonization step, the temperature rising rate when the ambient temperature is increased from 1800° C. to 2200° C. is 215° C./min or more and 300° C./min or less.

### Claim 22 (depends on 19)

The method for producing a carbon fiber bundle according to claim 19, wherein a difference between a maximum ambient temperature in the second carbonization step and an inlet ambient temperature in the third carbonization step is 500° C. or lower.

### Claim 23 (depends on 19)

The method for producing a carbon fiber bundle according to claim 19, wherein the difference between the maximum ambient temperature in the second carbonization step and the inlet ambient temperature in the third carbonization step is 300° C. or lower.

### Claim 24 (depends on 13)

The method for producing a carbon fiber bundle according to claim 13, wherein a maximum temperature of a heating temperature in the heating in the non-oxidizing atmosphere is from 2100 to 2300° C.