# US 2026/0062782 A1 · Steel sheet and method of manufacturing the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0062782 A1
- Document ID: US20260062782A1
- Status: Published application
- Kind: A1
- Application number: 19/107,433
- Filed: 2023-09-08
- Published: 2026-03-05
- Earliest claimed: 2022-09-09
- Assignees: Nippon Steel Corporation
- Applicants: Nippon Steel Corporation
- Inventors: Yuya SUZUKI; Masayoshi SAWADA; Masafumi AZUMA; Kengo TAKEDA
- Web page: https://patentgrep.com/patent/US20260062782A1

## CPC

- C22C 38/58: with more than 1.5% by weight of manganese
- B32B 15/013: {one layer being formed of an iron alloy or steel, another layer being formed of a metal other than iron or aluminium}
- C21D 1/18: Hardening (C21D1/02 takes precedence); Quenching with or without subsequent tempering (quenching devices C21D1/62)
- C21D 6/001: {containing Ni (C21D6/004 takes precedence)}
- C21D 6/002: {containing Cr (C21D6/004 takes precedence)}
- C21D 6/004: {containing Cr and Ni}
- C21D 6/005: {containing Mn}
- C21D 6/007: {containing Co}
- C21D 6/008: {containing Si}
- C21D 8/02: during manufacturing of plates or strips (C21D8/12 takes precedence)
- C21D 8/0226: {Hot rolling}
- C21D 8/0236: {Cold rolling}
- C21D 8/0263: {following hot rolling}
- C21D 8/0273: {Final recrystallisation annealing}
- C21D 8/0278: involving a particular surface treatment (C21D8/0294 takes precedence)
- C21D 9/46: for sheet metals
- C22C 38/00: Ferrous alloys, e.g. steel alloys (cast-iron alloys C22C37/00)
- C22C 38/001: {containing N}
- C22C 38/002: {containing In, Mg, or other elements not provided for in one single group C22C38/001 - C22C38/60}
- C22C 38/005: {containing rare earths, i.e. Sc, Y, Lanthanides}
- C22C 38/008: {containing tin}
- C22C 38/02: containing silicon
- C22C 38/04: containing manganese
- C22C 38/06: containing aluminium
- C22C 38/08: containing nickel {(C22C38/105 takes precedence)}
- C22C 38/12: containing tungsten, tantalum, molybdenum, vanadium, or niobium
- C22C 38/14: containing titanium or zirconium
- C22C 38/16: containing copper
- C22C 38/20: with copper
- C22C 38/22: with molybdenum or tungsten
- C22C 38/24: with vanadium
- C22C 38/26: with niobium or tantalum
- C22C 38/28: with titanium or zirconium
- C22C 38/30: with cobalt
- C22C 38/32: with boron
- C22C 38/38: with more than 1.5% by weight of manganese
- C22C 38/42: with copper
- C22C 38/44: with molybdenum or tungsten
- C22C 38/46: with vanadium
- C22C 38/48: with niobium or tantalum
- C22C 38/50: with titanium or zirconium
- C22C 38/52: with cobalt
- C22C 38/54: with boron
- C22C 38/60: containing lead, selenium, tellurium, or antimony, or more than 0.04% by weight of sulfur
- C23C 2/02: Pretreatment of the material to be coated, e.g. for coating on selected surface areas (C23C2/30 takes precedence)
- C23C 2/0224: {Two or more thermal pretreatments}
- C23C 2/024: {by cleaning or etching}
- C23C 2/06: Zinc or cadmium or alloys based thereon
- C23C 2/28: Thermal after-treatment, e.g. treatment in oil bath
- C23C 2/285: {for remelting the coating}
- C23C 2/40: Plates; Strips
- C21D 2211/001: Austenite
- C21D 2211/002: Bainite
- C21D 2211/005: Ferrite
- C21D 2211/008: Martensite
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM
- C21D: MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass C23F17/00; unidirectional solidification of eutectic materials or unidirectional demixing of eutectoid materials C30B)
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)

## Abstract

This steel sheet includes: a base steel sheet having a predetermined chemical composition; and a zinc-plated layer formed on a surface of the base steel sheet, in which, when a sheet thickness of the base steel sheet is denoted by t, a metallographic structure at a t/4 position, which is a position at t/4 from the surface in a cross section in a sheet thickness direction of the base steel sheet, contains, by volume percentage, tempered martensite: 85% or more, residual austenite: 7% or more, and one or more selected from ferrite, pearlite, bainite, and fresh martensite: 0% or more and 8% or less, a metallographic structure in a surface layer region, which is a range from the surface to a position of 50 μm in the cross section in the sheet thickness direction, contains, by volume percentage, 30% or more of bainite, and a remainder including one or more selected from ferrite, pearlite, tempered martensite, fresh martensite, and residual austenite, in the surface layer region, a diameter of prior austenite grains in the sheet thickness direction is 10.0 μm or less, and a tensile strength of the steel sheet is 1,470 MPa or more.

## Claims

### Claim 1

A steel sheet comprising:
a base steel sheet; and
a zinc-plated layer formed on a surface of the base steel sheet,
wherein the base steel sheet has a chemical composition including, by mass %,
C: 0.180% or more and 0.400% or less,
Si: 0.050% or more and 1.000% or less,
Mn: 2.00% or more and 4.00% or less,
Al: 0.10% or more and 2.00% or less,
Ti: 0.010% or more and 0.200% or less,
B: 0.0010% or more and 0.0100% or less,
N: 0.0010% or more and 0.0100% or less,
P: 0% or more and 0.0400% or less,
S: 0% or more and 0.0100% or less,
0: 0% or more and 0.0060% or less,
Cr: 0% or more and 0.50% or less,
Ni: 0% or more and 1.00% or less,
Cu: 0% or more and 1.00% or less,
Mo: 0% or more and 0.500% or less,
Nb: 0% or more and 0.200% or less,
V: 0% or more and 0.500% or less,
W: 0% or more and 0.100% or less,
Ta: 0% or more and 0.100% or less,
Sn: 0% or more and 0.050% or less,
Co: 0% or more and 0.500% or less,
As: 0% or more and 0.050% or less,
Sb: 0% or more and 0.050% or less,
Mg: 0% or more and 0.050% or less,
Ca: 0% or more and 0.040% or less,
REM: 0% or more and 0.050% or less,
Zr: 0% or more and 0.050% or less,
Bi: 0% or more and 0.050% or less,
Sr: 0% or more and 0.050% or less, and
a remainder: Fe and impurities,
when a sheet thickness of the base steel sheet is denoted by t, a metallographic structure at a t/4 position, which is a position at t/4 from the surface in a cross section in a sheet thickness direction of the base steel sheet, contains, by volume percentage,
tempered martensite: 85% or more,
residual austenite: 7% or more, and
one or more selected from ferrite, pearlite, bainite, and fresh martensite: 0% or more and 8% or less,
a metallographic structure in a surface layer region, which is a range from the surface to a position of 50 m in the cross section in the sheet thickness direction, contains, by volume percentage,
30% or more of bainite, and
remainder including one or more selected from ferrite, pearlite, tempered martensite, fresh martensite, and residual austenite,
in the surface layer region, a diameter of prior austenite grains in the sheet thickness direction is 10.0 m or less, and
a tensile strength of the steel sheet is 1,470 MPa or more.

### Claim 2 (depends on 1)

The steel sheet according to claim 1,
wherein, when an Al content is denoted by <<Al>>, a N content is denoted by <<N>>, and a Ti content is denoted by <<Ti>> in terms of atomic %, Expression (1) is satisfied,
〈
〈
Al
〉
〉
≥
〈
〈
N
〉
〉
-
0.5
×
〈
〈
Ti
〉
〉
.
(
1
)

### Claim 3 (depends on 1)

The steel sheet according to claim 1,
wherein the zinc-plated layer is a hot-dip galvanized layer.

### Claim 4 (depends on 1)

The steel sheet according to claim 1,
wherein the zinc-plated layer is a hot-dip galvannealed layer.

### Claim 5

A method of manufacturing a steel sheet, comprising:
a heating process of heating a slab such that a heating temperature T in units of K satisfies Expression (2) when an Al content is denoted by [Al] and a N content is denoted by [N] in terms of mass %;
a hot rolling process of hot-rolling the slab after the heating process to obtain a steel sheet;
a coiling process of cooling the steel sheet to a coiling temperature of 500° C. or lower at an average cooling rate of 20° C./sec or faster and coiling the steel sheet at the coiling temperature;
a cold rolling process of cold-rolling the steel sheet at a cumulative rolling reduction of 20% or less after pickling the steel sheet after the coiling process as necessary;
an annealing process of heating the steel sheet to an annealing temperature of an Ac3 point or higher and 900° C. or lower in an atmosphere having an oxygen potential of −1.50 or more and holding the steel sheet at the annealing temperature for 10 seconds or longer and 600 seconds or shorter;
a first cooling process of cooling the steel sheet after the annealing process to a first temperature range of an Ms point −100° C. or higher and a Bs point or lower at an average cooling rate of 20° C./sec or faster;
a holding process of holding the steel sheet in the first temperature range for 60 seconds or longer and 600 seconds or shorter; and
a second cooling process of cooling the steel sheet after the holding process to a second temperature range of 250° C. or lower and 150° C. or higher at an average cooling rate of 20° C./sec or faster,
log
10
(
[
Al
]
×
[
N
]
)
≤
-
9730
/
T
+
3.36
.
(
2
)

### Claim 6 (depends on 2)

The steel sheet according to claim 2,
wherein the zinc-plated layer is a hot-dip galvanized layer.

### Claim 7 (depends on 2)

The steel sheet according to claim 2,
wherein the zinc-plated layer is a hot-dip galvannealed layer.